journal article·2008-01

Influence of sintering conditions on microstructure and electrical conductivity of yttrium-substituted SrTiO3

Q.X. Fu, S.B. Mi, E. Wessel, F. Tietz

Publisher page

Abstract

Abstract The microstructure and electrical conductivity of Y-substituted SrTiO 3 ceramics (Sr 1− αx Y x TiO 3− δ , x = 0, 0.035, 0.07; α = 1.0, 1.5) sintered under both oxidizing and reducing conditions were studied in detail. In these compositions, Y 3+ ions have been found to occupy the Sr sites and act as donor substitutes. The observed interesting dependence of the microstructure and electrical property on the starting composition (cation nonstoichiometry) and the sintering or processing conditions indicates that the defect chemistry known for other donor-substituted SrTiO 3 (e.g. Sr 1− x La x TiO 3− δ ) ceramics also applies for Y-substituted SrTiO 3 ceramics. The positive charge from the Y-substitute can be compensated either electronically under reducing conditions or ionically under oxidizing conditions. Therefore, to obtain a single-phase and highly conductive yttrium-substituted SrTiO 3 material, e.g. as a candidate for an SOFC anode, a starting composition with (Sr + Y)/Ti = 1 and a high-temperature heat treatment (>1200 °C) under reducing conditions is required.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic and Structural Properties of Oxides · Advancements in Solid Oxide Fuel Cells · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Direct hydrocarbon solid oxide fuel cells10.1021/cr020725g ↗
2. Reduction and re-oxidation of anodes for solid oxide fuel cells10.1016/j.ssi.2005.06.014 ↗
3. Thermal, electrical, and electrocatalytical properties of lanthanum-doped strontium titanate10.1016/S0167-2738(02)00140-6 ↗
4. Electrical properties of yttrium-doped strontium titanate under reducing conditions10.1149/1.1420706 ↗
5. Microstructural changes during the reduction/reoxidation process in donor-doped BaTiO3 ceramics10.1111/j.1151-2916.2000.tb01594.x ↗
6. Compensating defects in highly donor-doped BaTiO310.1111/j.1151-2916.1986.tb07453.x ↗
7. Pechini, M.P., Method of preparing lead and alkaline earth titanates and niobates and coating method using the same to form a capacitor, U.S. Patent No. 3,330,697, 11 July 1967.
8. Dong · 1998
9. Indexing of powder diffraction patterns for low-symmetry lattices by the successive dichotomy method10.1107/S0021889891006441 ↗
10. Phase equilibria in the 1375°C isotherm of the system Sr–Ti–O10.1111/j.1151-2916.1969.tb09194.x ↗
11. New reduced ternary titanates from borate fluxes10.1016/0022-4596(91)90196-O ↗
12. Electrical conductivity and redox behaviour of yttrium-substituted SrTiO3: dependence on preparation and processing procedures
13. Electrical conductivity in strontium titanate10.1016/0022-4596(81)90270-X ↗
14. Crystal and defect chemistry of rare earth cations in BaTiO310.1023/A:1012218826733 ↗
15. Influence of ionic radii on the incorporation of trivalent dopants into BaTiO310.1016/0921-5107(88)90019-0 ↗
16. Incorporation of yttrium in barium titanate ceramics10.1111/j.1151-2916.1999.tb01921.x ↗
17. Solid solubility of holmium, yttrium, and dysprosium in BaTiO310.1111/j.1151-2916.2004.tb07729.x ↗
18. Defect chemistry of Y doped BaTiO310.1007/s10832-004-5196-6 ↗
19. Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
20. Self-compensation in lanthanum-doped strontium titanate10.1016/0022-4596(81)90365-0 ↗
21. Electrical conductivity in lanthanum-doped strontium titanate10.1149/1.2124008 ↗
22. Oxidation–reduction behaviour of La-doped SrTiO310.1007/BF00550814 ↗
23. Defect chemistry of donor-doped and undoped strontium titanate ceramics between 1000 and 1400°C10.1111/j.1151-2916.1997.tb03157.x ↗
24. Solubility of lanthanum in strontium titanate in oxygen-rich atmospheres10.1023/A:1018647117607 ↗
25. Kröger · 1956 · Vol. 3 · 307
26. Kinetics of equilibrium restoration in barium titanate ceramics
27. Influence of kinetic processes on the electrical conductivity of donor-doped BaTiO3 ceramics10.1002/pssa.2210470115 ↗
28. Smyth · 1993 · 47
29. Charge compensation mechanisms in La-doped BaTiO310.1023/A:1011400630449 ↗
30. The defect chemistry of donor-doped BaTiO3: a rebuttal10.1023/A:1023213208904 ↗
31. Two-fold diffusion kinetics of oxygen re-equilibration in donor-doped BaTiO310.1111/j.1551-2916.2005.00123.x ↗
32. Defect structure, electrical properties and transport in barium titanate. VII. Chemical diffusion in Nb-doped BaTiO310.1016/0272-8842(94)90061-2 ↗
33. Selbstdiffusion in Bariummetatitanat
34. Oxygen tracer diffusion in lanthanum-doped single-crystal strontium titanate10.1111/j.1151-2916.1994.tb07116.x ↗
35. Tracer diffusion and chemical diffusion of oxygen in acceptor doped SrTiO310.1016/S0022-3697(99)00421-7 ↗
36. Solubility of lanthanum in strontium titanate10.1111/j.1151-2916.1981.tb10288.x ↗
37. Oxygen partial pressure and grain growth in donor-doped BaTiO310.1111/j.1151-2916.1987.tb04999.x ↗
38. Anomalous grain growth in donor-doped barium titanate with excess barium oxide10.1111/j.1151-2916.2002.tb00146.x ↗
39. Dielectric properties of donor-doped polycrystalline SrTiO310.1007/BF00752196 ↗
40. Abnormal grain growth of BaTiO3 with small cation nonstoichiometry10.4028/www.scientific.net/MSF.204-206.491 ↗
41. Dependence of grain growth and grain-boundary structure on the Ba/Ti ratio in BaTiO310.1111/j.1551-2916.2004.00119.x ↗