Self-glazed zirconia reducing the wear to tooth enamel

Yihong Liu, Yong Wang, Dianzheng Wang, Jing Ma, Leifeng Liu, Zhijian Shen

Publisher page

Abstract

Abstract The wear behaviors of a newly developed grade of self-glazed zirconia against the enamel of freshly extracted teeth were investigated under simulated oral stresses and chemical environment. It was revealed that an inherently formed enamel-like surface on self-glazed zirconia that is very smooth on micrometer scale yet with nanoscale roughness has almost the same frictional coefficient against tooth enamel as the well-polished zirconia surface. The wear scars observed on the worn surface of enamel against self-glazed zirconia and well-polished zirconia surface revealed that in both cases fatigue wear is the dominating wear mechanism. It was concluded that the friction and wear performances of both the well-polished and self-glazed zirconia ceramics against natural enamel were very similar, which bears a very strong implication for the clinical safe use of the full contour zirconia restorations, yet the self-glazed zirconia provides sufficiently improved aesthetic appearance that ensures its potential for direct clinical uses.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Temporomandibular Joint Disorders

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Prospective study of zirconia-basedrestorations: 3-year clinical results
2. Fracture and interfacial delamination origins of bilayer ceramic composites for dental restorations10.1016/j.jeurceramsoc.2009.11.019 ↗
3. Failure modes and fracture origins of porcelain veneers on bilayer dental crowns10.11607/ijp.3608 ↗
4. In vitro failure and fracture resistance of veneered and full-contour zirconia restorations10.1016/j.jdent.2012.07.010 ↗
5. Properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulation10.1016/j.jdent.2014.08.011 ↗
6. Friction and wear behaviors of dental ceramics against natural tooth enamel10.1016/j.jeurceramsoc.2012.03.021 ↗
7. Wear of human enamel opposing monolithic zirconia, glass ceramic, and composite resin: an in vitro study10.1016/j.prosdent.2014.05.006 ↗
8. Clinical and laboratory surface finishing procedures for zirconia on opposing human enamel wear: a laboratory study10.1016/j.jmbbm.2015.06.007 ↗
9. Influence of artificial saliva on abrasive wear and microhardness of dental composites filled with nanoparticles10.1016/j.jdent.2008.05.001 ↗
10. Effect of the number of coloring liquid applications on the optical properties of monolithic zirconia10.1016/j.dental.2014.04.008 ↗
11. On the friction and wear behavior of human tooth enamel and dentin10.1016/S0043-1648(03)00079-6 ↗
12. SEM observations of Retzius lines and prism cross-striations in human dental enamel after different acid etching regimes10.1016/S0003-9969(03)00195-X ↗
13. Clinical enamel surface changes following an intra-oral acidic challenge10.1016/j.jdent.2015.04.002 ↗
14. Wear: mechanisms, manifestations and measurement10.1016/0300-5712(95)00043-7 ↗
15. The fracture behaviour of dental enamel10.1016/j.biomaterials.2009.09.050 ↗