Investigation of slag-refractory interactions for the Ruhrstahl Heraeus (RH) vacuum degassing process in steelmaking
Source abstract
Abstract
Abstract In order to determine the effect of slag composition during the RH process on refractory wear, magnesia–carbon and magnesia–chromite refractories were immersed for 10 min at 1600 °C in a ladle slag, two FeO-rich slags (20 and 40 wt% FeO) and two CaO–Al2O3 slags. Corrosion of magnesia–carbon refractory by the ladle and CaO–Al2O3 slags was limited as the refractory carbon phase efficiently prevented slag infiltration. Severe degradation was observed in contact with FeO-rich slags. FeO oxidized the carbon phase with formation of Fe droplets at the hot face. Regarding magnesia–chromite refractory, the corrosion mechanism consisted of severe slag infiltration, high temperature inactivation of the secondary chromite and primary chromite dissolution in the infiltrating slag. The FeO-rich slags seem to have generated more severe conditions as the infiltrating slag pushed apart the periclase grains, leading to severe refractory erosion. The degradation mechanisms are discussed by combining experimental results and thermodynamic calculations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · Iron and Steelmaking Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. A kinetic model for the Ruhrstahl Heraeus (RH) degassing process10.1007/s11663-011-9495-4 ↗
2. FactSage thermochemical software and databases—recent developments10.1016/j.calphad.2008.09.009 ↗
3. Carbon–MgO reactions in BOF refractories
4. Significance of oxidation–reduction reactions within BOF refractories10.1111/j.1151-2916.1971.tb12392.x-i1 ↗
5. Limitations on internal oxidation–reduction reactions in BOF refractories
6. Control of oxidation–reduction in magnesia–carbon refractories
7. Mechanism of dense magnesia layer formation near the surface of magnesia–carbon brick10.1111/j.1151-2916.1986.tb07482.x ↗
8. Effect of slag on carbon bearing MgO refractories
9. Evolution of in situ refractories in the 20th century10.1111/j.1151-2916.1998.tb02497.x ↗
10. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
11. Influence of chemical reactions in magnesia–graphite refractories: I. Effects on texture and high-temperature mechanical properties10.1111/j.1151-2916.1999.tb02276.x ↗
12. Influence of chemical reactions in magnesia–graphite refractories: II. Effects of aluminum and graphite contents in generic products10.1111/j.1151-2916.1999.tb02277.x ↗
13. Influence of additives on corrosion resistance and corroded microstructures of MgO–C refractories10.1016/S0955-2219(01)00208-4 ↗
14. Behaviour of magnesia–carbon refractories in vacuum-oxygen decarburisation ladle linings10.1179/030192303225003971 ↗
15. Degradation of MgO–C refractories by MnO-rich stainless steel slags10.1016/j.ceramint.2008.12.007 ↗
16. Penetration and corrosion of magnesia grain by silicate slags10.1179/096797800681036 ↗
17. Phenomenon of exsolution precipitates in the periclase solid solution of the system MgO–Al2O3–Fe2O3–Cr2O310.2109/jcersj1950.84.970_271 ↗
18. The direct bond in magnesia chromite and magnesia spinel refractories10.1111/j.1151-2916.1995.tb08885.x ↗
19. A study of slag-infiltrated magnesia–chromite refractories using hybrid microwave heating10.1016/S0955-2219(00)00343-5 ↗
20. Volume expansion and structural damage in periclase-chrome refractories
21. Refractory wear in the argon-oxygen-decarburization process
22. Fused basic refractories in the argon-oxygen decarburization process
23. Slag testing of refractories for ladle refining by ESR method
24. Texture and slag resistance of commercial fused magnesia–chrome clinkers
25. Application of high chromia magnesia chrome refractories to secondary refining systems
26. Effect of coal slag on the microstructure and creep behavior of a magnesium chromite refractory
27. Refractory/slag systems for ladles and secondary refining processes. Part XIII
28. New high-quality MgO–Cr2O3-bricks and Cr-free alternatives for the lining of RH/DH-vessels
29. Extending the life of ALZ NV's VOD ladle lining
30. Degradation mechanisms of magnesia–chromite refractories in vacuum-oxygen decarburisation ladles during production of stainless steel10.1179/030192300677525 ↗
31. Degradation mechanisms of magnesia–chromite refractories by high-alumina stainless steel slags under vacuum conditions10.1016/j.jeurceramsoc.2005.12.025 ↗
32. Using confocal scanning laser microscopy for the in situ study of high-temperature behavior of complex ceramic materials10.1016/j.jeurceramsoc.2007.01.022 ↗
33. Recent developments in research on basic refractories. 2. Microstructural relations in basic refractories