Ablation resistance of HfC coating reinforced by HfC nanowires in cyclic ablation environment
Source abstract
Abstract
Abstract To improve the ablation resistance of carbon/carbon composites in cyclic ablation environment, SiC/HfC ceramic coating reinforced by HfC nanowires was prepared. The microstructure, bonding strength, coefficient of thermal expansion and cyclic ablation resistance of the as-prepared coating were investigated. After incorporating HfC nanowires, the bonding strength between inner SiC coating and outer HfC coating was increased. HfC nanowires could relieve the coefficient of thermal expansion mismatch between inner and outer coating and improve the toughness of the outer coating. By introducing HfC nanowires, the coated sample’s cyclic ablation resistance was improved. After cyclic ablation under oxyacetylene flame for 60 s × 3, the mass and linear ablation rates of the coated sample with HfC nanowires were only 0.444 mg/s and −0.767 μm/s, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Oxidation kinetics and mechanisms of carbon/carbon composites and their components in water vapor at high temperatures10.1016/j.corsci.2014.10.027 ↗
2. Oxidation protective multilayer coatings for carbon–carbon composites10.1016/S0008-6223(01)00151-8 ↗
3. Oxidation protection of carbon/carbon composites with a plasma-sprayed ZrB2–SiC–Si/Yb2SiO5/LaMgAl11O19 coating during thermal cycling10.1016/j.jeurceramsoc.2015.01.015 ↗
4. Erosion resistance of C/C-SiC-ZrB2 composites exposed to oxyacetylene torch10.1016/j.jeurceramsoc.2016.04.007 ↗
5. A MoSi2/SiC oxidation protective coating for carbon/carbon composites10.1016/j.corsci.2010.11.024 ↗
6. Oxidation protection of ultra-high temperature ceramic ZrxTa1-xB2-SiC/SiC coating prepared by in-situ reaction method for carbon/carbon composites10.1016/j.jeurceramsoc.2014.09.038 ↗
7. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites10.1016/j.carbon.2009.09.035 ↗
8. Rapid oxidation characterization of ultrahigh temperature ceramics10.1111/j.1551-2916.2007.01861.x ↗
9. Hafnium carbide protective layer coatings on carbon/carbon composites deposited with a vacuum plasma spray coating method10.1016/j.jeurceramsoc.2016.01.032 ↗
10. Carbon fiber reinforced hafnium carbide composite10.1023/B:JMSC.0000041696.64055.8c ↗
11. Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame10.1016/j.corsci.2012.08.064 ↗
12. Phase diagram of the Al2O3-HfO2- Y2O3 system10.1016/j.jeurceramsoc.2010.04.041 ↗
13. HfC-based coating prepared by reactive melt infiltration on C/C composite substrate10.1016/j.ceramint.2012.12.059 ↗
14. Structural evolution and ablation mechanism of a hafnium carbide coating on a C/C composite in an oxyacetylene torch environment10.1016/j.corsci.2012.04.033 ↗
15. Ablative property of HfC-based multilayer coating for C/C composites under oxy-acetylene torch10.1016/j.apsusc.2010.11.020 ↗
16. In-situ fabrication of ZrB2-SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
17. Ablation resistance of ZrC/SiC gradient coating for SiC-coated carbon/carbon composites prepared by supersonic plasma spraying10.1016/j.jeurceramsoc.2016.02.047 ↗
18. SiC/HfC/SiC ablation resistant coating for carbon/carbon composites10.1016/j.surfcoat.2012.03.039 ↗
19. Oxidation protection of SiC-coated C/C composites by SiC nanowire-toughened CrSi2–SiC–Si coating10.1016/j.corsci.2011.11.001 ↗
20. A SiC whisker-toughened SiC–CrSi2 oxidation protective coating for carbon/carbon composites10.1016/j.apsusc.2006.07.092 ↗
21. Microstructure and mechanical properties of ultrafine bamboo-shaped SiC rod-reinforced HfC ceramic coating10.1016/j.surfcoat.2013.08.028 ↗
22. SiC nanowires toughened HfC ablative coating for C/C composites10.1016/j.jmst.2014.03.024 ↗
23. Effect of surface ablation products on the ablation resistance of C/C–SiC composites under oxyacetylene torch10.1016/j.corsci.2012.10.003 ↗
24. A Si-Mo-W coating to protect SiC-coated carbon/carbon composites against oxidation10.1111/j.1551-2916.2009.03144.x ↗
25. Effects of deposition temperature and time on HfC nanowires synthesized by CVD on SiC-coated C/C composites10.1016/j.ceramint.2015.12.078 ↗
26. Effect of carbon nanotubes on the toughness, bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites10.1016/j.jallcom.2015.04.223 ↗
27. Oxidation of hafnium carbide and hafnium carbide with additions of tantalum and praseodymium10.1007/BF01151590 ↗