Different approaches to produce coatings with bioactive glasses: Enamelling vs plasma spraying
Source abstract
Abstract
Abstract Two alternative approaches, enamelling and plasma spraying, were tested to deposit coatings made with two different bioactive glasses: the established Bioglass ® 45S5, which is considered as a term of comparison, and the experimental BioK. The strong points and weaknesses of the two methods were highlighted. From the analysed samples, it resulted that the enamelling approach works well on thermally stable substrates and creates a strong bond, characterized by a compositional gradient, with alumina substrates. However, the coating thickness must be carefully controlled to limit the thermal residual stresses and the glass formulation should be designed to reduce the glass tendency to crystallize. Instead plasma spraying is suitable for any kind of substrate and is highly automatizable, but the equipment is relatively expensive and the coatings are likely to retain some defectiveness, which makes a post-deposition thermal treatment necessary. Both enamelling and plasma spraying may induce crystallization phenomena, depending on the glass formulation. The introduction of potassium oxide in the glass composition, such as in the BioK, may be useful to hinder the crystallization.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Bioceramics10.1111/j.1151-2916.1998.tb02540.x ↗
2. Bioactive materials for tissue engineering, regeneration and repair10.1023/A:1027414700111 ↗
3. Mechanical properties of bioactive glasses, glass–ceramics and composites10.1243/0954411981533908 ↗
4. Bioactive glass coatings for orthopedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
5. The current techniques for preparing bioglass coatings10.1142/S0218625X05007347 ↗
6. Surface coatings of bioactive glasses on high strength ceramic composites10.1016/j.apsusc.2009.02.069 ↗
7. Hertzian-crack suppression in ceramics with elastic-modulus-graded surfaces10.1111/j.1151-2916.1998.tb02625.x ↗
8. Bioactivity of sol–gel bioactive glass coated alumina implants10.1002/1097-4636(200011)52:2<422::AID-JBM24>3.0.CO;2-P ↗
9. Fabrication and characterization of a bioactive glass coating on titanium implant alloys10.1016/S1359-6454(99)00280-3 ↗
10. Understanding plasma spraying10.1088/0022-3727/37/9/R02 ↗
11. Current status and future trends10.1557/mrs2000.119 ↗
12. 2004
13. Bioactive glass coating: physicochemical aspects and biological findings10.1016/0142-9612(95)91123-G ↗
14. Characteristics of plasma-sprayed bioactive glass coatings on Ti–6A1–4V alloy: an in vitro study10.1016/0257-8972(95)02463-8 ↗
15. Glasses and bioglasses: synthesis and coatings10.1016/S0955-2219(96)00176-8 ↗
16. Sintering and plasma spray deposition of bioactive glass–matrix composites for medical applications10.1016/S0955-2219(97)00134-9 ↗
17. Coating titanium implants with bioglass and with hydroxyapatite, a comparative study in sheep10.1007/s002640050282 ↗
18. Adhesion of new bioactive glass coating10.1002/(SICI)1097-4636(19990305)44:3<243::AID-JBM2>3.0.CO;2-O ↗
19. Adhesion of bioactive glass coating to Ti6Al4V oral implant10.1016/S0142-9612(00)00027-2 ↗
20. The effect of bond coat on mechanical properties of plasma sprayed bioglass–titanium coatings10.1016/S0272-8842(03)00107-X ↗
21. Microstructural and in vitro characterisation of high-velocity suspension flame sprayed (HVSFS) bioactive glass coatings10.1016/j.jeurceramsoc.2009.01.032 ↗
22. Glass-alumina composite coatings by plasma spraying. Part I. Microstructural and mechanical characterization10.1016/j.surfcoat.2005.10.039 ↗
23. Potassium-based composition for a bioactive glass10.1016/j.ceramint.2009.06.011 ↗
24. Influence of heat treatment on crystallization of bioactive glasses10.1016/j.jnoncrysol.2007.06.092 ↗
25. Chemical durability of commercial silicate glasses. I. Material characterization10.1016/S0022-3093(00)00442-7 ↗
26. Vickers indentation fracture test. Part 2. Application and critical evaluation of standardised indentation toughness equation10.1179/mst.1989.5.10.961 ↗
27. The self-setting properties and in vitro bioactivity of tricalcium silicate10.1016/j.biomaterials.2005.04.025 ↗
28. Sol–gel synthesis of Na2CaSiO4 and its in vitro biological behaviors10.1007/s10971-009-2006-2 ↗
29. Effect of coating thickness on thermal stresses in tungsten-coated optical fibers10.1063/1.372410 ↗
30. Miyamoto · 1999
31. Navarro · 1991
32. Plasma-sprayed glass–ceramic coatings on ceramic tiles: microstructure chemical resistance and mechanical properties10.1016/j.jeurceramsoc.2004.06.018 ↗
33. Concept and P/M fabrication of functionally graded materials10.1016/0272-8842(95)00143-3 ↗