journal article·2007-01

Strength recovery behavior of machined Al2O3/SiC nano-composite ceramics by crack-healing

Toshio Osada, Wataru Nakao, Koji Takahashi, Kotoji Ando, Shinji Saito

Publisher page

Abstract

The machined alumina/15 vol.% SiC nano-composites having a semicircular groove were conducted to various heat treatments. The change of the local fracture stress at the bottom of semicircular groove has been investigated as a function of crack-healing temperature and time. By heating at 1400 °C at 1 h, the machined specimen was fractured not from the cracks introduced by the hard machining but from the other region. Thus, it was concluded that the machining cracks were completely healed by the above heat treatment. Moreover, The strength at room temperature and elevated temperature (<1300 °C) of the machined sample healed exhibited the same levels as that of polished sample healed. It can be demonstrated that the crack-healing was useful for an increase in the strength of machined ceramics economically.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Strengthening of oxide ceramics by SiC and Si3N4 dispersions.
2. New design concept of structural ceramics–ceramic nanocomposites, the chemical issue of the ceramic society of Japan10.2109/jcersj.99.974 ↗
3. Study on strengthening of mullite by dispersion on carbide ceramics particles10.1299/kikaia.60.2829 ↗
4. Strengthening of mullite by dispersion of carbide ceramics particles (2nd report, effect of SiC grain size and heat treatment)10.1299/kikaia.61.1023 ↗
5. Damage healing and strengthening behavior in intelligent mullite/SiC ceramics10.1111/j.1460-2695.1995.tb00924.x ↗
6. Crack healing by heat treatment10.1111/j.1151-2916.1970.tb12002.x ↗
7. Healing of surface cracks in polycrystalline Al2O310.1111/j.1151-2916.1970.tb12148.x ↗
8. Spheroidization of tubular voids in A12O3 crystals at high temperatures10.1111/j.1151-2916.1972.tb13417.x ↗
9. The effect of annealing on surface machining damage of alumina ceramics10.2109/jcersj.99.384 ↗
10. Mechanical behavior of Al2O3–SiC nanocomposite10.1111/j.1151-2916.1993.tb03814.x ↗
11. Machining-introduced surface residual stress behavior in Al2O3–SiC nanocomposite10.1111/j.1151-2916.1996.tb08989.x ↗
12. Crack healing and surface relaxation in Al2O3–SiC “nanocomposite”10.1111/j.1151-2916.1995.tb08215.x ↗
13. The strength of Al2O3/SiC nanocomposite after grinding and annealing10.1016/S1359-6454(98)00068-8 ↗
14. Crack-healing behavior of monolithic alumina and strength of crack-healed member10.2472/jsms.52.667 ↗
15. Crack-healing and mechanical behavior of Al2O3/SiC composites at elevated temperature10.1111/j.1460-2695.2004.00785.x ↗
16. High temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers10.1111/j.1151-2916.2004.tb07720.x ↗
17. Crack-healing behavior of mullite/SiC/Y2O3 composites and its application to the structural integrity of machined components10.1016/j.jeurceramsoc.2004.08.024 ↗
18. Effect of crack-healing and proof-testing procedures on fatigue strength and reliability of Si3N4/SiC components10.1016/S0955-2219(02)00232-7 ↗
19. Threshold stress for crack-healing of Si3N4/SiC and resultant cyclic fatigue strength at the healing temperature10.1111/j.1551-2916.2005.00106.x ↗
20. Critical crack-healing condition under stress of SiC whisker reinforced alumina10.1016/j.jeurceramsoc.2004.09.021 ↗
21. Crack-healing behavior under stress, strength and fracture toughness of Mullite/SiC whisker composite ceramics10.2472/jsms.54.207 ↗
22. 1993
23. Nishida · 1967