Abstract
Structural ceramics are brittle and sensitive to flaws. As a result, the structural integrity of a ceramic component may be seriously affected. To overcome this problem, there are three ways: (a) inspect carefully and repair the unacceptable flaws, (b) toughen the ceramics by fiber reinforcing, (c) heal the flaws and recover strength. At the moment, there is no technique to heal embedded flaws. Therefore, a new technique to guarantee the reliability of ceramics components is demanded and so we proposed new technique: (crack-healing+proof test). For this technique, the mechanical behaviour of the crack-healed zone is very important for the structural integrity. Bending strength and fatigue strength test results of the crack-healed zone at high temperature are described. Using a process zone size failure criterion, an equation for the temperature-dependence of proof stress (σPT) is derived. The accuracy of the equation has been verified for monotonic loading tests up to 1300°C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Crack-healing by heat treatment10.1111/j.1151-2916.1970.tb12002.x ↗
2. Healing of surface cracks in polycrystalline Al2O310.1111/j.1151-2916.1970.tb12148.x ↗
3. Controlled surface flaws in hot-pressed SiC10.1111/j.1151-2916.1976.tb09381.x ↗
4. Crack-healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗
5. Crack-healing behavior of hot-pressed silicon nitride due to oxidation10.1016/0956-716X(92)90574-X ↗
6. Study on strengthening of mullite by dispersion of carbide ceramics particles10.1299/kikaia.60.2829 ↗
7. Damage healing and strengthening behavior in intelligent mullite/SiC ceramics10.1111/j.1460-2695.1995.tb00924.x ↗
8. Strengthening of mullite by dispersion of carbide ceramics particles10.1299/kikaia.61.1023 ↗
9. High temperature crack annealing effect on fracture toughness of alumina and alumina–SiC composite
10. A preliminary study on crack healing behavior of Si3N4/SiC composite ceramics10.1046/j.1460-2695.1998.00052.x ↗
11. Crack-healing behavior of silicon nitride ceramics(effect of chemical composition on crack healing ability)
12. The study on crack healing behavior of silicon nitride ceramics10.1299/kikaia.64.1936 ↗
13. Crack healing in a Silicon Nitride Ceramics10.1111/j.1151-2916.1998.tb02558.x ↗
14. Crack healing behavior and high temperature strength of mullite/SiC composite ceramics10.2472/jsms.48.489 ↗
15. Fatigue strength properties of crack healed mullite/SiC composite ceramics10.2472/jsms.48.1173 ↗
16. Crack healing behavior and high temperature strength of silicon nitride ceramics10.1299/kikaia.65.1132 ↗
17. Fatigue strength of crack-healed Si3N4/SiC composite ceramics10.1046/j.1460-2695.1999.00210.x ↗
18. Crack-healing behavior, high-temperature and fatigue strength of SiC-reinforced silicon nitride composite10.1023/A:1006715825737 ↗
19. Crack healing behavior of SiC ceramics10.1111/j.1151-2916.2000.tb01632.x ↗
20. The low-cycle fatigue strength of crack-healed Si3N4/SiC composite ceramics
21. Effect of pre-crack size and testing temperature on fatigue strength properties of crack-healed mullite10.2472/jsms.50.920 ↗
22. Static and cyclic behaviour of crack-healed Si3N4/SiC composite ceramics10.1016/S0955-2219(00)00279-X ↗
23. Proof-testing of hot-pressed silicon nitride10.1007/BF00548742 ↗
24. Proof testing of ceramics (part 1 Experiment)10.1007/BF00552317 ↗
25. Proof testing of ceramics (part 2 Theory)10.1007/BF00552317 ↗
26. High-temperature fatigue behavior of polycrystalline alumina10.1111/j.1151-2916.1980.tb10635.x ↗
27. Jakus, K., Fahey, J. P. and Ritter, J. E. Jr., Improving the reliability of hot-pressed silicon nitride. In Fract. Mech. Ceram. 5, ed. R. C. Bradt, A. G. Evans, D. P. H., Hasselman and F. F. Lange. Plenum Publishing Co., 1983, pp. 425–434.10.1007/978-1-4613-3488-0_26 ↗
28. Fatigue properties of ceramics after proof testing (1st report theoretical analysis)10.1299/kikaia.56.212 ↗
29. Fatigue properties of ceramics after proof testing (2nd report experimental study)10.1299/kikaia.56.220 ↗
30. Ando, K., Sato, S., Sone, S. and Kobayashi, Y. Probabilistic study on fatigue life of proof tested ceramics spring. In Fracture From Defects (ECF-12), ed. M. W. Brown, E. R. de los Rios and K. J. Miller. EMAS. Publishing, 1998, pp. 569–574.
31. Ando, K., Sato, S., Kobayashi, Y. and Chu, M. C. Crack healing behaviour of Si3N4 ceramics and its application to structural integrity. In Fracture From Defects (ECF-12), ed. M. W. Brown, E. R. de los Rios and K. J. Miller. Engineering Materials Advisory Services, 1998, pp. 497–502.
32. Process zone size failure criterion and probabilistic fracture aassessment curves for ceramics10.1111/j.1460-2695.1992.tb00044.x ↗
33. Yielding of steel sheets containing slits10.1016/0022-5096(60)90013-2 ↗
34. Effect of crack length, notch root radius and grain size on fracture toughness of fine ceramics10.1111/j.1460-2695.1993.tb00134.x ↗
35. A fracture and severity analysis of composite ceramics10.1111/j.1460-2695.1993.tb00091.x ↗
36. The location of crack initiation sites in alumina, polycarbonate and mild steel
37. A study on strength characteristics of Si3N4 coil spring10.1111/j.1460-2695.1996.tb00989.x ↗