Residual stress induced failure of Ti-6Al-4V/Si3N4 joints brazed with Ag-Cu-Ti filler: The effects of brazing zone’s elasto-plasticity and ceramics' intrinsic properties
Source abstract
Abstract
Abstract The residual-stress induced failure of Ti-6Al-4V/Si3N4 joints brazed with two different Si3N4 ceramics possessing different intrinsic properties was elucidated through experimental and finite-element (FE) thermo-mechanical simulations incorporating the local elasto-plastic properties of the as-received Ag-Cu-Ti filler and the brazing zone characterized by nano-indentation. All tested joints fractured mainly from the ceramics due to residual stress, and their bending strengths increased when using Si3N4 ceramics of higher intrinsic strength. FE-analysis based on the as-received filler’s properties overestimated the nominal bending strengths by approximately 100 MPa in both joints; nano-indentation revealed that the depletion of ductile Ag-Cu phase and growth of hard Cu-Ti intermetallic compounds reduced the plastically deformable thickness after being brazed, whereby they resulted in higher residual stress in the ceramics. Finally, the validity of FE-estimated bending strengths was enhanced when considering the effective plastically deformable thickness of filler (30 μm) instead of the as-received state (50 μm).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Oxidation and corrosion of silicon nitride ceramics with different sintering additives at 1200 and 1500°C in air, water vapour, SO2 and HCl environments – A comparative study10.1016/j.corsci.2008.12.014 ↗
2. Choi · 2006
3. Development of ceramic based 500 N class bipropellant thruster10.2514/6.IAC-05-C4.3.01 ↗
4. Evaluation of the strength of brazed joints in ceramics/metal thruster
5. Solid state bonding of silicon nitride with a nickel interlayer10.1016/0022-5088(90)90431-I ↗
6. Residual stresses and cracking in brittle solids bonded with a thin ductile layer10.1016/0001-6160(88)90305-7 ↗
7. Residual stress cracking of metal/ceramic bonds10.1016/0956-7151(91)90245-V ↗
8. Intermetallics evolution and fracture behavior of Nb interlayer inserted Si3N4/Ti joints brazed with AgCuTi filler10.1016/j.msea.2019.138096 ↗
9. Uncovering the critical factor in determining the residual stresses level in Si3N4–GM filler alloy–42CrMo joints by FEM analysis and experiments10.1016/j.ceramint.2012.06.082 ↗
10. Comparison of three different active filler metals used for brazing ceramic-to-ceramic and ceramic-to-metal10.1002/adem.200500234 ↗
11. Properties and fractography of Si3N4/TiN ceramic joined to steel with active single layer and double layer braze filler alloys10.1016/j.actamat.2004.06.016 ↗
12. Numerical analysis on the residual stress distribution and its influence factor analysis for Si3N4/42CrMo brazed joint10.1016/j.simpat.2019.04.007 ↗
13. Relief of the residual stresses in Si3N4/Invar joints by multi-layered braze structure - Experiments and simulation10.1016/j.ceramint.2016.01.096 ↗
14. Microstructural evolution and mechanical characterization of Nb-interlayer-inserted Ti–6Al–4V/Si3N4 joints brazed with AuNiTi filler10.1016/j.msea.2020.139093 ↗
15. Brazing TC4 alloy to Si3N4 ceramic using nano-Si3N4 reinforced AgCu composite filler10.1016/j.matdes.2015.03.046 ↗
16. Brazing of silicon nitride ceramic composite to steel using SiC-particle-reinforced active brazing alloy10.1016/j.ceramint.2006.03.010 ↗
17. Critical flaw size reduction in commercial Si3N4-TiN composites for wear applications
18. Rangaswamy · 2000
19. Neilsen · 1996
20. Stress singularity of symmetric free-edge joints with elasto-plastic behaviour10.1016/j.commatsci.2011.02.001 ↗
21. Stress singularities at the interface in bonded dissimilar materials under mechanical and thermal loading10.1115/1.2894053 ↗
22. Understanding nanoindentation unloading curves10.1557/JMR.2002.0386 ↗
23. The indentation size effect: A critical examination of experimental observations and mechanistic interpretations10.1146/annurev-matsci-070909-104456 ↗
24. Strain energy distribution in ceramic-to-metal joints10.1016/S1359-6454(01)00352-4 ↗
25. Characterization of the residual stresses and strength of ceramic-metal braze joints10.1115/1.3078305 ↗
26. Thermodynamic modelling of the Ag–Cu–Ti ternary system10.3139/146.110472 ↗
27. Nanostructure of wetting triple line in a Ag–Cu–Ti/Si3N4 reactive system10.1016/S1359-6454(98)00375-9 ↗
28. Microstructural characterization of Si3N4/42CrMo joint brazed with Ag–Cu–Ti + TiNp composite filler10.1016/j.jallcom.2015.08.138 ↗
29. Microstructural evolution of Si3N4/Ti6Al4V joints brazed with nano-Si3N4 reinforced AgCuTi composite filler10.1016/j.vacuum.2017.05.005 ↗
30. Low-temperature interface reaction between titanium and the eutectic silver-copper brazing alloy10.1007/s11669-008-9424-7 ↗
31. Al-Cu-Ti (Aluminum-Copper-Titanium)
32. The Si-Ti-V system (Silicon-Titanium-Vanadium)10.1007/BF02667489 ↗
33. Self-propagating synthesis joining of Cf/Al composites and TC4 alloy using AgCu filler with Ni–Al–Zr interlayer10.1007/s12598-020-01520-3 ↗
34. Crack deflection at an interface between dissimilar elastic materials: Role of residual stresses10.1016/0020-7683(94)90025-6 ↗
35. Effects of non-planarity on the mixed mode fracture resistance of bimaterial interfaces10.1016/0001-6160(89)90017-5 ↗
36. The fracture energy of bimaterial interfaces10.1007/BF02646986 ↗
37. FEM study of the effects of interlayers and creep in reducing residual stresses and strains in ceramic-metal joints10.1016/0961-9526(95)00035-L ↗
38. Correlation of nanoindentation and conventional mechanical property measurements10.1557/PROC-649-Q7.11 ↗