Orientation control and electrical properties of PZT/LNO capacitor through chemical solution deposition
Source abstract
Abstract
Abstract This paper describes the deposition of PZT/lanthanum nickel oxide (LNO) electrode thin-film capacitor on a Si(1 0 0) substrate with a chemical solution deposition (CSD). Highly (1 0 0)-oriented LNO film with a perovskite structure was deposited by annealing at 700 °C from a precursor solution of La(NO 3 ) 3 and Ni(CH 3 COO) 2 . In addition, highly (1 0 0)&(0 0 1)-oriented PZT/LNO capacitor was deposited on LNO/Si substrate by annealing at 600 °C, showing P r = 18 μC/cm 2 and E c = 36 kV/cm. Furthermore, the resultant PZT/LNO thin-film capacitor exhibited no fatigue up to 10 8 switching cycles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Ferroelectric characteristics of oriented Pb(Zr1−xTix)O3 films10.1063/1.1394159 ↗
2. Enhanced ferroelectric properties of Pb(Zr0.53Ti0.47)O3 thin films on SrRuO3/Ru/SiO2/Si substrates10.1063/1.1480099 ↗
3. Ferroelectric properties of Pb(Zi, Ti)O3 capacitor with thin SrRuO3 films within both electrodes10.1143/JJAP.39.2110 ↗
4. Effects of crystalline quality and electrode material on fatigue in Pb(Zr,Ti)O3 thin film capacitors10.1063/1.109739 ↗
5. Preparation of Pb(Zr,Ti)O3 thin films on Ir and IrO2 electrodes10.1143/JJAP.33.5207 ↗
6. Fatigue of ferroelectric PbZrxTiyO3 capacitors with Ru and RuOx electrodes10.1557/JMR.1993.0012 ↗
7. Comparative analysis for the crystalline and ferroelectric properties of Pb(Zr,Ti)O3 thin films deposited on metallic LaNiO3 and Pt electrodes10.1016/S0040-6090(02)00254-7 ↗
8. Ferroelectric La-Sr-Co-O/Pb-Zr-Ti-O/La-Sr-Co-O heterostructures on silicon via template growth10.1063/1.110106 ↗
9. Preparation and evaluation of LaNiO3 thin film electrode with chemical solution deposition10.1016/S0955-2219(03)00382-0 ↗
10. Low-temperature processing of ferroelectric Pb(Zr0.53Ti0.47)O3 thin film from molecular-designed alkoxide precursor solution10.1143/JJAP.35.4896 ↗