journal article·2011-05Open access

Ultra-high temperature ablation behavior of Ti2AlC ceramics under an oxyacetylene flame

G.M. Song, S.B. Li, C.X. Zhao, W.G. Sloof, S. van der Zwaag, Y.T. Pei, J.Th.M. De Hosson

Abstract

The linear and mass ablation rates of Ti2AlC ceramics under an oxyacetylene flame at a temperature up to 3000 degrees C were examined by measuring the dimensions and weight change of the ablated samples. The linear ablation rate was decreased from 0.14 mu m s(-1) the first 30s of the ablation to 0.08 mu m s(-1) after 180s. Ti2AlC ceramics gained small amounts of weight upon ablation, which is attributed to the formation of oxidation products on the ablated surface. The ablation surface exhibits a two-layer structure: an oxide outer layer, consisting mainly of alpha-Al2O3 and TiO2 and some Al2TiO5, and a porous sub-surface layer containing Ti2Al1-xC and TiCxOy. With increasing ablation time, the content of TiO2 and Al2TiO5 in the outer layer increased, and more pores developed in the sub-surface layer. The thermal oxidation of Ti2AlC under the flame and scouring of the viscous oxidation products by high-speed flow of gas torch are the main ablation mechanisms. Crown Copyright (C) 2010 Published by Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. The Mn+1AXn phases: a new class of solids, the thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Oxidation induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
3. Reaction synthesis of layered ternary Ti2AlC ceramic10.1016/j.jeurceramsoc.2008.05.039 ↗
4. Microstructural characterization of layered ternary Ti2AlC10.1016/j.actamat.2005.10.028 ↗
5. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
6. Microstructure and residual stress of alumina scale formed on Ti2AlC at high temperature in air10.1007/s11085-007-9063-0 ↗
7. 1990
8. A first-principles investigation of the phase stability of Ti2AlC with Al vacancies10.1016/j.scriptamat.2007.09.048 ↗
9. Ab initio modeling of the formation and migration of monovacancies in Ti2AlC10.1016/j.scriptamat.2008.06.044 ↗
10. National Standard Committee of China. GJB323A-96: measurement standard of ablation properties of materials. Beijing; 1996.
11. 1979
12. Measurement of surface temperatrues of a material during ablation
13. Artifact-free cross-sections
14. Early stages of oxidation of Ti3AlC2 ceramics10.1016/j.matchemphys.2008.06.038 ↗
15. Rusband · 2010
16. Elevated temperature ablation resistance and thermophysical properties of tungsten matrix composites reinforced with ZrC particles10.1023/A:1017989913219 ↗
17. Effect of carbide particles on the ablation properties of tungsten composites10.1016/S1044-5803(03)00123-2 ↗
18. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites10.1016/j.carbon.2009.09.035 ↗
19. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
20. Ablation behavior of ZrB2–SiC–ZrO2 ceramic composites by means of the oxyacetylene torch10.1016/j.corsci.2009.05.035 ↗
21. Overview of the TiC/TiO2 (rutile) interface10.1016/j.ssi.2004.02.055 ↗
22. Phase segregation of titanium–aluminium carbide (Ti2AlC) at high pressure and high temperature10.1016/j.jallcom.2007.08.032 ↗
23. Differential thermal analysis study of phase segregation of Ti2AlC under high pressure and high temperature10.1016/j.jallcom.2008.09.010 ↗
24. Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC10.1016/j.scriptamat.2007.09.011 ↗
25. First-principles study of oxygen incorporation and migration mechanisms in Ti2AlC10.1557/jmr.2009.0377 ↗
26. Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon10.1021/cm030022v ↗
27. Microstructure of high velocity oxy-fuel sprayed Ti2AlC coatings10.1007/s10853-010-4263-4 ↗
28. Phase stability of Ti2AlC upon oxygen incorporation: a first-principles investigation10.1103/PhysRevB.81.024111 ↗
29. Formation of the MAX-phase oxycarbide Ti2AlC1−xOx studied via electron energy-loss spectroscopy and first-principles calculations10.1103/PhysRevB.80.092102 ↗
30. Oxygen incorporation in Ti2AlC thin films10.1063/1.2838456 ↗
31. Reformation of phase composition in decomposed aluminium titanate10.1016/j.matchemphys.2008.03.017 ↗
32. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗