journal article·2010-03Open access

Fabrication and properties of ZrB2–SiC–BN machinable ceramics

Haitang Wu, Weigang Zhang

Abstract

ZrB2-SiC-BN ceramics were fabricated by hot-pressing under argon at 1800 degrees C and 23MPa pressure. The microstructure, mechanical and oxidation resistance properties of the composite were investigated. The flexural strength and fracture toughness of ZrB2-SiC-BN (40 vol%ZrB2-25 vol%SiC-35 vol%BN) composite were 378 MPa and 4.1 MPa M 112, respectively. The former increased by 34% and the latter decreased by 15% compared to those of the conventional ZrB2-SiC (80vol%ZrB2-20vol%SiC). Noticeably, the hardness decreased tremendously by about 67% and the machinability improved noticeably compared to the relative property of the ZrB2-SiC ceramic. The anisothermal and isothermal oxidation behaviors of ZrB2-SiC-BN composites from 1100 to 1500 degrees C in air atmosphere showed that the weight gain of the 80 vol%ZrB2-20 vol%SiC and 43.1 vol%ZrB2-26.9 vol%SiC-30 vol%BN composites after oxidation at 1500 degrees C for 5 h were 0.0714 and 0.0268 g/cm(2), respectively, which indicates that the addition of the BN enhances oxidation resistance of ZrB2-SiC composite. The improved oxidation resistance is attributed to the formation of ample liquid borosilicate film below 1300 degrees C and a compact film of zirconium silicate above 1300 degrees C. The formed borosilicate and zirconium silicate on the surface of ZrB2-SiC-BN ceramics act as an effective barriers for further diffusion of oxygen into the fresh interface of ZrB2-SiC-BN. (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Fabrication and properties of reactively hot pressed ZrB2–SiC ceramics10.1016/j.jeurceramsoc.2006.11.074 ↗
2. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
3. Hot pressed ZrB2–SiC–C ultra high temperature ceramics with polycarbosilane as a precursor10.1016/j.matlet.2006.06.024 ↗
4. Processing and properties of ultra-high temperature ceramics for space applications10.1016/j.msea.2007.08.054 ↗
5. Characterization of hot-pressed short carbon fiber reinforced ZrB2–SiC ultra-high temperature ceramic composites10.1016/j.jallcom.2008.04.092 ↗
6. Microstructures, properties and fabrication of machinable ceramics
7. Development in machinable ceramics and machining technology of engineering ceramics
8. Scratching and grinding of a machinable glass-ceramic with weak interfaces and rising T-curve10.1111/j.1151-2916.1995.tb08831.x ↗
9. Nonoxide–boron nitride composites: in situ synthesis, microstructure and properties10.1016/S0955-2219(02)00115-2 ↗
10. Analysis of micro-machining characteristics of Si3N4–hBN composites10.1016/j.jeurceramsoc.2006.08.002 ↗
11. Fabrication and properties of machinable 3Y–ZrO2/BN nanocomposites10.1016/j.msea.2005.01.038 ↗
12. Fabrication and microstructure of silicon nitride/boron nitride nanocomposites10.1111/j.1151-2916.2002.tb00514.x ↗
13. Fabrication and characterization of machinable Si3N4/h-BN functionally graded materials10.1016/S0025-5408(02)00773-0 ↗
14. Machinable Al2O3/BN composite ceramics with strong mechanical properties10.1016/S0025-5408(02)00786-9 ↗
15. Fabrication of machinable silicon carbide–boron nitride ceramic nanocomposites10.1111/j.1551-2916.2004.00565.x ↗
16. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
17. High-temperature oxidation of boron nitride: ii. Boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
18. Fibrous monolithic ceramics: III. mechanical properties and oxidation behavior of the silicon carbide/boron nitride system10.1111/j.1151-2916.1994.tb05399.x ↗
19. Relationship between oxidation resistance and structure of B4C–SiC/C composites with self-healing properties10.1016/S0008-6223(98)00184-5 ↗
20. Oxidation of zirconium diboride–silicon carbide at 1500°C at a low partial pressure of oxygen10.1111/j.1551-2916.2006.01229.x ↗