journal article·2000-12

Room and elevated temperature tensile properties of single tow Hi-Nicalon, carbon interphase, CVI SiC matrix minicomposites

J. Martı́nez-Fernández, G.N. Morscher

Journal of the European Ceramic Society· Volume 20· Issue 14-15
Publisher page

Abstract

Single tow Hi-Nicalon(TM), C interphase, CVI SiC matrix minicomposites were tested in tension at room temperature, 700 C, 950 C, and 1200 C in air. Monotonic loading with modal acoustic emission monitoring was performed at room temperature in order to determine the dependence of matrix cracking on applied load. Modal acoustic emission was shown to correlate directly with the number of matrix cracks formed. Elevated temperature constant load stress-rupture and low-cycle fatigue experiments were performed on precracked specimens. The elevated temperature rupture behavior was dependent on the precrack stress, the lower precrack stress resulting in longer rupture life for a given stress. It was found that the rupture lives of C-interphase Hi-Nicalon(TM) minicomposites were superior to C-interphase Ceramic Grade Nicalon(TM) minicomposites and inferior to those of BN-interphase Hi-Nicalon(TM) minicomposites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
2. Tensile stress rupture of SiCf/SiCm minicomposites with carbon and boron nitride interphases at elevated temperatures in air10.1111/j.1151-2916.1997.tb03087.x ↗
3. Lara-Curzio, E., Ferber, M. K. and Tortorelli, P. F., Interface Oxidation and Stress–Rupture of Nicalon, TM/SiC CFCCs at Intermediate Temperatures. Key Engineering Materials, Vols. 127–131. Trans. Tech. Publications, Switzerland, 1997, pp. 1069–1082.10.4028/www.scientific.net/KEM.127-131.1069 ↗
4. Stress–rupture of Nicalon/SiC continuous fiber ceramic matrix composites in air at 950°C10.1111/j.1151-2916.1997.tb03266.x ↗
5. Atmospheric effects on high-temperature lifetime of ceramic composites10.1002/9780470294444.ch42 ↗
6. Verrilli, M. J., Calomino, A. M. and Brewer, D. N., Creep–rupture behavior of a Nicalon/SiC composite. In Thermal and Mechanical Test Methods and Behavior of Continuous-Fiber Ceramic Composites (ASTM STP 1309), ed. M. G. Jenkins, S. T. Gonczy, E. Lara-Curzio, N. E. Ashbaugh and L. Zawada. ASTM, 1997, pp. 158–175.10.1520/STP11819S ↗
7. Stress rupture of an enhanced Nicalon™/SiC composite at intermediate temperatures10.1111/j.1151-2916.1998.tb02598.x ↗
8. Theory of mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
9. Strength, structure, and fracture properties of ceramic fibers produced from polymeric precursors: I, base-line studies10.1111/j.1151-2916.1987.tb05631.x ↗
10. Fiber-matrix interphases and interfaces in ceramic matrix composites processed by CVI10.1163/156855493X00112 ↗
11. Effect of coating on lifetime of nicalon fiber-silicon carbide composites in air, Mater10.1016/S0921-5093(97)00079-8 ↗
12. High-temperature oxidation of boron nitride: II, boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
13. Determination of interfacial properties using a single fiber microcomposite test10.1111/j.1151-2916.1996.tb08551.x ↗
14. Thermomechanical behavior of advanced SiC fiber multifilament tows10.1002/9780470314876.ch5 ↗
15. A time-temperature relationship for rupture and creep stresses
16. Conway, J. B., Numerical methods for creep and rupture analyses. Gordon and Breach, Science Publ., New York, pp. 155–177.
17. Yun H. M. and DiCarlo, J. A., Time/temperature dependent tensile strength of SiC and Al2O3-based fibers. In Ceramic Transactions, Vol. 74, Advances in Ceramic-Matrix Composites III, ed. N. P. Bansal and J. P. Singh, 1996, pp. 17–26.
18. The effect of static and cyclic tensile stress and temperature on failure for precracked Hi-Nicalon/BN/CVD SiC minicomposites in air10.1002/9780470294437.ch80 ↗
19. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
20. Oxidation of a continuos carbon phase in a nonreactive matrix10.1111/j.1151-2916.1995.tb08424.x ↗
21. Fiber effects on minicomposite mechanical properties for several silicon carbide fiber-chemically vapor-infiltrated silicon carbide matrix systems10.1111/j.1151-2916.1999.tb01734.x ↗
22. Modal acoustic emission of damage accumulation in a woven SiC/SiC composite10.1016/S0266-3538(98)00121-3 ↗