journal article·2009-05

Suppression of grain growth in sub-micrometer alumina via two-step sintering method

Z. Razavi Hesabi, M. Haghighatzadeh, Mehdi Mazaheri, Dusan Galusek, S.K. Sadrnezhaad

Publisher page

Abstract

Abstract Two-step sintering (TSS) was applied to suppress the accelerated grain growth of sub-micron (∼150 nm) alumina powder. The application of an optimum TSS regime led to a remarkable decrease of grain size down to ∼500 nm; while the grain size of the full-dense structures produced by conventional sintering ranged between 1 and 2 μm. To find how important the temperatures at sintering steps might be, several TSS regimes were conducted. The results showed that the temperatures at both sintering steps play vital roles in densification and grain growth of the alumina compacts. Based on the results, the optimum regime consisted of heating the green bodies up to 1250 °C (first step) and then holding at 1150 °C for more than 60 h (second step). This yielded the finest microstructure with no deterioration of the densification. Heating at 1300 °C (first step) and then at 1200 °C (second step) was not a successful procedure. Lowering the temperature of the second step down to 1100 °C resulted in exhaustion of the densification at 88% -theoretical density. A nearly full-dense structure with an average grain size of 850 nm was obtained when the temperature of the second step was increased to 1150 °C. Empirical results show that not only the first step temperature has to be high enough to reach a structure containing unstable pores, but the second sintering temperature must also be high enough to activate the densification mechanism without grain growth. This means that a considerable densification at the first step does not imply enough second-step densification.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Mechanical properties of an ultrafine-grained Al—7.5 pct Mg alloy10.1007/s11661-003-0095-z ↗
2. Yield stress of fine grained materials10.1016/S1359-6454(98)00150-5 ↗
3. The influence of shaping method on the grain size dependence of strength in dense submicrometre alumina10.1016/0955-2219(96)00044-1 ↗
4. Processing and properties of nanophase ceramics
5. Stability of nanostructured metals and alloys10.1016/j.scriptamat.2004.05.014 ↗
6. Influence of the second-phase particle size on grain growth based on computer simulation10.1016/S0921-5093(99)00177-X ↗
7. Mazaheri, M., Valefi, M., Razavi Hesabi, Z., and Sadrnezhaad, S. K., Two-step sintering of nanocrystalline 8Y2O3 stabilized ZrO2 synthesized by glycine nitrate peocess. Ceramics International, in press.
8. Mechanaical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
9. Colloidal processing and sintering of nanosized transition aluminas10.1016/j.powtec.2005.05.015 ↗
10. The principles of grain refinement in equal-channel angular pressing10.1016/j.msea.2006.02.473 ↗
11. Using ECAP to achieve grain refinement, precipitate fragmentation and high strain rate superplasticity in a spraycast aluminum alloy10.1016/S1359-6454(03)00433-6 ↗
12. Effect of nanopowder deagglomeration on the densities of nanocrystalline ceramic green bodies and their sintering behavior10.1016/S0965-9773(99)00348-7 ↗
13. From powders to sintered pieces: forming, transformations and sintering of nanostructured ceramic oxides10.1016/S0032-5910(02)00183-3 ↗
14. Processing of high-density submicrometer Al2O3 for new applications10.1111/j.1151-2916.2003.tb03339.x ↗
15. Effects of the homogeneity of particle coordination on solid-state sintering of transparent alumina10.1111/j.1551-2916.2006.00985.x ↗
16. Phase stability, microstructural evolution and room temperature mechanical properties of TiO2 doped 8mol% Y2O3 stabiized ZrO2 (8Y-CSZ)10.1016/j.ceramint.2006.10.015 ↗
17. Influence of MgO or TiO2 doping on the sintering path and on the optical properties of a submicronic alumina material10.1016/j.scriptamat.2007.01.047 ↗
18. Spark plasma sintering of magnesia-doped alumina with high hardness and fracture toughness10.1111/j.1551-2916.2007.02094.x ↗
19. Grain growth controlled by mobile particles on grain boundaries10.1016/j.scriptamat.2006.04.006 ↗
20. Sintering dense nanocrystalline ceramics without final-stage grain growth10.1038/35004548 ↗
21. Densification and grain growth of Al2O3 nanoceramics during pressureless sintering10.1111/j.1551-2916.2005.00654.x ↗
22. Fracture toughness (KIC), hardness, sintering and grain growth behavior of 8YSCZ/Al2O3 composites produced by colloidal processing10.1016/j.jallcom.2004.08.084 ↗
23. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
24. Two-step sintering of nanocrystalline ZnO compacts: effect of temperature on densification and grain growth10.1111/j.1551-2916.2007.02029.x ↗
25. Two-stage sintering of alumina with submicrometer grain size10.1111/j.1551-2916.2006.01408.x ↗
26. Spark plasma sintering of alumina10.1111/j.1151-2916.2002.tb00381.x ↗