journal article·2020-09

A promising molten silicate resistant material: Rare-earth oxy-apatite RE9.33(SiO4)6O2 (RE = Gd, Nd or La)

Han Zhang, Jie Lu, Xiao Shan, Di Wu, Xiaofeng Zhao, Fangwei Guo, Ping Xiao

Publisher page

Abstract

Abstract In this work we reported a new class of rare earth oxy-apatite, RE9.33(SiO4)6O2, with superior molten silicate resistant capability which shows promising application for thermal barrier coatings (TBCs). Three RE elements with different ion radius, i.e., Gd, Nd and La, were selected to prepare RE9.33(SiO4)6O2 bulk using co-precipitation and pressless-sintering. After 8-h CMAS attack at 1300 °C, the specimens exhibited a dense, continuous reprecipitated layer at RE-apatite/CMAS interface, which is predominantly controlled by a dissolution-reprecipitation mechanism distinguishing from the sacrificial material which is usually with reaction layer being formed. With an increase of ion radius, apatite is easier to crystallize in the melt.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Thermal barrier coating materials10.1016/S1369-7021(05)70934-2 ↗
3. Emerging materials and processes for thermal barrier systems10.1016/j.cossms.2004.03.009 ↗
4. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
5. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
6. A delamination mechanism for thermal barrier coatings subject to calcium–magnesium–alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
7. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
8. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part II, β-Yb2Si2O7 and β-Sc2Si2O710.1016/j.jeurceramsoc.2018.03.010 ↗
9. W.C. Hasz, C.A. Johnson, M.P. Borom, inventors; General Electric Company, assignee. Protection of Thermal Barrier Coating with an Impermeable Barrier Coating. United States patent 5871820. 16 February 1999.
10. A comparative study on hot corrosion resistance of three types of thermal barrier coatings: YSZ, YSZ+Al2O3 and YSZ/Al2O310.1016/j.msea.2007.06.001 ↗
11. In situ synthesis of α-alumina layer on thermal barrier coating for protection against CMAS (CaO-MgO-Al2O3-SiO2) corrosion10.1016/j.surfcoat.2014.11.064 ↗
12. Research of in situ modified PS-PVD thermal barrier coating against CMAS (CaO-MgO-Al2O3-SiO2) corrosion10.1016/j.ceramint.2015.10.106 ↗
13. Protectiveness of Pt and Gd2Zr2O7 layers on EB-PVD YSZ thermal barrier coatings against calcium–magnesium–alumina–silicate (CMAS) attack10.1016/j.ceramint.2015.05.128 ↗
14. CMAS (CaO-MgO-Al2O3-SiO2) resistance of Y2O3-stabilized ZrO2 thermal barrier coatings with Pt layers10.1016/j.ceramint.2017.09.197 ↗
15. CMAS-resistant thermal barrier coatings (TBC)10.1111/j.1744-7402.2009.02373.x ↗
16. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
17. Effects of cation substitution and temperature on the interaction between thermal barrier oxides and molten CMAS10.1016/j.jeurceramsoc.2014.09.006 ↗
18. Degradation of La2Zr2O7 and other novel EB-PVD thermal barrier coatings by CMAS (CaO-MgO-Al2O3-SiO2) and volcanic ash deposits10.1016/j.surfcoat.2013.07.029 ↗
19. Molten silicate interactions with thermal barrier coatings10.1016/j.surfcoat.2014.04.007 ↗
20. Hot corrosion behavior of LaMgAl11O19 ceramic coated with molten CMAS deposits at temperature of 1250 °C in air10.1016/j.jallcom.2016.05.272 ↗
21. Plasma sprayed nanostructured GdPO4 thermal barrier coatings: preparation microstructure and CMAS corrosion resistance10.1111/jace.14924 ↗
22. Calcium-magnesium-alumina-silicate (CMAS) resistance characteristics of LnPO4 (Ln = Nd, Sm, Gd) thermal barrier oxides10.1016/j.jeurceramsoc.2016.08.013 ↗
23. Calcium-magnesium alumino-silicate interaction with yttrium monosilicate environmental barrier coatings10.1111/j.1551-2916.2010.03916.x ↗
24. Hot corrosion behaviour of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
25. Calcium–magnesium aluminosilicate (CMAS) reactions and degradation mechanisms of advanced environmental barrier coatings10.1016/j.surfcoat.2013.08.036 ↗
26. Thermal conductivity of the gadolinium calcium silicate apatites: effect of different point defect types10.1016/j.actamat.2011.03.008 ↗
27. Reinvestigation of phase relations around the oxyapatite phase in the Nd2O3–SiO2 system10.1016/S0022-0248(02)01908-5 ↗
28. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings
29. Effect of microstructure on early oxidation of MCrAlY coatings10.1016/j.actamat.2018.08.018 ↗
30. Structural evolution and thermal conductivities of (Gd1−xYbx)2Zr2O7 (x = 0, 0.02, 0.04, 0.06, 0.08, 0.1) ceramics for thermal barrier coatings10.1016/j.ceramint.2015.06.090 ↗
31. Interaction of yttrium disilicate environmental barrier coatings with calcium-magnesium-iron alumino-silicate melts10.1016/j.actamat.2017.12.004 ↗
32. Phase equilibria in the calcia-gadolinia-silica system10.1016/j.jallcom.2016.10.263 ↗
33. Microstructure formation and evolution in composites during liquid-phase sintering10.1007/s11106-013-9480-3 ↗
34. The microstructures of silicon nitride ceramics during hot-pressing transformations
35. Enthalpies of formation of lanthanide oxyapatite phases10.1557/JMR.2001.0381 ↗
36. Crystal structure of apatite type rare-earth silicate (Sr2RE2)(RE6)(SiO4)6O2 (RE = La, Pr, Tb, Tm, and Y)10.1111/j.1551-2916.2011.04388.x ↗
37. Electrical properties of new type high oxide ionic conductor RE10Si6O27 (RE = La, Pr, Nd, Sm, Gd, Dy)10.1016/S0955-2219(98)00032-6 ↗
38. Forces between aluminum oxide grains in a silicate melt and their effect on grain boundary wetting10.1111/j.1151-2916.1991.tb06791.x ↗
39. Hertzian-crack suppression in ceramics with elastic-modulus-graded surfaces10.1111/j.1151-2916.1998.tb02625.x ↗
40. Gradients in elastic modulus for improved contact-damage resistance. Part I: the silicon nitride–oxynitride glass system10.1016/S1359-6454(01)00200-2 ↗
41. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part I, YAlO3 and γ-Y2Si2O710.1016/j.jeurceramsoc.2018.03.021 ↗
42. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
43. Effects of crystal structure and cation size on molten silicate reactivity with environmental barrier coating materials10.1111/jace.16694 ↗
44. Mullite whisker reinforced porous anorthite ceramics with low thermal conductivity and high strength10.1016/j.jeurceramsoc.2015.10.002 ↗
45. Thermal expansion of lanthanum silicate oxyapatite (La9.33+2x(SiO4)6O2+3x), lanthanum oxyorthosilicate (La2SiO5) and lanthanum sorosilicate (La2Si2O7)10.1016/j.jssc.2012.04.043 ↗