journal article·2021-12

Relationships between fracture toughness, Y2O3 fraction and phases content in modern dental Yttria-doped zirconias

Renan Belli, Katrin Hurle, Jana Schürrlein, Anselm Petschelt, Katharina Werbach, Herwig Peterlik, Torsten Rabe, Björn Mieller, Ulrich Lohbauer

Publisher page

Abstract

Abstract The relationship between fracture toughness and Yttria content in modern zirconia ceramics was revised. For that purpose, we evaluated here 10 modern Y2O3-stabilized zirconia (YSZ) materials currently used in biomedical applications, namely prosthetic and implant dentistry. The most relevant range between 2-5 mol% Y2O3 was addressed by selecting from conventional opaque 3 mol% YSZ up to more translucent compositions (4−5 mol% YSZs). A technical 2YSZ was used to extend the range of our evaluation. The bulk mol% Y2O3 concentration was measured by X-Ray Fluorescence Spectroscopy. Phase quantification by Rietveld refinement considered two tetragonal phases or an additional cubic phase. A first-account of the fracture toughness (KIc) of the pre-sintered blocks is given, which amounted to 0.4 – 0.7 MPa√m. In the fully-densified state, an inverse power-law behavior was obtained between KIc and bulk mol% Y2O3 content, whether using only our measurements or including literature data, challenging some established relationships. A linear relationship between KIc and the fraction of the transformable t-phase was established within the range of 30–70 vol%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Bone Tissue Engineering Materials · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
2. The slippery slope - Critical perspectives on in vitro research methodologies10.1016/j.dental.2011.09.001 ↗
3. Correlation of clinical performance with’ in vitro tests’ of restorative dental materials that use polymer-based matrices10.1016/j.dental.2011.08.594 ↗
4. On edge chipping testing and some personal perspectives on the state of the art of mechanical testing10.1016/j.dental.2014.08.378 ↗
5. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
6. Practical and theoretical considerations on the fracture toughness testing of dental restorative materials10.1016/j.dental.2017.11.016 ↗
7. ADM guidance-ceramics: fracture toughness testing and method selection10.1016/j.dental.2017.03.006 ↗
8. ADM guidance-ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
9. Translational research on clinically failed zirconia implants10.1016/j.dental.2018.11.033 ↗
10. Report on fractures of trilayered all-ceramic fixed dental prostheses10.1016/j.csefa.2016.10.001 ↗
11. Critical notch-root radius effect in SENB-S fracture toughness testing10.1016/0955-2219(95)00197-2 ↗
12. Polished notch modification of SENB-S fracture toughness testing10.1016/S0955-2219(97)00024-1 ↗
13. Sintering and characterization of polycrystalline monoclinic, tetragonal, and cubic zirconia10.1111/j.1151-2916.1992.tb04480.x ↗
14. Effect of molten zone ablated by femtosecond laser on fracture toughness of oxide ceramics10.1016/j.jeurceramsoc.2017.12.049 ↗
15. Determination of fracture toughness of zirconia ceramics with different yttria concentrations by SEVNB method10.1016/j.ceramint.2017.04.064 ↗
16. Trade-off between fracture resistance and translucency of zirconia and lithium-disilicate glass ceramics for monolithic restorations10.1016/j.actbio.2019.04.043 ↗
17. Structural and electrical properties of the 2Bi(2)O(3) center dot 3ZrO(2) system10.1016/j.jssc.2008.02.038 ↗
18. Crystal structure of zirconia by Rietveld refinement, science in China, series a: mathematics, physics
19. Phase stability in plasma-sprayed, partially stabilized zirconia-yttria
20. Phase relationships in Zirconia-Yttria system10.1007/BF01031853 ↗
21. Effect of Yo1.5 dopant on unit-cell parameters of Zro2 at low contents of Yo1.510.1111/j.1151-2916.1989.tb06191.x ↗
22. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
23. ASTMC1421 · 2010
24. ISO24370 · 2005
25. Advanced technical ceramics - test method for determination of fracture toughness of monolithic ceramics - part 3: chevron notched beam (CNB) method
26. Influence of subcritical crack growth on the determination of fracture toughness in brittle materials10.1016/j.jeurceramsoc.2015.11.047 ↗
27. Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs10.1016/j.jeurceramsoc.2018.08.012 ↗
28. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
29. Crack-healing during two-stage crystallization of lithium (di)silicate glass-ceramics10.1016/j.dental.2019.05.013 ↗
30. Thermal healing of cracks in glass10.1016/0022-3093(88)90116-0 ↗
31. How and when does fabrication damage adversely affect the clinical performance of ceramic restorations?10.1016/j.dental.2012.07.001 ↗
32. New perspectives for recycling dental zircoina waste resulting from CAD/CAM manufacturing process10.1016/j.jclepro.2017.03.117 ↗
33. Crystallographic and morphological analysis of sandblasted highly translucent dental zirconia10.1016/j.dental.2017.12.008 ↗
34. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications10.1016/j.dental.2018.03.006 ↗
35. New multi-layered zirconias: composition, microstructure and translucency10.1016/j.dental.2019.02.017 ↗
36. Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations10.1016/j.dental.2016.09.025 ↗
37. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗
38. Assessment of thermodynamic parameters in the system ZrO2-Y2O3-Al2O310.3139/146.017909 ↗
39. On the phase relations in the ZrO2-YO1.5-AlO1.5 system10.1016/j.jallcom.2005.09.079 ↗
40. On the microstructures resulting from the diffusionless cubic-]Tetragonal transformation in Zro2-Y2o3 alloys10.1111/j.1151-2916.1986.tb07356.x ↗
41. Phase stability of thermal barrier oxides: a comparative study of Y and Yb additions10.3139/146.101595 ↗
42. The displacive cubic-]Tetragonal transformation in Zro2 alloys10.1016/0001-6160(87)90189-1 ↗
43. Ferroelastic domain switching as a toughening mechanism in Tetragonal Zirconia10.1111/j.1151-2916.1986.tb07341.x ↗
44. Effect of Yttria content on the zirconia unit cell parameters10.1111/j.1551-2916.2011.04862.x ↗
45. Phase stability of t’ -Zirconia-Based thermal barrier coatings: mechanistic insights10.1111/j.1551-2916.2011.04531.x ↗
46. High temperature x-ray diffraction study on cubic-tetragonal phase transition in the ZrO2-RO1.5 Systems (R: Rare Earths)
47. Cubic-formation and grain-growth mechanisms in tetragonal zirconia polycrystal10.1111/j.1151-2916.2003.tb03483.x ↗
48. Phase evolution upon aging of air-plasma sprayed t’-Zirconia coatings: ISynchrotron X-Ray diffraction10.1111/j.1551-2916.2012.05451.x ↗
49. In situ diffraction study of the high-temperature decomposition of t’ -Zirconia10.1111/jace.13249 ↗
50. Phase evolution upon aging of air plasma sprayed t’-Zirconia coatings: II-Microstructure evolution10.1111/j.1551-2916.2012.05460.x ↗
51. Microstructure of veneered zirconia after surface treatments: a TEM study10.1016/j.dental.2013.07.022 ↗
52. Indentation studies on Y2o3-Stabilized Zro2 .1. Development of indentation-induced cracks10.1111/j.1151-2916.1994.tb05391.x ↗
53. Correlation of the indentation fracture resistance measured using high-resolution optics and the fracture toughness obtained by the single edge-notched beam (SEPB) method for typical structural ceramics with various microstructures10.1016/j.ceramint.2016.01.116 ↗
54. A reinvestigation of the validity of the indentation fracture (IF) method as applied to ceramics10.1016/j.jeurceramsoc.2017.07.027 ↗
55. Toughness measurement on ball specimens. Part II: Experimental procedure and measurement uncertainties10.1016/j.jeurceramsoc.2013.12.052 ↗
56. Fracture toughness of ceramics by the surface crack in flexure method: results from the VAMAS round robin10.1002/9780470314555.ch30 ↗
57. Transformation toughening .3. Experimental-observations in the ZrO2-Y2O3 system10.1007/BF00809059 ↗
58. Mechanical-properties of toughened ZrO2-Y2O3 ceramics10.1111/j.1151-2916.1986.tb04823.x ↗
59. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
60. On a ferroelastic mechanism governing the toughness of metastable tetragonal-prime (t’) yttria-stabilized zirconia10.1098/rspa.2007.1829 ↗
61. Fracture toughness of nanocrystalline tetragonal zirconia with low Yttria content10.1016/S1359-6454(02)00283-5 ↗
62. High toughness ceramics and ceramic composites10.1016/0079-6425(89)90005-4 ↗
63. On the transformation toughening of Y-ZrO2 ceramics with mixed Y-TZP/PSZ microstructures10.1016/S0955-2219(00)00273-9 ↗
64. Microstructure, mechanical properties and low temperature degradation resistance of 2Y-TZP ceramic materials derived from nanopowders prepared by laser vaporization10.1016/j.jeurceramsoc.2015.03.006 ↗
65. Toughness tailoring of yttria-doped zirconia ceramics10.1016/j.msea.2004.03.065 ↗
66. Transformation and microcrack toughening as complementary processes in ZrO2-Toughened Al2O310.1111/j.1151-2916.1986.tb07405.x ↗
67. Significance of internal-stresses for the martensitic-transformation in Yttria-stabilized tetragonal zirconia polycrystals during degradation10.1111/j.1151-2916.1986.tb04789.x ↗
68. Anisotropic thermal-expansion coefficients of Y2o3-stabilized tetragonal zirconia10.1111/j.1151-2916.1986.tb07424.x ↗
69. Cation self-diffusion of Ca-44, Y-88, and Zr-96 in single-crystalline calcia- and yttria-doped zirconia10.1063/1.1628379 ↗
70. Cation diffusion in yttria-zirconia by molecular dynamics10.1016/j.ssi.2011.10.006 ↗
71. Low-temperature degradation increases the cyclic fatigue resistance of 3Y-TZP in bending10.1016/j.dental.2020.05.002 ↗
72. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
73. Reliability assessment in advanced nanocomposite materials for orthopaedic applications10.1016/j.jmbbm.2010.10.010 ↗
74. Fracture variability and R-curve behavior in yttria-stabilized zirconia ceramics10.1023/A:1017923008382 ↗
75. Effect of heat-treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
76. Grain-size-dependent transformation behavior in polycrystalline tetragonal zirconia10.1111/j.1151-2916.1992.tb07832.x ↗