journal article·2016-01

Molten salts electrochemical synthesis of Cr 2 AlC

Amr M. Abdelkader

Publisher page

Abstract

Abstract The unique combination of electrical, mechanical and chemical properties of MAX phase ceramics makes them attractive for energy and structural industrial applications. Here, an inexpensive and simple electrochemical deoxidation process is used to produce high quality, homogeneous micron-size particles of one of the most widely studied MAX phases, Cr2AlC. The process used cathode precursors made of cheap and available oxides of both chromium and aluminum and applied a constant potential difference in molten NaCl–CaCl2 as the electrolyte. It was found that the reduction mechanism took an unusual pathway through the formation of sub-stoichiometric oxides and oxycarbide phases that did not necessarily involve reactions between the cathode and the electrolyte. The Cr2AlC powder produced could be easily pressed into a monolithic bulk that have 4.8 ± 0.8 GPa hardness and showed excellent oxidation resistance at temperatures below 1100 °C. The method is quite generally applicable to the preparation of other MAX phases. Implications are drawn considering the industrial scale-up of this method for the low-cost production of MAX ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. The MAX phases: unique new carbide and nitride materials: tertiary ceramics are soft and machinable, yet heat-tolerant, strong and lighweight10.1511/2001.28.736 ↗
2. MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
3. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
4. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
5. Synthesis and thermal stability of Cr2AlC10.1016/j.jeurceramsoc.2011.01.009 ↗
6. Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics10.1016/j.actamat.2011.03.035 ↗
7. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
8. Oxidation and crack healing behavior of a fine-grained Cr2AlC ceramic10.1111/jace.12170 ↗
9. W.E. Lee, E. Giorgi, R. Harrison, A. Maître, O. Rapaud, Nuclear Applications for Ultra-High Temperature Ceramics and MAX Phases. Ultra-High Temperature Ceramics: Materials for Extreme Environment Applications, 2014, p. 391–415.10.1002/9781118700853.ch15 ↗
10. Thermal and electrical properties of Nb2AlC, (Ti, Nb)2AlC and Ti2AlC10.1007/s11661-002-0262-7 ↗
11. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
12. MAX phases: bridging the gap between metals and ceramics
13. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
14. Phase formation sequence of Cr2AlC ceramics starting from Cr–Al–C powders10.1016/j.msea.2006.08.064 ↗
15. Microstructures, electrical, thermal, and mechanical properties of bulk Ti2AlC synthesized by self-propagating high-temperature combustion synthesis with pseudo hot isostatic pressing10.1111/j.1551-2916.2011.04934.x ↗
16. Properties of hot-pressed Ti2AlN obtained by SHS process
17. Fabrication of highly dense Ti3SiC2 ceramics by pressureless sintering of mechanically alloyed elemental powders10.1023/A:1024490720287 ↗
18. DC voltammetry of electro-deoxidation of solid oxides10.1021/cr200305x ↗
19. Electrochemical synthesis and characterization of a NdCo5 permanent magnet10.1039/c0jm00096e ↗
20. Aspects of the preparation of NdCo5 intermetallic via the FFC-Cambridge process
21. Utilization of constant current chronopotentiometry to synthesize a Co–Cr alloy10.1149/1.3427511 ↗
22. Synthesis of self-passivated, and carbide-stabilized zirconium nanopowder10.1007/s11051-013-2112-5 ↗
23. Electrochemical synthesis of hafnium carbide powder in molten chloride bath and its densification10.1016/j.jeurceramsoc.2012.07.010 ↗
24. The electrochemical synthesis of TiC reinforced Fe based composite powder from titanium-rich slag10.1039/C4NJ02414A ↗
25. Solid state electrochemical synthesis of titanium carbide10.1016/j.cplett.2015.01.004 ↗
26. Direct electrochemical preparation of Nb–10Hf–1Ti alloy10.1016/j.electacta.2009.12.082 ↗
27. Electro-deoxidation of hafnium dioxide and niobia-doped hafnium dioxide in molten calcium chloride10.1016/j.electacta.2011.11.107 ↗
28. Synthesis of niobium aluminides by electro-deoxidation of oxides10.1016/j.jallcom.2009.06.176 ↗
29. Phase composition and microstructure of Al2O3–Cr2O3 solid solutions prepared by self-propagating high-temperature synthesis10.1134/S0020168507070102 ↗
30. Reaction mechanism in alumina/chromia (Al2O3–Cr2O3) solid solutions obtained by coprecipitation10.1111/j.1151-2916.2000.tb01508.x ↗
31. Sintering of Al2O3–Cr2O3 powder prepared by sol–gel process10.2472/jsms.56.526 ↗
32. The electrochemical reduction of chromium sesquioxide in molten calcium chloride under cathodic potential control
33. XPS study of group IA carbonates
34. Alkali reduction of graphene oxide in molten halide salts: production of corrugated graphene derivatives for high-performance supercapacitors10.1021/nn505700x ↗
35. Use of tetraneopentylchromium as a precursor for the organometallic chemical vapor deposition of chromium carbide: a reinvestigation10.1021/cm00040a019 ↗
36. XPS investigation of the a-C:H/Al interface10.1016/0039-6028(93)90395-Z ↗
37. Small area MXPS- and TEM-measurements on temper-embrittled 12% Cr steel
38. Novel electrochemical measurements on direct electro-deoxidation of solid TiO2 and ZrO2 in molten calcium chloride medium10.1007/s10800-010-0242-3 ↗
39. Synthesis and thermal stability of Cr2AlC10.1016/j.jeurceramsoc.2011.01.009 ↗
40. Mechanical properties of low temperature synthesized dense and fine-grained Cr2AlC ceramics10.1016/j.jeurceramsoc.2010.08.014 ↗
41. Processing and mechanical properties of Ti3SiC2: I. Reaction path and microstructure evolution10.1111/j.1151-2916.1999.tb02166.x ↗
42. Kinking nonlinear elastic deformation of Ti3AlC2, Ti2AlC, Ti3Al(C0.5,N0.5)2 and Ti2Al(C0.5,N0.5)10.1016/j.jallcom.2010.03.099 ↗
43. Synthesis of high-purity, isotropic or textured Cr2AlC bulk ceramics by spark plasma sintering of pressure-less sintered powders10.1016/j.jeurceramsoc.2014.11.008 ↗
44. Microstructure and mechanical properties of porous Ti3SiC210.1016/j.actamat.2005.05.034 ↗
45. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
46. Oxidation behavior of Cr2AlC ceramics at 1100 and 1250°C10.1007/s10853-008-2516-2 ↗
47. Long-time oxidation of Cr2AlC between 700 and 1000°C in air10.1007/s11085-012-9285-7 ↗