journal article·2026-04Open access

Controlling microsegregation–induced phase formation and pitting corrosion in wire-arc additively manufactured precipitation-hardened martensitic stainless steel

Y.H. Mozumder, M. Taylor, V. Bongiorno, Y. Lu, J. Wang, S. Williams, P.B. Prangnell, E.J. Pickering, F. Scenini

Abstract

Wire-arc additive manufacturing (WAAM) often leads to elemental microsegregation and non-equilibrium phase formation during solidification, which can compromise the corrosion performance of alloys. This study presents the first detailed investigation of WAAM processed Custom 465® (C465), a precipitation-hardened martensitic stainless steel, focusing on the effect of post-printing heat treatment strategies on the microstructure and its pitting corrosion behaviour, benchmarked against the conventionally manufactured wrought C465 material. As-printed C465 exhibited large columnar prior austenite grains (PAGs) and pronounced microsegregation, which stabilised the retained austenite and Laves phases. The standard solution treatment (SST) refined the PAGs but was insufficient to eliminate microsegregation. Guided by diffusion-controlled transformation (DICTRA) simulations, a suitable homogenisation treatment was developed that effectively reduced WAAM-induced microsegregation and associated secondary phases. Ageing treatment after the SST only partially promoted martensite-to-austenite reversion, likely driven by pre-existing retained austenite and Ni-segregation. In contrast, ageing treatment after homogenisation and SST largely suppressed this transformation, resulting in a microstructure comparable to the wrought counterpart. The corrosion performance of C465 produced by both WAAM and conventional routes was further evaluated using cyclic potentiodynamic polarisation and electrochemical noise techniques. With the standard heat treatment, the WAAM material exhibited inferior pitting resistance compared to its wrought counterpart. Surface characterisation following anodic polarisation revealed pit initiation at Cr-depleted interdendritic retained austenite regions and Laves/matrix interfaces in the WAAM material. However, homogenisation prior to SST and ageing treatment significantly enhanced the pitting resistance by eliminating preferential pit nucleation sites, thereby achieving a performance comparable to the wrought counterpart. Overall, this work demonstrates the critical role of post-printing heat treatment strategies in addressing WAAM-induced microstructural heterogeneities and mitigating pitting susceptibilities. • As-printed WAAM C465 exhibited coarse grains and pronounced microsegregation. • Standard heat treatment refined grains but microsegregation persisted. • DICTRA-based homogenisation treatment substantially reduced microsegregation. • WAAM C465 showed lower pitting resistance than wrought C465. • Homogenisation improved pitting resistance by reducing key pit nucleation sites.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Hydrogen embrittlement and corrosion behaviors in metals · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
2. Energy and emissions saving potential of additive manufacturing: the case of lightweight aircraft components10.1016/j.jclepro.2015.04.109 ↗
3. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
4. Ultrahigh-strength steels for aerospace applications10.1007/BF03220942 ↗
5. High strength materials for aircraft landing gear10.1108/eb036313 ↗
6. Cadmium replacement in coatings10.1177/02670844251336526 ↗
7. Development of Custom 465® corrosion-resisting steel for landing gear applications10.1007/s11665-015-1830-5 ↗
8. Carpenter Technology, Custom 465®, (2022). 〈https://www.carpentertechnology.com/alloy-finder/custom-465〉 (accessed November 13, 2025).
9. SAE International, Steel, Corrosion-Resistant, Bars, Wire, and Forgings 12Cr - 11Ni - 1.7Ti - 1Mo Vacuum Induction Plus Vacuum Consumable Electrode Remelted Solution Heat Treated, Precipitation Hardenable, (2012). https://doi.org/10.4271/AMS5936C.10.4271/AMS5936C ↗
10. Carpenter Technology, C465 Datasheet, (n.d.). 〈https://www.carpentertechnology.com/hubfs/Data〉 Sheets/Custom_465_Datasheet.pdf (accessed November 15, 2025).
11. Effect of aging temperature on the austenite reversion and mechanical properties of a Fe-10Cr-10Ni cryogenic maraging steel10.1016/j.jmrt.2020.12.096 ↗
12. The effect of ɳ-Ni 3 Ti precipitates and reversed austenite on the passive film stability of nickel-rich Custom 465 steel10.1016/j.corsci.2019.04.016 ↗
13. Influence of austenitizing temperature on the microstructure and mechanical properties of an Fe-Cr-Ni-Mo-Ti maraging stainless steel10.1007/s11665-019-04279-6 ↗
14. Hydrogen diffusivity measurement and microstructural characterization of Custom 465 stainless steel10.1016/j.electacta.2015.08.016 ↗
15. The relation between aging temperature, microstructure evolution and hardening of Custom 465® stainless steel10.1016/j.matchar.2017.02.023 ↗
16. Microstructural evolution and mechanical properties of maraging steel produced by wire+arc additive manufacture process10.1016/j.matchar.2017.12.002 ↗
17. The current state of research of wire arc additive manufacturing (WAAM): a review10.3390/app11188619 ↗
18. Microstructural evolution and mechanical behavior of Custom 465 precipitation hardening stainless steel fabricated via laser powder bed fusion10.1016/j.msea.2023.146069 ↗
19. Laser powder bed fusion of crack-susceptible stainless maraging steel undergoing solid-state phase transformations10.1016/j.actamat.2023.119534 ↗
20. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
21. Corrosion of additively manufactured stainless steels—process, structure, performance: a review10.5006/3741 ↗
22. A critical review of corrosion characteristics of additively manufactured stainless steels10.1080/09506608.2020.1855381 ↗
23. Process-microstructure-corrosion of additively manufactured steels: a review10.1080/10408436.2023.2255616 ↗
24. Inter-melt pool corrosion and repassivation of SS316L stainless steel processed by laser powder bed fusion10.1016/j.corsci.2023.111668 ↗
25. Corrosion performance of additively manufactured stainless steel parts: a review
26. On the pitting behaviour of laser powder bed fusion prepared 316L stainless steel upon post-processing heat treatments10.1016/j.corsci.2021.110060 ↗
27. On the microstructural characteristics and corrosion performance of as-printed and heat-treated PH 13–8Mo martensitic stainless steel fabricated by wire arc additive manufacturing
28. Influence of postbuild microstructure on the electrochemical behavior of additively manufactured 17-4 PH stainless steel10.1007/s11837-016-2237-y ↗
29. Stainless steel pitting and early-stage stress corrosion cracking under ultra-low elastic load10.1016/j.corsci.2013.08.028 ↗
30. Thermo-Calc & DICTRA, computational tools for materials science
31. Electrochemical noise studies of the effect of nitrogen on pitting corrosion resistance of high nitrogen austenitic stainless steels10.1016/j.corsci.2011.08.027 ↗
32. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
33. Electrochemical noise (Ecn) measurements as a corrosion monitoring tool: a review10.1515/CORRREV.2002.20.4-5.359 ↗
34. Bemerkungen zur Schichtkristallbildung
35. An experimental confirmation of the pitting potential model of galvele10.1016/0010-938X(88)90069-8 ↗
36. Localised dissolution kinetics, salt films and pitting potentials10.1016/S0010-938X(97)00049-8 ↗
37. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
38. Interpretation of electrochemical noise data10.5006/1.3290350 ↗
39. Potentiostatic pulse technique to determine the efficiency of hydrogen absorption by alloys10.1007/BF01077581 ↗
40. The use of potentiostatic pulse testing to study the corrosion behavior of welded stainless steels in sodium chloride solution10.1016/j.matdes.2015.09.001 ↗
41. Influence of solidification structure on austenite to martensite transformation in additively manufactured hot-work tool steels10.1016/j.actamat.2021.117044 ↗
42. Microstructure engineering during wire-arc additive manufacturing of high-strength martensitic steels10.1007/s11661-025-07988-x ↗
43. The potential for grain refinement of Wire-Arc Additive Manufactured (WAAM) Ti-6Al-4V by ZrN and TiN inoculation
44. High-strength Damascus steel by additive manufacturing10.1038/s41586-020-2409-3 ↗
45. Designing an Fe-Ni-Ti maraging steel tailor-made for laser additive manufacturing
46. Solute and phase heterogeneous distribution at different scales and its effect on ageing physical phenomena in a laser powder bed fusion produced maraging steel
47. Correlation between solidification parameters and weld microstructures10.1179/imr.1989.34.1.213 ↗
48. Phase-field modeling and Experimental investigation for rapid solidification in wire and arc additive manufacturing10.1016/j.jmrt.2024.01.021 ↗
49. Effect of dendritic morphology and central segregation of billet castings on the microstructure and mechanical property of hot-rolled wire rods10.1002/srin.201600426 ↗
50. Comparison of maraging steel micro- and nanostructure produced conventionally and by laser additive manufacturing
51. In-Situ EBSD Study of Austenitisation in a Wire-Arc Additively Manufactured High-Strength Steel10.1088/1757-899X/1310/1/012001 ↗
52. Microstructural refinement by spontaneous recrystallization without prior deformation of a 15-5 PH steel alloy and its mechanism10.1016/j.matdes.2023.112370 ↗
53. Microstructural evolution and corrosion behaviors of Inconel 718 alloy produced by selective laser melting following different heat treatments
54. Tailoring the nanostructure of laser powder bed fusion additively manufactured maraging steel
55. On the role of cellular microstructure in austenite reversion in selective laser melted maraging steel10.1016/j.jmst.2023.10.032 ↗
56. Precipitation and reverted austenite formation in maraging 350 steel: competition or cooperation?10.1016/j.actamat.2024.119865 ↗
57. Optimizing microstructure and mechanical properties in additively manufactured 18Ni (300) maraging steel by controlling strengthening agents10.1016/j.matdes.2025.114114 ↗
58. Effect of ageing temperature on the microstructure and localised corrosion of 15–5PH stainless steel10.1016/j.corsci.2025.112800 ↗
59. Corrosion resistance of 13wt% Cr martensitic stainless steels: Additively manufactured CX versus wrought Ni-containing AISI 42010.1016/j.corsci.2021.109362 ↗
60. Elucidating the effect of titanium alloying on the pitting corrosion of ferritic stainless steel10.1016/j.jmrt.2023.12.032 ↗
61. The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions10.1016/0010-938X(92)90074-D ↗
62. Effect of titanium nitride (TiN) on the corrosion behavior of a supermartensitic stainless steel10.1002/maco.201810289 ↗