journal article·2021-04

Ultra-high-temperature mechanical behaviors of two-dimensional carbon fiber reinforced silicon carbide composites: Experiment and modeling

Tianbao Cheng

Publisher page

Abstract

Abstract Carbon fiber reinforced silicon carbide (C/SiC) composites are enabling materials for components working in ultra-high-temperature extreme environments. However, their mechanical properties reported in the literature are mainly limited to room and moderate temperatures. In this work, an ultra-high-temperature testing method for the mechanical properties of materials in inert atmosphere is presented based on the induction heating technology. The flexural properties of a 2D plain-weave C/SiC are studied up to 2600 °C in inert atmosphere for the first time. The deformation characteristics and failure mechanisms at elevated temperatures are gained. Theoretical models for the high-temperature Young’s modulus and tensile strength of 2D ceramic matrix composites are then developed based on the mechanical mechanisms revealed in the experiments. The factors contributing to the mechanical behaviors of C/SiC at elevated temperatures are thus characterized quantitatively. The results provide significant understanding of the mechanical behaviors of C/SiC under ultra-high-temperature extreme environment conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Flexural properties of carbon-carbon composites at temperatures up to 2600°C10.1088/2053-1591/ab23c9 ↗
2. Krenkel · 2008
3. Bansal · 2015
4. Low · 2018
5. Bansal · 2005
6. Zhang · 2009
7. Progress in research work of new CMC-SiC
8. Discussion on strategies of sustainable development of continuous fiber reinforced ceramic matrix composites
9. Processing and properties of self-healing C/SiC ceramic matrix composites
10. Comparison of the mechanical hysteresis of carbon/ceramic-matrix composites with different fiber preforms10.1016/j.carbon.2008.12.025 ↗
11. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
12. Phenomenal failure criteria of a plain woven C/SiC composite
13. Experimental investigation on plain woven C/SiC composites under complex stress states
14. An approach to the mechanical behaviour of SiC/SiC and C/SiC ceramic matrix composites: Part 1 Experimental results10.1007/BF02403937 ↗
15. High-temperature flexural properties of SiBC modified C/SiC composites10.1016/j.ceramint.2013.11.072 ↗
16. Flexural performance of 3D-C/SiC composites at high temperature and influence of post-heat-treatment on flexural performance
17. Tensile behavior of a 2D woven C/SiC composite at ambient and elevated temperature
18. Fracture behavior of C/SiC composites at elevated temperature10.1007/s12206-017-0702-3 ↗
19. Tensile behavior of 2D-C/SiC composites at elevated temperatures: Experiment and modeling10.1016/j.jeurceramsoc.2016.11.011 ↗
20. Tensile properties of two-dimensional carbon fiber reinforced silicon carbide composites at temperatures up to 1800°C in air10.1016/j.eml.2019.100546 ↗
21. Tensile properties of two-dimensional carbon fiber reinforced silicon carbide composites at temperatures up to 2300°C10.1016/j.jeurceramsoc.2019.10.030 ↗
22. Fracture strength behaviors of ultra-high-temperature materials10.1115/1.4045046 ↗
23. Compressive strength and damage mechanisms of 2D-C/SiC composites at high temperatures10.1016/j.ceramint.2018.04.255 ↗
24. Failure and strength of 2D-C/SiC composite under in-plane shear loading at elevated temperatures10.1016/j.matdes.2011.02.054 ↗
25. Temperature dependency of interlaminar shear strength of 2D-C/SiC composite10.1016/j.matdes.2011.10.048 ↗
26. The dynamic tensile properties of 2D-C/SiC composites at elevated temperatures10.1016/j.ijimpeng.2014.10.006 ↗
27. An investigation of dynamic failure progress and properties of 2D C/SiC composite from 173K to 1273K by SHTB10.1016/j.compositesb.2017.02.009 ↗
28. Research on mechanical behavior of 2D C/SiC composites at elevated temperature under uniaxial compression
29. Compressive behavior of C/SiC composites over a wide range of strain rates and temperatures10.1016/j.carbon.2013.06.044 ↗
30. Effects of frequency on fatigue behavior of CVI C/SiC at elevated temperature10.1016/j.compscitech.2005.06.020 ↗
31. Experimental investigation on the fatigue characteristics about high temperature of plain-woven C/SiC composite
32. The properties of fibre composites
33. Matrix fracture in fiber-reinforced ceramics10.1016/0022-5096(86)90035-9 ↗
34. The mechanics of matrix cracking in brittle-matrix fiber composites10.1016/0001-6160(85)90124-5 ↗
35. Tensile tests of ceramic-matrix composites: Theory and experiment10.1111/j.1151-2916.1990.tb05273.x ↗
36. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
37. Relationships between hysteresis measurements and the constituent properties of ceramic matrix composites: I, Theory10.1111/j.1151-2916.1995.tb08046.x ↗
38. Ablation behavior of C/SiC composites in plasma wind tunnel10.1016/j.carbon.2016.02.085 ↗
39. Carbon fiber reinforced silicon carbide composite-based sharp leading edges in high enthalpy plasma flows10.1016/j.compositesb.2017.09.060 ↗
40. The tensile behavior of carbon fibers at high temperatures up to 2400°C10.1016/j.carbon.2003.11.020 ↗
41. Thermomechanical properties of carbon fibres at high temperatures (up to 2000°C)10.1016/S0266-3538(01)00140-3 ↗
42. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
43. Material properties of a sintered α-SiC10.1063/1.556000 ↗
44. Transverse and longitudinal coefficient of thermal expansion of carbon fibers at high temperatures (300–2500K)10.1016/j.carbon.2008.07.035 ↗
45. Microstructure and high-temperature strength of silicon carbide with 2000 ppm yttria10.1016/j.jeurceramsoc.2017.07.002 ↗
46. Nanohardness and elastic modulus of pyrocarbon
47. The in-situ modulus of carbon fiber bundle in C/SiC composites based on finite element computational micromechanics
48. Measurement and calculation of thermal residual stress in fiber reinforced ceramic matrix composites10.1016/j.compscitech.2008.08.015 ↗
49. Finite element simulation of interface shear strength of C/SiC composites with thermal residual stress
50. Wang · 2003
51. The temperature-dependent surface energy of ceramic single crystals10.1111/jace.14689 ↗
52. Damage evolution and microstructural characterization of a cross-woven C/SiC composite under tensile loading
53. Yuan · 2009
54. Experiments on fatigue damage failure test of carbon fiber yarn
55. Damage of carbon fiber during the preparing of Cf/SiC composites
56. Weibull strength scaling for standardized rectangular flexure specimens10.1111/j.1151-2916.2003.tb03329.x ↗
57. The direct uniaxial tensile strength of chemical vapor deposited zinc sulfide from room temperature to 600°C10.1016/j.matlet.2015.05.161 ↗
58. Reliability analysis of 2D C/SiC composite
59. Study on Weibull modulus of flexural strength for SiC at elevated temperatures
60. Understanding the ultra-high-temperature mechanical behaviors of advanced two-dimensional carbon-carbon composites10.1016/j.ceramint.2020.05.237 ↗
61. Application of weakest-link fracture statistics to fiber-reinforced ceramic-matrix composites10.1111/j.1151-2916.1997.tb03013.x ↗
62. Luo · 2014