Ambient and elevated temperature mechanical properties of hot-pressed fused silica matrix composite
Source abstract
Abstract
Abstract The ambient and elevated temperature mechanical properties of two kinds of hot-pressed fused silica matrix composites, SiO 2 +5 vol.% Si 3 N 4 and SiO 2 +5 vol.% Si 3 N 4 + 10 vol.% C f , were investigated. Si 3 N 4 additions greatly enhanced the ambient strength and fracture toughness, while, further incorporation of chopped carbon fibers only but sharply increased the fracture toughness value from 1.22 to 2.4 MPa m 1/2 . The strength of the two composites synchronously exhibited anomalous gains at certain elevated temperature range especially from 1000 to 1200 °C, and reached their maximum values at 1000 °C, 168.9 and 130.6 MPa, which were 77.0 and 77.4% higher than their ambient strength, respectively. The two composites exhibited catastrophic fracture even at 1000 °C, but manifested prominent plastic deformation at 1200 °C and usually no fracture occurred during the strength test. Vickers’ indentation crack propagation behavior, combined with fractographs studies, suggested that toughening from carbon fiber was attributed primarily to the fiber bridging, pull-out and crack deflection.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Fiber-reinforced polymer composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Yu · 1993
2. Exploratory research on the applications of carbon fiber reinforced silica on the thermal-protective structure of satellite and aero-ship
3. Guo, J. K. and Huang, X. X., Dielectric ceramic composite. In Second China–US Bilateral Seminar on Inorganic Materials Research Held in Gnithersberg, USA, 1987, p. 110.
4. Guo · 1984
5. Investigation on thermology properties and thermal shock resistance of SiO2–Si3N4 antenna window material
6. Mechanical properties and its toughening mechanisms of SiO2–Si3N4 composite
7. Co-enhanced SiO2–BN ceramics for high-temperature dielectric applications10.1016/S0955-2219(00)00107-2 ↗
8. Han, H. Q. Microstructure and Properites of Several SiO2 Matrix Composites. Ms thesis, Harbin Institute of Technology, Harbin, 1995, pp. 47–50.
9. Strength and toughness of slip-cast fused-silica composites10.1111/j.1151-2916.1994.tb09776.x ↗
10. Reinforcing fused silica with high-purity fibers
11. Influences of hot-pressing process on the microstructure and mechanical properties of SiO2f/SiO2 composites
12. Toughening of ceramics by circumferential microcracking10.1111/j.1151-2916.1981.tb09877.x ↗
13. The analysis of residual stress and toughening mechanisms of particulate reinforced dual-phase ceramics
14. Crack deflection process I10.1016/0001-6160(83)90046-9 ↗
15. Toughening behavior in SiC-whisker-reinforced alumina10.1111/j.1151-2916.1984.tb19694.x ↗
16. Toughening behavior in whisker-reinforced ceramic matrix composites10.1111/j.1151-2916.1988.tb05791.x ↗
17. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗
18. Feng, Y, Interface Structure of SiC Whisker Reinforced Oxide Based Ceramics and Its Effect on Mechanical Properties. PhD thesis, Harbin Institute of Technology, Harbin, 1995, pp. 60–70.
19. Properties and structure of vitreous silica10.1016/0022-3093(70)90190-0 ↗
20. High-temperature effects in the fracture mechanical behavior of silicon carbide liquid-phase sintered with AlN-Y2O3 additives10.1016/S0955-2219(00)00317-4 ↗
21. The role of interfaces in fiber-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗