Fast interdiffusion and Kirkendall effects of SiC-coated C/SiC composites joined by a Ti-Nb-Ti interlayer via spark plasma sintering

Xing Zhao, Liuyang Duan, Yiguang Wang

Publisher page

Abstract

Abstract SiC-coated 3D C/SiC composites were successfully joined with a Ti-Nb-Ti interlayer by SPS. When joined at 1200 °C, the apparent shear strength of the samples was as high as 61 ± 6 MPa as a result of an appropriate interface diffusion reaction. However, higher joining temperature (1600 °C) resulted in significantly lower shear strengths, and this was associated with the observed depletion of Si atoms and Kirkendall voids at the joining interface. Subsequently, a detailed characterization was performed by FIB/TEM/STEM. The interdiffusion mechanism of the samples during the joining process was revealed by thermodynamics and diffusion kinetics, and different interdiffusion mechanisms were associated with the evolution of the phase composition. The micro voids formed via Kirkendall effect were observed to grow rapidly with the joining temperature, resulting in catastrophic joint failure. Finally, these results were used to propose a failure model for the joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
2. Recent progress in the development of SiC composites for nuclear fusion applications10.1016/j.jnucmat.2018.06.017 ↗
3. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
4. Silver assisted crack healing in SiC10.1016/j.actamat.2015.11.052 ↗
5. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
6. Postirradiation fiber debonding and pull-out in SiC-SiC composites10.1016/0022-3115(94)90174-0 ↗
7. Ablation behavior of C/SiC composites in plasma wind tunnel10.1016/j.carbon.2016.02.085 ↗
8. Ablation behavior of C/SiC-HfC composites in the plasma wind tunnel10.1016/j.jeurceramsoc.2016.03.017 ↗
9. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
10. Secure tightening of a CMC fastener for the heat shield of re-entry vehicles10.1016/j.compstruct.2009.07.002 ↗
11. Shear and bending strength of SiC/SiC joined by a modified commercial adhesive10.1111/j.1744-7402.2011.02739.x ↗
12. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
13. Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites
14. Reactive brazing Cf/SiC to itself and to Mo using the NiPdPtAu-Cr filler alloy10.1016/j.jeurceramsoc.2017.05.025 ↗
15. Effect of brazing parameters on microstructure and mechanical properties of Cf/SiC and Nb-1Zr joints brazed with Ti-Co-Nb filler alloy10.1016/j.jeurceramsoc.2016.09.031 ↗
16. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
17. Flash joining of CVD-SiC coated Cf/SiC composites with a Ti interlayer10.1016/j.jeurceramsoc.2017.05.016 ↗
18. Effects of z-pin’s porosity on shear properties of 2D C/SiC z-pinned joint10.1016/j.compstruct.2017.04.013 ↗
19. Radiation stable, hybrid, chemical vapor infiltration/preceramic polymer joining of silicon carbide components10.1016/j.jnucmat.2017.02.012 ↗
20. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
21. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using Spark Plasma sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
22. High temperature properties of the monolithic CVD beta-SiC materials joined with a pre-sintered MAX phase Ti3SiC2 interlayer via solid-state diffusion bonding10.1016/j.jeurceramsoc.2016.11.006 ↗
23. Improved shear strength of SiC-coated 3D C/SiC composite joints with a tailored Ti-Si-C interlayer10.1016/j.jeurceramsoc.2018.11.016 ↗
24. Joining of 3D C/SiC composites to niobium alloy10.1016/j.scriptamat.2006.03.050 ↗
25. Understanding the spark plasma sintering from the view of materials joining10.1016/j.scriptamat.2016.06.014 ↗
26. Effects of residual S on Kirkendall void formation at Cu/Sn–3.5Ag solder joints10.1016/j.actamat.2008.07.022 ↗
27. Fe addition to Sn-3.5Ag solder for the suppression of Kirkendall void formation10.1016/j.scriptamat.2013.04.010 ↗
28. Bifurcation of the Kirkendall marker plane and the role of Ni and other impurities on the growth of Kirkendall voids in the Cu-Sn system10.1016/j.actamat.2017.03.068 ↗
29. Mapping of the Nb-Ti-Si phase diagram using diffusion multiples10.1016/j.msea.2003.08.008 ↗
30. Joining of ceramics demonstrated by the example of SiC/Ti10.1016/0955-2219(90)90012-5 ↗
31. Phase reaction and diffusion path of the SiC/Ti system10.1007/s11661-997-0275-3 ↗
32. Investigation of the damage behavior in CVD SiC irradiated with 70 keV He ions by NEXAFS, Raman and TEM10.1016/j.jeurceramsoc.2016.11.046 ↗
33. Growth mechanism of phases by interdiffusion and diffusion of species in the niobium-silicon system10.1016/j.actamat.2010.11.022 ↗
34. Reactive diffusion in the Ti-Si system and the significance of the parabolic growth constant10.1080/14786435.2013.859759 ↗
35. Diffusion pattern in MSi2 and M5Si3 silicides in group VB (M = V, Nb, Ta) and VIB (M = Mo, W) refractory metal-silicon systems10.1080/14786435.2014.888103 ↗
36. Thermal expansion and elastic moduli of the silicide based intermetallic alloys Ti5Si3(X) and Nb5Si310.1016/S1359-6462(97)00496-X ↗
37. Chawla · 1990