The influence of ZnO in fayalite slag on the degradation of magnesia-chromite refractories during secondary Cu smelting
Source abstract
Abstract
Abstract In order to study the role of ZnO in the degradation of magnesia-chromite refractories, the chemical corrosion behaviour in a ZnO-containing fayalite slag (FeO–SiO 2 –ZnO–Al 2 O 3 ) is investigated using a rotating magnesia-chromite refractory finger corrosion test under a reducing atmosphere at 1200 °C. The results show that, likewise to ZnO-free fayalite slag, periclase is predominantly corroded. Both ZnO and FeO diffused into the original periclase and chromite grains thereby forming, respectively, (Zn,Fe,Mg)O solid solution and (Zn,Fe,Mg)[Cr,Al,Fe] 2 O 4 spinel. Concurrently, ZnO and FeO were also incorporated into the (Zn,Fe,Mg) 2 SiO 4 olivine during its formation. None of these phase formations resulted in new crack generation in the refractory. Considering the infiltrated slag is almost completely depleted in ZnO at 4 mm from the hot face, the severe slag penetration up to the centre of the refractory sample is not caused by the ZnO presence in the initial slag.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Petkov · 2007
2. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
3. A study of basic brick from copper anode furnaces10.1111/j.1151-2916.1961.tb15360.x ↗
4. Wear of chrome magnesite bricks in copper smelting furnaces
5. Mechanisms of refractory wear in copper converters
6. Factors affecting the corrosion by fayalite slags and the thermal shock performance of magnesia-chrome bricks
7. Thermodynamic modeling of the FeO–Fe2O3–MgO–SiO2 system10.1111/j.1151-2916.2002.tb00554.x ↗
8. International Copper Study Group · 2013
9. Secondary copper processing using Outotec Ausmelt TSL technology
10. Rentz · 1999
11. Diffusion of Zn2+ in single-crystal MgO10.1063/1.1695903 ↗
12. The system MgO–ZnO–SiO210.1111/j.1151-2916.1965.tb14778.x ↗
13. Failure mechanisms of refractory linings for non-ferrous flashsmelting furnaces
14. Viscosity and electrical–conductivity of Na2O–SiO2–ZnO and CaO–SiO2–ZnO10.2320/jinstmet1952.46.3_280 ↗
15. Modeling the viscosity of silicate melts containing zinc oxide10.1016/j.calphad.2011.09.005 ↗
16. The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO–SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
17. Chemical corrosion mechanisms of magnesia–chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
18. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
19. Experimental study of phase equilibria in the systems Fe–Zn–O and Fe–Zn–Si–O at metallic iron saturation10.1007/s11663-000-0006-2 ↗
20. Penetration and corrosion of magnesia grain by silicate slags10.1179/096797800681036 ↗
21. Reactions of dense MgO with calcium ferrite-based slags at 1573K10.1007/s11663-005-0055-7 ↗
22. Grain–boundary reactions in magnesia-chrome refractories: application of the electron probe, II10.1111/j.1151-2916.1966.tb13178.x ↗