Abstract
This work deals with the mechanical behavior of a zirconia ceramic doped with 1.5 mol% of yttria, recently developed by Tosoh (Japan). The results show that this material offers an attractive combination of strength (1 GPa) and toughness (8.5 MPa√m), near the optimum between a brittle and ductile behavior. This is attributed to the crack shielding effect of phase transformation toughening mechanism, which is here more developed compared to conventional 3Y-TZP. Moreover, a relatively high Weibull modulus of 16 and a significant crack growth resistance were observed. It was also shown that the obtained slow crack growth threshold (5.6 MPa√("m" )) is roughly twice that of 3Y-TZP. A qualitative investigation showed that phase transformation also occurred during impact testing, which is promising for the impact resistance of this material. Although tough and strong, the material exhibits a high resistance to aging compared to standard 3Y-TZP.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Transformation toughening in zirconia containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
2. Fourty years after the promise of " ceramic steel? ": zirconia-based composites with a metal-like mechanical behavior10.1111/jace.16903 ↗
3. Review-transformation toughening in ceramics: martensitic transformations in crack-tip stress fields10.1111/j.1151-2916.1980.tb10712.x ↗
4. Clinical trials in zirconia: a systematic review
5. Fracture toughness of zirconia from a shallow notch produced by ultra-short pulsed laser ablation10.1016/j.jeurceramsoc.2014.05.009 ↗
6. Fracture behavior of Ce TZP/Alumina/Aluminate composites with different amounts of transformation toughening. Influence of the testing methods10.1016/j.jeurceramsoc.2017.09.052 ↗
7. Grain size dependence of toughness and transformability of 2 mol% Y-TZP ceramics10.1007/BF01742233 ↗
8. Effect of heat-treatment on grain size phase assemblage, and mechanical properties of 3 mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
9. R-curve behaviour of 2Y-TZP with submicron grain size10.1016/j.jeurceramsoc.2005.11.012 ↗
10. Toughening of yttria-stabilised tetragonal zirconia ceramics10.1179/174328005X41113 ↗
11. Warm pressing of zirconia nanoparticles by the spark plasma sintering technique10.1016/j.scriptamat.2008.02.015 ↗
12. High fracture toughness of 3Y-TZP ceramic over a wide sintering range10.1016/j.matchemphys.2020.122693 ↗
13. Low-temperature processing and mechanical properties of zirconia and zirconia-alumina nanoceramics10.1111/j.1151-2916.2003.tb00015.x ↗
14. Determination of fracture toughness of Y-TZP ceramics10.1016/j.ceramint.2017.09.004 ↗
15. Higher fracture toughness of tetragonal zirconia ceramics through nanocrystalline structure10.1016/j.scriptamat.2009.03.019 ↗
16. Effects of stabilizer content and sintering conditions on Y-TZP ceramics made from stabilizer coated nanopowders
17. Inelastic deformation of Mg-PSZ and its significance for strength-toughness relationship of zirconia toughened ceramics10.1016/0001-6160(85)90131-2 ↗
18. Alumina toughened zirconia from yttria coated powders10.1016/j.jeurceramsoc.2012.03.014 ↗
19. Fracture toughness and mechanical strength of Y-TZP/PSZ ceramics10.1016/S1359-6462(01)01020-X ↗
20. Towards long lasting zirconia-based composites for dental implants, Part I: innovative synthesis, microstructural characterization and in vitro stability10.1016/j.biomaterials.2015.01.018 ↗
21. Towards long lasting zirconia-based composites for dental implants: Transformation induced plasticity and its consequence on ceramic reliability10.1016/j.actbio.2016.11.040 ↗
22. Forty years after the promise of "ceramic steel?": Zirconia‐based composites with a metal‐like mechanical behavior10.1111/jace.16903 ↗
23. TOSOH, “Technical Data Sheet Zgaia™ 1 .5Y-HT,” Version 2.1, December 2021.
24. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
25. Fracture toughness of nanocrystalline tetragonal zirconia with low yttria content10.1016/S1359-6454(02)00283-5 ↗
26. K. Matsui, K. Hosoi, B. Feng, H. Yoshida, Y. Ikuhara, Ultrahigh toughness polycrystalline ceramics without fading of strength, arXiv:2112.14372 [cond-mat.mtrl-sci], 2021. https://doi.org/10.48550/arXiv.2112.14372.
27. Mechanical properties of toughened ZrO2-Y2O310.1111/j.1151-2916.1986.tb04823.x ↗
28. Y-TZP ceramics with optimized toughness: new results10.1016/j.jallcom.2004.02.014 ↗
29. Y-TZP ceramics with tailored toughness
30. Critical influence of alumina content on the low temperature degradation of 2–3 mol% yttria-stabilized TZP for dental restorations10.1016/j.jeurceramsoc.2014.09.018 ↗
31. Thermal shock resistance of Y-TZP with Palmqvist10.1016/S0955-2219(02)00065-1 ↗
32. Fracture variability and R-curve behavior in yttria-stabilized zirconia ceramics10.1023/A:1017923008382 ↗
33. Average grain size in polycrystalline10.1111/j.1151-2916.1969.tb11975.x ↗
34. Phase analysis in Zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
35. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays
36. A 3-balls-on-3-balls strength test for ceramic disks10.1016/j.jeurceramsoc.2006.02.033 ↗
37. Fracture toughness of ceramics using the sevnb method: first results of a joint VAMAS/ESIS round robin10.1002/9780470294567.ch57 ↗
38. Measurement of rising R-curve behavior in toughened silicon nitride by stable crack propagation in bending10.1111/j.1151-2916.1995.tb09092.x ↗
39. Wide range stress intensity factor expressions of ASTM E 399 standard fracture toughness specimens10.1007/BF00032844 ↗
40. Double torsion testing a 3Y-TZP Ceramic10.1016/0272-8842(95)00076-3 ↗
41. A method for evaluating the time-dependent failure characteristics of brittle materials and its applications to polycrystalline alumina10.1007/BF00550196 ↗
42. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
43. The double-torsion testing technique for determination of fracture toughness and slow crack growth behavior of materials: A review10.1007/s10853-005-5553-0 ↗
44. A simple method for studying slow crack growth10.1520/JTE10015J ↗
45. Chevalier · Bioceramics · 1997 · 10 · 135
46. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
47. Unbiased estimation of Weibull modulus using linear least squares analysis—A systematic approach10.1016/j.jeurceramsoc.2016.07.008 ↗
48. Strength and reliability of surface treated YTZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
49. Influence of precracking procedure, environment, temperature and microstructure on R-curve behavior of alumina and PSZ10.1016/0955-2219(93)90005-C ↗
50. Introduction to a tough, strong and stable Ce-TZP/MgAl2O4 composite for biomedical applications10.1016/j.jeurceramsoc.2012.02.002 ↗
51. B. Lawn, Fracture of Brittle Solids, second edition, Cambridge University Press, Cambridge, 1993.10.1017/CBO9780511623127 ↗
52. Crack growth resistance of alumina, zirconia, and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
53. Crack propagation behavior of alumina with different grain sizes under static and cyclic fatigue10.4028/www.scientific.net/KEM.317-318.449 ↗
54. Slow crack growth and hydrothermal aging stability of an alumina-toughened zirconia composite made from La2O3-doped 2Y-TZP10.1016/j.jeurceramsoc.2016.11.003 ↗
55. Subcritical crack growth in ceramics
56. Effect of loading configuration on strength values in a highly transformable zirconia-based composite10.1016/j.dental.2016.06.023 ↗
57. Mechanical behaviour of extremely tough tzp bioceramics10.1016/j.jmbbm.2018.11.001 ↗
58. Phase transformation induces plasticity with negligible damage in ceria-stabilized zirconia-based ceramics10.1016/j.actamat.2019.10.046 ↗
59. Mechanics of transformation-toughening in brittle materials10.1111/j.1151-2916.1982.tb10426.x ↗
60. X-Ray determination of transformation depths in ceramics containing tetragonal ZrO210.1111/j.1151-2916.1981.tb10285.x ↗
61. Slow crack growth resistance of electrically conductive zirconia-based composites with non-oxide reinforcements10.1016/j.jeurceramsoc.2018.09.034 ↗
62. Large increase in fracture resistance of stishovite with crack extension less than one micrometer10.1038/srep10993 ↗
63. R-curve behavior of 3Y-TZP at cryogenic temperatures10.1111/j.1551-2916.2011.04711.x ↗
64. Crack propagation and fatigue in zirconia-based composites, Composites Part A: Applied Science and Manufacturing
65. Slow crack-growth behavior of alumina ceramics10.1557/JMR.2000.0024 ↗
66. Strength limitations of transformation-toughened zirconia alloys10.1111/j.1151-2916.1986.tb04785.x ↗
67. Ashby · 2005
68. Effects of grain size and ceria addition on Ageing behavior and tribological properties of Y-TZP ceramics10.1016/S0955-2219(97)00153-2 ↗
69. Hydrothermal aging behavior of nanocrystalline Y-TZP Ceramics10.1111/j.1551-2916.2010.04341.x ↗
70. Effect of alumina addition on the tetragonal-to-monoclinic phase transformation in zirconia- 3 mol% Yttria10.1111/j.1151-2916.1991.tb06905.x ↗