journal article·2017-04Open access

Oxidation behavior of ZrB2-SiC-ZrC at 1700 °C

Yuki Kubota, Hiroki Tanaka, Yutaro Arai, Ryo Inoue, Yasuo Kogo, Ken Goto

Abstract

Abstract The oxidation behaviors of four compositions of ZrB 2 -SiC-ZrC and one composition of ZrB 2 -SiC were studied at 1700 °C in air and under low oxygen partial pressure. Volatility diagrams for ZrB 2 -SiC-ZrC and ZrB 2 -SiC were used to thermodynamically elucidate the oxidation mechanisms. SiO 2 and ZrO 2 layers formed on the surfaces of ZrB 2 -SiC-ZrC and ZrB 2 -SiC oxidized at 1700 °C. A SiC-depleted layer only formed on the surface of the ZrB 2 -SiC oxidized under low oxygen partial pressure. The oxide layer thickened with increasing ZrC volume content during oxidation in air and under low oxygen partial pressure. The ZrB 2 -SiC-ZrC oxide surface exploded in air when the ZrC volume content was more than 50%. Under low oxygen partial pressure, the oxide surfaces of all the ZrB 2 -SiC-ZrC specimens bubbled.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Plasma torch test of an ultra-high-temperature ceramics nose cone demonstrator10.2514/1.42834 ↗
2. D.J. Thomas, Design and Analysis of UHTC Leading Edge Attachment, NASA/CR 2002 211505.
3. Aerothermodynamic study of UHTC-based thermal protection systems10.1016/j.ast.2004.12.003 ↗
4. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
5. Ablation behavior of ZrB2-SiC sharp leading edges10.1016/j.jallcom.2013.03.067 ↗
6. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
7. High-temperature chemistry and oxidation of ZrB2-ceramic containing SiC, Si3N4, Ta5Si3, and TaSi210.1111/j.1551-2916.2008.02420.x ↗
8. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
9. Oxidation of ZrB2-SiC ultrahigh-temperature ceramic composites in dissociated air10.2514/1.39970 ↗
10. The high-temperature oxidation behavior of a HfB2+20v/o SiC composite10.1149/1.2134436 ↗
11. Oxidation resistance of HfB2-SiC composite for protection of carbon-based materials
12. Thermodynamic analysis of ZrB2-SiC oxidation: formation of SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
13. Ablation behavior of ZrB2-SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions10.1016/j.compscitech.2008.02.009 ↗
14. Structure evolution of ZrB2-SiC during the oxidation in air10.1557/JMR.2008.0251 ↗
15. Oxidation-resistant ZrB2-SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
16. The oxidation behavior of a ZrB2-SiC-ZrC ceramic10.1016/j.solidstatesciences.2010.12.022 ↗
17. J. Bull, M.J. White, L. Kaufman, Ablation Resistant Zirconium and Hafnium Ceramics, United States Patent, No. 5750450, May 12, 1998.
18. Volatility diagrams for silica, silicon nitride, and silicon carbide and their application to high-temperature decomposition and oxidation10.1111/j.1151-2916.1990.tb06677.x ↗
19. Oxidation mechanism of ZrB2/SiC ceramics based on phase-field model10.1016/j.compscitech.2012.04.003 ↗
20. Modeling oxidation kinetics of SiC-containing refractory diborides10.1111/j.1551-2916.2011.04927.x ↗
21. Thermal and oxidation response of UHTC leading edge samples exposed simulated hypersonic flight conditions10.1111/jace.12180 ↗
22. Chase · 1998
23. High-temperature oxidation at 1900°C of ZrB2-xSiC ultrahigh-temperature ceramic composites10.1111/j.1551-2916.2008.02660.x ↗
24. Oxidation of ZrB2- and HfB2-based ultra-high temperature ceramics: effect of Ta additions10.1023/B:JMSC.0000041693.32531.d1 ↗
25. Effects of oxygen partial pressure and atomic oxygen on the microstructure of oxide scale of ZrB2-SiC composites at 1500°C10.1016/j.corsci.2013.03.023 ↗
26. Oxidation behavior of zirconium diboride-silicon carbide ceramic composites under low oxygen partial pressure10.1016/j.corsci.2011.07.020 ↗
27. Effect of an SiC addition on the oxidation of ZrB2
28. Oxidation behavior of ZrB2-SiC composites at low pressures10.1111/jace.13281 ↗
29. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
30. Thermochemical and mechanical stabilities of the oxide scale of ZrB2-SiC and oxygen transport mechanisms10.1111/j.1551-2916.2008.02319.x ↗
31. Oxidation of SiC-based ceramics at high temperature10.2320/materia.52.434 ↗
32. High-temperature active/passive oxidation and bubble formation of CVD SiC in O2 and CO2 atmospheres10.1016/S0955-2219(02)00139-5 ↗