journal article·2026-06

Harnessing non-isothermal annealing to unlock the microstructure-property nexus in solid-state additively manufactured age-hardenable aluminum alloy

Nan Li, Qiang Wang, Shuo Yin, Shouxun Ji, Kuaishe Wang, Wenjuan Niu, Mingxing Zhang

Publisher page

Abstract

High-strength age-hardenable aluminum (Al) alloys are widely used in aerospace and advanced manufacturing due to their excellent strength-to-weight ratio and heat-treatable properties. However, the wide solidification temperature range leads to the formation of coarse columnar grains and hot cracking when processed via fusion-based additive manufacturing (AM). In the present study, laser-assisted cold spray (LACS), a solid-state AM approach, is employed to fabricate high strength Al alloys through high strain-rate plastic deformation of metal particles. Subsequently, the microstructural evolution, precipitation behavior, and micro/nano-hardening mechanisms of the severely plastically deformed alloy under non-isothermal annealing conditions are systematically investigated. Key findings revealed that the synergistic coupling of laser thermal energy and high velocity particle kinetic energy enabled the fabrication of Al-Zn-Mg-Cu/AlO composite deposits with ultrahigh density and a bimodal grain distribution. Laser preheating significantly enhanced interparticle bonding quality and microstructural homogeneity, establishing an optimal foundation for subsequent non-isothermal annealing. The severe plastic deformation (SPD) introduced a high density of dislocations, which acted as preferential nucleation sites for precipitates. Concurrently, localized transient heating promoted solute diffusion, accelerating η/η′-MgZn phase formation while suppressing Guinier Preston (G-P) zone precipitation. Notably, non-isothermal annealing preserved the classical precipitation sequence of η/η′-MgZn strengthening phases. As annealing temperatures increased to 270 °C, the deposits reached a peak microhardness of 170 HV, while the nanoindentation hardness significantly increased to 4.1 ± 0.2 GPa. Meanwhile, the ultimate tensile strength reaches its maximum value of 485 MPa at the annealing temperature of 270 °C, achieving a simultaneous enhancement of both strength and ductility. Quantitative strengthening analysis confirms that this improvement in strength is primarily attributed to precipitation strengthening, which accounts for 32% of the total increase in strength. This work demonstrated the efficacy of coupling solid-state AM with non-isothermal annealing in tailoring microstructures and properties of thermally sensitive Al alloys. By integrating SPD with programmable heat treatment, a paradigm in solid-state AM is established, in which deformation-inherited microstructures are utilized to control precipitation kinetics and ultimately tailor the microstructure-property nexus in age-hardenable alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Microstructure control for inoculated high-strength aluminum alloys fabricated by additive manufacturing: a state-of-the-art review10.1016/j.pmatsci.2025.101502 ↗
2. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
3. Solidification in metal additive manufacturing: challenges, solutions, and opportunities10.1016/j.pmatsci.2024.101361 ↗
4. Origin of thermal deformation induced crystallization and microstructure formation in additive manufactured FCC, BCC, HCP metals and its alloys10.1016/j.ijplas.2023.103831 ↗
5. Tailored porosity in additive manufacturing of 7075 aluminum alloy for crack suppression and high strength10.1016/j.jmatprotec.2024.118620 ↗
6. Additive manufacturing of high-strength and crack-sensitive aluminum alloy using novel in-situ ceramics reinforced powder10.1016/j.jmst.2025.07.036 ↗
7. Mechanical field assisted additive manufacturing of ultrahigh strength aluminum alloy10.1088/2631-7990/adbb95 ↗
8. Recent advances in inoculation treatment for powder-based additive manufacturing of aluminium alloys10.1016/j.mser.2024.100773 ↗
9. Effect of laser melting process on a modified AA7075 alloy with Ti-B-Zr modifiers10.1007/s11665-021-06432-6 ↗
10. Cold spray additive manufacturing and repair: fundamentals and applications
11. Solid-state cold spraying of Ti and its alloys: a literature review10.1016/j.pmatsci.2019.100633 ↗
12. Nanotwinning-assisted dynamic recrystallization at high strains and strain rates10.1038/s41563-022-01250-0 ↗
13. Towards high-strength cold spray additive manufactured metals: methods, mechanisms, and properties10.1016/j.jmst.2023.05.047 ↗
14. Quantifying dislocation drag at high strain rates with laser-induced Microprojectile impact10.1016/j.ijplas.2024.103924 ↗
15. On the solidification characteristics, deformation, and functionally graded interfaces in additively manufactured hybrid aluminum alloys10.1016/j.ijplas.2020.102840 ↗
16. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
17. Metals strengthen with increasing temperature at extreme strain rates10.1038/s41586-024-07420-1 ↗
18. Strength gradient in impact-induced metallic bonding
19. Al matrix composites fabricated by solid-state cold spray deposition: a critical review10.1016/j.jmst.2021.01.026 ↗
20. Cold spray additive manufacturing of metal matrix composites (MMCs) using a novel nano-TiB2-reinforced 7075Al powder10.1016/j.jallcom.2019.152962 ↗
21. Thermo-mechanical post-treatment: A strategic approach to improve microstructure and mechanical properties of cold spray additively manufactured composites10.1016/j.matdes.2018.06.062 ↗
22. Achieving simultaneously improved tensile strength and ductility of a nano-TiB2/AlSi10Mg composite produced by cold spray additive manufacturing10.1016/j.compositesb.2020.108404 ↗
23. A new strategy for strengthening additively manufactured cold spray deposits through in-process densification
24. Effect of laser power on the microstructure and mechanical properties of laser-assisted cold sprayed 7075 aluminum alloy deposits10.1016/j.msea.2023.145224 ↗
25. Recover the tensile strength of hard aluminum alloy through laser assisted cold spray10.1016/j.surfcoat.2024.130966 ↗
26. Two laser beam modulation of microstructure and residual stress field in cold sprayed Al alloy for recovering fatigue performance10.1016/j.ijplas.2023.103598 ↗
27. Microstructure and fatigue performance of hard Al alloy repaired by supersonic laser deposition with laser shock peening treatment10.1016/j.matchar.2023.112827 ↗
28. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
29. Structural integrity of additively manufactured aluminum alloys: effects of build orientation on microstructure, porosity, and fatigue behavior
30. Laser assisted cold spray of aluminum alloy 6061: experimental results
31. Deformation-driven precipitate evolution in cold sprayed age-hardenable aluminum alloys10.1016/j.apsusc.2025.164914 ↗
32. Microstructural and tribological properties of high-performance Inconel 625 alloy-WS2 self-lubricious composite coating by laser assisted cold spray10.1016/j.jallcom.2024.173840 ↗
33. Achieving superior strength and ductility synergy in bulk ultrafine grained Al-Mg-Sc-Zr alloy via powder pre-aging10.1016/j.ijplas.2024.104143 ↗
34. Achieving exceptional strength-ductility synergy in a complex-concentrated alloy via architected heterogeneous grains and nano-sized precipitates10.1016/j.ijplas.2022.103398 ↗
35. Additively manufactured fine-grained ultrahigh-strength bulk aluminum alloys with nanostructured strengthening defects10.1016/j.mattod.2024.05.006 ↗
36. Tuning the microstructure and mechanical properties of additive manufactured aluminum matrix composites by cold spray10.1016/j.surfcoat.2021.127847 ↗
37. Effect of annealing treatment on microstructure and mechanical properties of cold sprayed TiB2/AlSi10Mg composites
38. Significant improvement of mechanical properties of cold-spray-additive manufactured FeCoNiCrMn high-entropy alloy via post-annealing10.1016/j.matchar.2023.113350 ↗
39. The role of annealing temperature on fracture of cold-sprayed copper deposits: toward damage-tolerant additive manufacturing process10.1016/j.jmrt.2025.07.045 ↗
40. 3D microstructure-based modelling of ductile damage at large plastic strains in an aluminum sheet10.1016/j.ijplas.2024.104088 ↗
41. Strain localization and damage development during elevated temperature deformation of AA7075 Aluminum sheet10.1016/j.ijplas.2022.103513 ↗
42. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
43. Microstructure and mechanical properties of cold sprayed 7075 deposition during non-isothermal annealing10.1016/j.surfcoat.2015.07.016 ↗
44. Optimization of cold spray additive manufactured AA2024/Al2O3 metal matrix composite with heat treatment10.1016/j.jmst.2021.07.036 ↗
45. Microstructural evolution of 7075 Al gas atomized powder and high-pressure cold sprayed deposition10.1016/j.surfcoat.2014.04.035 ↗
46. Coupled Eulerian-Lagrangian (CEL) simulation of multiple particle impact during Metal Cold Spray process for coating porosity prediction10.1016/j.surfcoat.2020.125433 ↗
47. Effects of interface bonding on the residual stresses in cold-sprayed Al-6061: a numerical investigation10.1007/s11666-019-00827-7 ↗
48. Adiabatic shear instability is not necessary for adhesion in cold spray10.1016/j.actamat.2018.07.065 ↗
49. Mesoscale modeling of jet initiation behavior and microstructural evolution during cold spray single particle impact10.1016/j.actamat.2019.10.039 ↗
50. Bonding mechanism in cold gas spraying10.1016/S1359-6454(03)00274-X ↗
51. Ductile and high strength Cu fabricated by solid-state cold spray additive manufacturing10.1016/j.jmst.2022.07.003 ↗
52. Heterogeneous microstructural evolution during hydrodynamic penetration of a high-velocity copper microparticle impacting copper10.1016/j.mattod.2023.11.015 ↗
53. The effect of severe plastic deformation on precipitation in supersaturated Al–Zn–Mg alloys10.1016/j.msea.2007.01.001 ↗
54. Dynamic recrystallization of titanium: effect of pre-activated twinning at cryogenic temperature10.1016/j.actamat.2018.05.057 ↗
55. Tensile properties and microstructural evolution of 17–4 PH stainless steel fabricated by laser hybrid additive manufacturing technology10.1016/j.ijplas.2024.103885 ↗
56. Making strong nanomaterials ductile with gradients10.1126/science.1255940 ↗
57. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper10.1126/science.1200177 ↗
58. Additive manufacturing of an ultrastrong, deformable Al alloy with nanoscale intermetallics10.1038/s41467-024-48693-4 ↗
59. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
60. Correlation between microstructure and calorimetric behavior of aluminum alloy 7075 and Al Zn Mg alloys in various tempers10.1016/0921-5093(89)90859-9 ↗
61. Retrogression and re-ageing of 7075 aluminium alloy: microstructural characterization10.1016/S0924-0136(99)00219-8 ↗
62. Nanomechanics of Hall–Petch relationship in nanocrystalline materials10.1016/j.pmatsci.2009.03.008 ↗
63. Influence of stacking-fault energy on microstructural characteristics of ultrafine-grain copper and copper–zinc alloys10.1016/j.actamat.2007.10.053 ↗
64. Mechanical properties of copper/bronze laminates: role of interfaces10.1016/j.actamat.2016.06.023 ↗
65. Tailoring properties of directed energy deposited Al-Mg alloy by balancing laser shock peening and heat treatment10.1016/j.jmst.2024.03.051 ↗
66. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
67. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
68. Grain refinement in 7075 aluminum by thermomechanical processing10.1007/BF02642340 ↗
69. Solution hardening by tetragonal dist ortions: application to irradiation hardening in F.C.C. crystals10.1016/0001-6160(62)90098-6 ↗
70. Substitutional solution hardening10.1016/0001-6160(63)90213-X ↗
71. Strengthening mechanisms in a high-strength bulk nanostructured Cu–Zn–Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
72. Study of microstructural and mechanical anisotropy of 7075 Al deposits fabricated by cold spray additive manufacturing10.1016/j.matdes.2021.110271 ↗
73. Cold spray additive manufacturing of metal matrix composites (MMCs) using a novel nano-TiB2-reinforced 7075Al powder10.1016/j.jallcom.2019.152962 ↗
74. A hybrid approach to improve microstructure and mechanical properties of cold spray additively manufactured A380 aluminum composites10.1016/j.msea.2019.138828 ↗
75. Achieving simultaneously improved tensile strength and ductility of a nano-TiB2/AlSi10Mg composite produced by cold spray additive manufacturing10.1016/j.compositesb.2020.108404 ↗
76. Microstructure and performance of cold sprayed Al-SiC composite coatings with high fraction of particulates10.1016/j.surfcoat.2016.11.047 ↗
77. Cold spray additive manufacturing: a viable strategy to fabricate thick B4C/Al composite coatings for neutron shielding applications10.1016/j.surfcoat.2018.02.007 ↗
78. Cold sprayed AA2024/Al2O3 metal matrix composites improved by friction stir processing: microstructure characterization, mechanical performance and strengthening mechanisms10.1016/j.jallcom.2017.11.132 ↗
79. Microstructures and tensile properties of a selective laser melted Al–Zn–Mg–Cu (Al7075) alloy by Si and Zr microalloying10.1016/j.msea.2020.139492 ↗
80. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties