journal article·2013-04

Production and characterization of transparent MgAl2O4 prepared by hot pressing

Laura Esposito, Andreana Piancastelli, Stefano Martelli

Publisher page

Abstract

The high strength and hardness and the high temperature stability of spinel MgAl2O4 are among the properties that makes it an excellent candidate for advanced electromagnetic windows. The main requirement for this application is a high transparency. Due to its cubic structure, spinel can be produced in a transparent form. However since today spinel has not been extensively commercialized because of the difficulties encountered in the production process. Advancements in the comprehension of the experimental features affecting the transparency of spinel are presented. Transparent MgAl2O4 has been produced by hot pressing of a stoichiometric mixture of Al2O3 and MgO powders. Powders with a high purity level and with a high specific surface area have been selected and homogenously mixed by wet ball milling. LiF has been used as sintering additive. The influence of different hot pressing sintering cycles on the optical properties of spinel was studied. Various sintering cycles have been tested. The relationship among the processing conditions (sintering cycle), microstructure and transparency has been studied.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Transparent compact ceramics: inherent physical issues10.1016/j.optmat.2008.12.009 ↗
2. Transparent ceramics for high energy laser systems10.1016/j.optmat.2010.10.038 ↗
3. Fine-grained transparent spinel windows by the processing of different nanopowders10.1111/j.1551-2916.2010.03814.x ↗
4. A review on the sintering and microstructure development of transparent spinel (MgAl2O4)10.1111/j.1551-2916.2009.03108.x ↗
5. Gentilman RL, Maguire EA, Dolhert LE, Transparent aluminum oxynitride and method of manufacture, US Patent 4,520,116 (1985), Rayteon Company.
6. Chu HS-H, Lillo TM, Method of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor, US Patent 2008/0000573 A1 (2008), Batelle Energy Alliance.
7. Patel JP, Gilde G, McCauley JW, Transient liquid phase reactive sintering of aluminum oxynitride (ALON), US Patent 7,045,091 B1 (2006), The US Army.
8. McCauley JW, Corbin ND, Process for producing polycrystalline cubic aluminum oxynitride, US Patent 4,241,000 (1980), The USA Army.
9. Gentilman RL, Maguire EA, Dolhert LE, Transparent aluminum oxynitride and method of manufacture, US Patent 4,720,362 (1988).
10. Maguire EA, Hartnett TM, Gentilman RL, Method of producing aluminum oxynitride having improved optical characteristics, US Patent 4,686,070 (1987), Rayteon Company.
11. Infrared properties of shapphire, spinel and yttria as a function of temperature10.1117/12.936415 ↗
12. Hot isostatic pressing of MgAl2O4 spinel infrared windows10.1080/10426919408934941 ↗
13. An economic comparison of hot pressing vs. pressurelss sintering for transparent spinel armor
14. Transparent polycrystalline MgAl2O4 spinel with submicon grains, by low temperature sintering10.2109/jcersj2.117.1281 ↗
15. Transparent MgAl2O4 spinel from powder prepared by flame spray pyrolysis10.1111/j.1551-2916.2008.02788.x ↗
16. Transparent MgAl2O4 ceramic produced by spark plasma sintering10.1016/j.scriptamat.2009.03.039 ↗
17. Transparent MgAl2O4 spinel ceramics produced by HIP post-sintering10.2109/jcersj.114.802 ↗
18. Spark plasma sintering condition optimization for producing transparent MgAl2O4 spinel polycrystal10.1111/j.1551-2916.2009.03074.x ↗
19. Fine-grained transparent MgAl2O4 spinel obtained by spark plasma sintering of commercially available nanopowders10.1016/j.ceramint.2011.06.045 ↗
20. Evaluation of hot pressing and hot isostatic pressing parameters on the optical properties of spinel10.1111/j.1551-2916.2005.00527.x ↗
21. Synthesis and densification of transparent magnesium aluminate spinel by SPS processing10.1111/j.1551-2916.2008.02893.x ↗
22. Transparent solid solution magnesium aluminate spinel polycrystalline ceramic with the alumina-rich composition MgO·1.2 Al2O310.1111/j.1551-2916.2011.04798.x ↗
23. Fabrication of transparent spinel ceramics by reactive hot-pressing10.2109/jcersj1950.85.981_225 ↗
24. Transparent spinel fabricated from novel powders: synthesis, microstructure and optical properties
25. Sintering kinetics of a MgAl2O4 spinel doped with LiF10.1111/j.1551-2916.2007.02185.x ↗
26. Chemical interaction between LiF and MgAl2O4 spinel during sintering10.1111/j.1551-2916.2007.01723.x ↗
27. Degradation of magnesium aluminum spinel by lithium fluoride sintering aid10.1111/j.1551-2916.2005.00209.x ↗
28. Influence of graphite contamination on the optical properties of transparent spinel obtained by spark plasma sintering10.1016/j.scriptamat.2008.09.027 ↗
29. Investigation of high-alumina spinel: effect of LiF and CaCo3 addition10.1111/j.1151-2916.1997.tb03259.x ↗
30. Investigation of high alumina-spinel: effects of LiF and CaCO3 addition (part 2)10.1016/S0921-5093(98)00881-8 ↗
31. Sintering analysis of a fine-grained alumina-magnesia spinel powder10.1111/j.1551-2916.2010.04271.x ↗
32. West · 1984
33. Spark plasma sintering (SPS) of transparent magnesium–aluminate spinel10.1007/s10853-007-1672-0 ↗
34. Direct comparison between hot pressing and electric field-assisted sintering of submicron alumina10.1016/j.actamat.2009.07.043 ↗
35. Transparent spinel fabricated from novel powders: synthesis, microstructure and optical properties, ADM201976
36. The effect of precipitation parameters on preparation of lithium fluoride (LiF) nanopowders10.1080/00986440701244309 ↗
37. Deterioration in the final-stage sintering of magnesium aluminate spinel10.1111/j.1151-2916.2000.tb01436.x ↗