journal article·2016-07

The catalytic effect of iron oxides on the formation of nano-carbon by the Boudouard reaction in refractories

N. Bost, M.R. Ammar, M.L. Bouchetou, J. Poirier

Publisher page

Abstract

Abstract The catalytic decomposition of carbon monoxide via the Boudouard reaction in the presence of iron has been a subject of numerous studies. This reaction produces a solid carbon deposit in which CO is a reactant and results in deleterious effects on refractory materials. Only a few studies have used a gas mixture primarily composed of CO + H2, which is generated in new energy applications. We investigated the effect of the degree of oxidation and the grain size of the FexOy catalyst particles on the amount of carbon, in CO + H2, using thermogravimetric analysis and Raman-spectroscopy as well as scanning and transmission electron microscopy. All of the FexOy resulted in similar carbon formation. The effect of the grain size and specific surface particles was demonstrated, in particular due to the large decrease in the catalyst particle size. This study could be helpful for the future development of new refractories materials in reducing conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced materials and composites · Carbon Nanotubes in Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Les phénomènes de combustion dans les foyers industriels
2. The predictability of co resistance of refractory materials by state-of-the-art test methods—a technical and scientific approach
3. Carbon formation from carbon monoxide–hydrogen mixtures over iron catalysts: II. Rates of carbon formation10.1021/j150572a003 ↗
4. Catalytic effect of iron on decomposition of carbon monooxide: I. Carbon deposition in H2–CO mixtures10.1007/BF02642919 ↗
5. The influence of carbon deposition on the reduction kinetics of commercial grade hematite pellets with CO, H2 and N210.1007/BF02654354 ↗
6. Formation and characterization of catalytic carbons obtained from CO disproportionation over an Iron Nickel Catalyst — I fragmentation and rates of carbon deposition10.1016/0008-6223(81)90113-5 ↗
7. Micromechanisms of metal dusting on Fe-base and Ni-base alloys10.1002/(SICI)1521-4176(199805)49:5<309::AID-MACO309>3.0.CO;2-1 ↗
8. Thermodynamics, mechanisms and kinetics of metal dusting10.1002/(SICI)1521-4176(199805)49:5<303::AID-MACO303>3.0.CO;2-P ↗
9. Study of Metal Dusting Mechanism in Iron Using Raman
10. Investigation of metal-dusting mechanism in Fe-base alloys using Raman spectroscopy, X-ray diffraction, and electron microscopy10.1023/A:1016068625429 ↗
11. Ranzani da Costa · 2011
12. Decomposition of Methane over iron catalysts at the range of moderate temperatures: the influence of structure of the catalytic systems and the reaction conditions on the yield of carbon and morphology of carbon filaments10.1006/jcat.2001.3243 ↗
13. Filamentous carbon formation caused by catalytic metal particles from iron oxide10.1002/maco.200303742 ↗
14. Raman spectroscopy of amorphous, nanostructured, diamond-like carbon, and nanodiamond10.1098/rsta.2004.1452 ↗
15. How to obtain a reliable structural characterization of polished graphitized carbons by Raman microspectroscopy10.1002/jrs.3014 ↗
16. Determination of crystallite size in polished graphitized carbon by Raman spectroscopy10.1103/PhysRevB.86.134205 ↗
17. Characterizing various types of defects in nuclear graphite using Raman scattering: heat treatment, ion irradiation and polishing10.1016/j.carbon.2015.07.095 ↗
18. Graphitization at low temperatures (600–1200(C)) in the presence of iron implications in planetology10.1016/j.carbon.2013.08.056 ↗
19. Relative crystallographic orientations of carvon and metal in a filamentous catalytic carbon10.1016/0008-6223(80)90080-9 ↗
20. FIlamentous carbon growth on nickel–iron surfaces: the effect of various oxide additives10.1016/0021-9517(80)90518-7 ↗
21. Hydrogen control of carbon deposit morphology10.1016/0008-6223(94)00122-G ↗
22. Carbon depostion over Fe, Ni, and Co foils and CO–H2–H20 gas mixtures: I. Morphology10.1016/0008-6223(92)90111-9 ↗
23. Rouzaud J-N, high temperature iron-based catalysts for hydrogen and nanostructured carbon production by methane decomposition10.1016/j.ijhydene.2011.01.184 ↗