Corrosion and recession of mullite in water vapor environment

Shunkichi Ueno, Tatsuki Ohji, Hua-Tay Lin

Publisher page

Abstract

Abstract In the development of environmental barrier coating system for silicon nitride ceramic, a corrosion behavior of mullite was examined under static state water vapor environment at elevated temperatures. Results showed that a small amount of sodium, which was present in mullite bulk as an impurity, accelerated the water vapor corrosion of silica component and decomposition of mullite into alumina phase. To improve the selective corrosion of the boundary phase in silicate compounds, a mullite/Lu 2 Si 2 O 7 eutectic system without boundary glassy phase was developed. The eutectic composition was Al 2 O 3 :SiO 2 :Lu 2 O 3 = 27.3:54.6:18.1 in molar ratio and the eutectic temperature was estimated to be ∼1500–1520 °C. No weight loss was measured after the static state water vapor corrosion test at 1300 °C for 100 h. However, the recession of mullite phase in the eutectic oxide occurred after exposure to high speed steam jet environment at 1200 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Water vapor effects on high-temperature oxidation and volatilization of ceramics10.1111/j.1151-2916.2003.tb03458.x ↗
2. Additive effects on Si3N4 oxidation/volatilization in water vapor10.1111/j.1151-2916.2003.tb03462.x ↗
3. High-temperature stability of SiC-based composites in high-water-vapor-pressure environments10.1111/j.1151-2916.2003.tb03463.x ↗
4. Development and evaluation of ceramic components for gas turbine
5. Mechanical reliability evaluation of silicon nitride ceramic components after exposure in industrial gas turbines10.1016/S0955-2219(02)00146-2 ↗
6. Evaluation of Mechanical Reliability of Silicon Nitride Vanes After Field Tests in an Industrial Gas Turbine
7. Development of oxide-based EBC for silicon nitride10.1111/j.1744-7402.2004.tb00187.x ↗
8. Upper temperature limit of environmental barrier coatings based on mullite and BSAS10.1111/j.1151-2916.2003.tb03466.x ↗
9. Comparison of water vapor corrosion mechanisms of polycrystalline and eutectic Lu2Si2O7
10. Decomposition of mullite10.1111/j.1151-2916.1972.tb11218.x ↗
11. Water vapor corrosion of mullite containing small amount of sodium10.1016/j.ceramint.2004.03.044 ↗
12. Corrosion behavior of Al2O3 in static state water vapor environment at high temperature10.1023/B:JMSC.0000044908.23241.e5 ↗
13. Iler · 1979
14. Molten-salt corrosion of silicon nitride: I sodium carbonate10.1111/j.1151-2916.1988.tb05828.x ↗
15. Molten-salt corrosion of silicon nitride: II sodium sulfate10.1111/j.1151-2916.1988.tb05828.x ↗
16. Comparison of water vapor corrosion behavior of silicon nitride with various EBC layers
17. Phase-equilibria and properties of glasses in the Al2O3–Yb2O3–SiO2 system10.2109/jcersj.101.1101 ↗
18. Recession behavior of Lu2Si2O7/mullite eutectic in steam jet at high temperature10.1007/s10853-005-2095-4 ↗
19. Exposure test of Lu2Si2O7 in combustion gas flow at high temperature and high speed