Strength of hot pressed ZrB2–SiC composite after exposure to high temperatures (1000–1700 °C)
Source abstract
Abstract
Abstract Residual strength (room temperature strength after exposure in air at high temperatures) of hot pressed ZrB2–SiC composites was evaluated as function of SiC contents (10–30 vol%) as well as exposure temperatures for 5 h (1000–1700 °C). Multilayer oxide scale structures were found after exposures. The composition and thickness of these multilayered oxide scale structure was dependent on exposure temperature and SiC contents in composites. After exposure to 1000 °C for 5 h, the residual strength of ZrB2–SiC composites improved by nearly 60% compared to the as-hot pressed composites with 20 and 30 vol% SiC. On the other hand, the residual strength of these composites remained unchanged after 1500 °C for 5 h. A drastic degradation in residual strength was observed in composites with 20 and 30 vol% SiC after exposure to 1700 °C for 5 h in ZrB2–SiC. An attempt was made to correlate the microstructural changes and oxide scales with residual strength with respect to variation in SiC content and temperature of expsoure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Materials for ultrahigh temperature structural applications
2. Talmy IG Zaykoski JA, Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
3. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
4. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
5. Karlsdottir SN. PhD thesis. University of Michigan, USA; 2007.
6. Toward oxidation-resistant ZrB2–SiC ultra high temperature ceramics10.1007/s11661-010-0540-8 ↗
7. Structure evolution of ZrB2–SiC during the oxidation in air10.1557/JMR.2008.0251 ↗
8. Thermodynamic analysis of ZrB2–SiC oxidation. Formation of a SiC – depleted region10.1111/j.1551-2916.2006.01329.x ↗
9. Pressureless sintering of ZrB2–SiC ceramics: the effect of B4C content10.1016/j.scriptamat.2008.12.003 ↗
10. Effect of thermal exposure on strength of ZrB2-based composites with nano-sized SiC particles10.1016/j.compscitech.2008.06.021 ↗
11. Oxidation resistance and strength retention of ZrB2–SiC ceramics10.1016/j.jeurceramsoc.2010.01.028 ↗
12. Effect of oxidation at 1100°C on the strength of ZrB2–SiC–graphite ceramics10.1016/j.jallcom.2011.03.163 ↗
13. Residual strength of hot pressed zirconium diboride (ZrB2) after exposure to high temperatures10.1016/j.msea.2011.12.062 ↗
14. Calibration curve for quantitative analysis of the monoclinic–tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
15. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
16. Mechanical properties of sintered ZrB2–SiC ceramics10.1016/j.jeurceramsoc.2010.11.013 ↗
17. High strength zirconium diboride-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
18. Oxidation behavior of hot pressed ZrB2–SiC and HfB2–SiC composites10.1016/j.jeurceramsoc.2010.08.018 ↗
19. Effect of an SiC addition on the oxidation of ZrB2
20. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
21. Liquid oxide flow during oxidation of zirconium diboride–silicon carbide ultra high temperature ceramics10.4028/www.scientific.net/KEM.434-435.144 ↗
22. Zirconia transport by liquid convection during oxidation of zirconium diboride–silicon carbide10.1111/j.1551-2916.2007.02142.x ↗
23. Oxidation of ZrB2–SiC: influence of SiC content on solid and liquid oxide phase formation10.1111/j.1551-2916.2008.02874.x ↗
24. The high temperature oxidation, reduction, and volatilization reactions of silicon and silicon carbide10.1007/BF00613092 ↗
25. Volatility diagrams for silica, silicon nitride, and silicon carbide and their application to high temperature decomposition and oxidation10.1111/j.1151-2916.1990.tb06677.x ↗