journal article·2024-01

Atomic level out-diffusion and interfacial reactions of MAX phases in contact with metals and air

Chaosheng Ma, Wenbo YU, Yihu Ma, Guozheng Ma, Haidou Wang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. The MAX phases: unique new carbide and nitride materials - ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and lightweight10.1511/2001.28.334 ↗
2. The MN+1AXN phases: a new class of solids: thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
3. Fully reversible, dislocation-based compressive deformation of Ti3SiC2 to 1GPa10.1038/nmat814 ↗
4. Effect of microstructure anisotropy on the deformation of MAX polycrystals studied by in-situ compression combined with neutron diffraction10.1063/1.4884601 ↗
5. Dislocation analysis of Ti2AlN deformed at room temperature under confining pressure10.1080/14786435.2012.715250 ↗
6. Evidence of dislocation cross-slip in MAX phase deformed at high temperature10.1038/srep06358 ↗
7. Dislocation modelling in Ti2AlN MAX phase based on the Peierls-Nabarro model10.1080/14786435.2015.1066938 ↗
8. Two-dimensional nanocrystals produced by exfoliation of Ti3AlC210.1002/adma.201102306 ↗
9. New two-dimensional niobium and vanadium carbides as promising materials for Li-Ion batteries10.1021/ja405735d ↗
10. Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon10.1021/cm030022v ↗
11. Microstructure evolution and bonding mechanism of Ti2SnC-Ti6Al4V joint by using Cu pure foil interlayer10.1016/j.matchar.2017.01.035 ↗
12. Prediction of the stability of the M(n+1)AX(n) phases from first principles10.1103/PhysRevB.80.214113 ↗
13. Temperature dependent phase stability of nanolaminated ternaries from first-principles calculations10.1016/j.commatsci.2014.04.055 ↗
14. High temperature damping behavior and dynamic Young's modulus of magnesium matrix composite reinforced by Ti2AlC MAX phase particles10.1016/j.mechmat.2018.12.001 ↗
15. Oxidation of Ti2AlC bulk and spray deposited coatings10.1016/j.corsci.2010.08.004 ↗
16. Element replacement approach by reaction with Lewis acidic molten salts to synthesize nanolaminated MAX phases and MXenes10.1021/jacs.9b00574 ↗
17. Two-dimensional nanosheets of titanium carbonitride Ti3CNTx MXene for microwave absorption in the X and Ku bands10.1021/acsanm.2c04062 ↗
18. New insight into the helium-induced damage in MAX phase Ti3AlC2 by first-principles studies10.1063/1.4931398 ↗
19. First principles investigation of point defect-related properties in Ti2AlN10.1039/C4RA07200F ↗
20. Large grain-boundary magnetoresistance in MnFe2O4 nanoparticle compact10.1016/j.jmmm.2007.05.023 ↗
21. Insights into high temperature oxidation of Al2O3-forming Ti3AlC210.1016/j.corsci.2012.01.011 ↗
22. First-principles investigation of intrinsic defects and (N, O) impurity atom stimulated Al vacancy in Ti2AlC10.1063/1.3058718 ↗
23. Role of the A-Element in the structural, mechanical, and electronic properties of Ti(3)AC(2) MAX Phases10.1021/acs.inorgchem.1c03358 ↗
24. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu–Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
25. Fabrication and mechanical properties of pressureless melt infiltrated magnesium alloy composites reinforced with TiC and Ti2AlC particles10.1016/j.msea.2014.09.039 ↗
26. Synthesis and characterization of the mechanical properties of Ti3SiC2/Mg and Cr2AlC/Mg alloy composites10.1016/j.msea.2017.08.068 ↗
27. A review of novel ternary nano-layered MAX phases reinforced AZ91D magnesium composite10.1016/j.jma.2022.05.013 ↗
28. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
29. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
30. Oxidation behavior of Cr(2)AlC ceramics at 1,100 and 1,250 degrees C10.1007/s10853-008-2516-2 ↗
31. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
32. Oxidation of Cr2AlC at 1300 degrees C in air10.1016/j.corsci.2007.03.044 ↗
33. Oxidation behavior of Ti3AlC2 at 1000–1400 °C in air10.1016/S0010-938X(02)00177-4 ↗
34. Oxidation of Cr2AlC Between 900 and 1200 °C in Air10.1007/s11085-007-9071-0 ↗
35. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
36. High temperature healing of Ti2AlC: On the origin of inhomogeneous oxide scale10.1016/j.scriptamat.2011.03.031 ↗
37. Oxidation of Tin+1AlXn (n=1-3 and X = C, N) - I. Model10.1149/1.1380255 ↗
38. Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics10.1016/j.actamat.2011.03.035 ↗
39. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
40. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
41. Healing performance of Ti2AlC ceramic studied with in situ microcantilever bending10.1016/j.jeurceramsoc.2012.09.012 ↗
42. Self-healing performance of Ti2AlC ceramic10.1039/c2jm16123k ↗
43. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
44. Joining of Ti–Al–C ceramics by oxidation at low oxygen partial pressure10.1016/j.jeurceramsoc.2009.03.014 ↗
45. Frank partial dislocation in Ti2AlC-MAX phase induced by matrix-Cu diffusion10.1016/j.scriptamat.2020.09.007 ↗
46. Thermal stability of Ti3SiC2 thin films10.1016/j.actamat.2006.10.010 ↗
47. Oxidation mechanisms in bulk Ti2AlC: Influence of the grain size10.1016/j.jeurceramsoc.2020.01.042 ↗
48. On the effect of texture on the mechanical and damping properties of nanocrystalline Mg-matrix composites reinforced with MAX phases10.1016/j.msea.2010.01.073 ↗
49. Interfacial microstructure and properties of brazed joints of Ti3SiC2 ceramic and TC4 alloy
50. In situ formed TiCx in high chromium white iron composites: formation mechanism and influencing factors10.1016/j.jallcom.2019.02.292 ↗
51. Powder metallurgy processing and compressive properties of Ti3AlC2/Al composites10.1016/j.msea.2011.09.068 ↗
52. Processing and mechanical properties of Ti2AlC MAX phase reinforced AE44 magnesium composite10.3390/ma13040995 ↗
53. Synthesis and characterization of textured Ti2AlC reinforced magnesium composite10.1016/j.jallcom.2017.09.303 ↗
54. Joining Ti3SiC2 MAX phase with 308 stainless steel and aluminum fillers by tungsten inert gas (TIG)-brazing process10.1016/j.ceramint.2015.09.026 ↗
55. Plasma spray of Ti2AlC MAX phase powders: Effects of process parameters on coatings' properties, Surface and Coatings Technology
56. Alleviating delamination of Ti2AlC coating upon oxidation at 600 °C with heavy incorporation of TiC10.1016/j.jallcom.2019.03.236 ↗
57. Isothermal oxidation of the Ti2AlC MAX phase coatings deposited by kerosene-fuelled HVOF spray10.1016/j.corsci.2018.04.022 ↗
58. Kerosene-fuelled high velocity oxy-fuel (HVOF) spray of Ti2AlC MAX phase powders10.1016/j.jallcom.2017.11.157 ↗
59. Cold-spray deposition of Ti2AlC coatings10.1016/j.vacuum.2013.01.023 ↗
60. Cold spray deposition of Ti2AlC coatings for improved nuclear fuel cladding10.1016/j.jnucmat.2015.06.028 ↗
61. Development of the phase composition and the properties of Ti2AlC and Ti3AlC2 MAX-phase thin films – a multilayer approach towards high phase purity10.1016/j.apsusc.2020.147864 ↗
62. Direct deposition of extremely low interface-contact-resistant Ti2AlC MAX-phase coating on stainless-steel by mid-frequency magnetron sputtering method10.1016/j.jeurceramsoc.2020.02.033 ↗
63. Diffusion-controlled intercalation approach to synthesize the Ti2AlC MAX phase coatings at low temperature of 550 °C10.1016/j.apsusc.2019.144130 ↗
64. Cathodic arc co-deposition of highly oriented hexagonal Ti and Ti2AlC MAX phase thin films10.1016/j.tsf.2010.09.007 ↗
65. Microstructural analysis of in-situ reacted Ti2AlC MAX phase composite coating by laser cladding10.1016/j.surfcoat.2020.125360 ↗
66. Ag/Ti3AlC2 composites with high hardness, high strength and high conductivity10.1016/j.matlet.2017.11.038 ↗
67. Processing, microstructural characterization and mechanical properties of a Ti2AlC/nanocrystalline Mg-matrix composite10.1016/j.compscitech.2008.11.007 ↗
68. Contact-reactive brazing of Ti3SiC2 ceramic to TC4 alloy using a Ni interlayer: Interfacial microstructure and joining properties10.1016/j.ceramint.2018.04.006 ↗
69. Interfacial microstructure and mechanical properties of TC4/Ti3SiC2 contact-reactive brazed joints using a Cu interlayer10.1016/j.ceramint.2018.08.328 ↗
70. C.S. Ma, W.B. Yu, G.Z. Ma, H.D. Wang, Recent progress on high temperature radar absorbing coatings (RACs): a review, CRITICAL REVIEWS IN SOLID STATE AND MATERIALS SCIENCES.
71. Intermediate-temperature oxidation behavior of Ti2AlC in air10.1557/JMR.2002.0431 ↗
72. Oxidation of Tin+1AlXn (n=1-3 and X = C, N) - II. Experimental results10.1149/1.1380256 ↗
73. Early stages of oxidation of Ti3AlC2 ceramics10.1016/j.matchemphys.2008.06.038 ↗
74. Ultra-high temperature ablation behavior of Ti2AlC ceramics under an oxyacetylene flame10.1016/j.jeurceramsoc.2010.11.035 ↗
75. Kinetic aspects of Ti2AlC MAX phase oxidation10.1007/s11085-015-9526-7 ↗
76. Long-term oxidation of Ti2AlC in air andwater vapor at 1000-1300 degrees c temperature range10.1149/2.052202jes ↗
77. Oxygen incorporation in M2AlC (M=Ti, V, Cr)10.1016/j.actamat.2012.05.011 ↗
78. Mechanism for breakaway oxidation of the Ti2AlC MAX phase10.1016/j.actamat.2021.117025 ↗
79. A new strategy for long-term complex oxidation of MAX phases: Database generation and oxidation kinetic model establishment with aid of machine learning10.1016/j.actamat.2022.118378 ↗
80. Studying the oxidation of Ti2AlC MAX phase in atmosphere: A review10.1016/j.ijrmhm.2016.07.006 ↗
81. The MN+ 1AXN phases: A new class of solids10.1016/S0079-6786(00)00006-6 ↗
82. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu-Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
83. Oxygen diffusivity in alumina scales grown on Al-MAX phases10.1016/j.corsci.2014.11.030 ↗
84. Microstructures and adhesion of the oxide scale formed on titanium aluminum carbide substrates10.1111/j.1551-2916.2006.01141.x ↗
85. Environmental resistance of Cr2AlC MAX phase under thermal gradient loading using a burner rig10.1111/jace.15425 ↗
86. Oxidation resistance of Ti3AlC2 and Ti3Al0.8Sn0.2C2 MAX phases: a comparison10.1111/jace.16780 ↗
87. Oxidation of Al2O3 scale-forming MAX phases in turbine environments10.1007/s11661-017-4346-9 ↗
88. Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.510.1007/s11661-006-0243-3 ↗
89. R. Morrell, Handbook of properties of technical & engineering ceramics, Handbook of properties of technical & engineering ceramics1985.
90. A first-principles investigation of the phase stability of Ti2AlC with Al vacancies10.1016/j.scriptamat.2007.09.048 ↗
91. TEM study of the initial oxide scales of Ti2AlC10.1016/j.actamat.2011.04.058 ↗
92. Lide · 2001
93. Yang · Oxid. REsistance Improvement Tial Intermetallics Using Surf. Modif., 台大工程 · 2003 · 89
94. Electronic structure and chemical bonding in Ti2AlC investigated by soft x-ray emission spectroscopy10.1103/PhysRevB.74.195108 ↗
95. Oxidation behavior of Ti3AlC2 at 1000-1400 degrees C in air10.1016/S0010-938X(02)00177-4 ↗
96. Microstructure and properties of Ti3AlC2 prepared by the solid-liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
97. High-temperature oxidation behavior of Ti3AlC2 in air10.1016/S1003-6326(06)60318-X ↗
98. Oxidation of tic at low-temperatures10.1007/BF01107214 ↗
99. Thermodynamic aspects of tial and TISI2 oxidation - the AL-TI-O AND SI-TI-O phase-diagrams10.1007/BF00666500 ↗
100. Stability of protective oxide-films on TI-base alloys10.1007/BF01151593 ↗