Abstract

Abstract Dense ZrB2 containing 15 vol.% SiC and 15 vol.% graphite was exposed to flowing air at 1500 °C. A layered scale structure developed that consisted of (1) a uniform SiO2-rich layer on the surface, (2) a layer of ZrO2 and SiO2, (3) a layer of ZrO2 (4) a partially oxidized layer composed of porous ZrB2, ZrO2, and graphite, and (5) unaffected ZrB2–SiC–C. A thermodynamic model based on volatility diagrams and consistent with the experimental observations was constructed to explain the development of the layered structure. Oxidation behavior was consistent with passive oxidation and formation of a protective surface layer. Analysis indicated that it may not be possible to form a protective surface layer without actively oxidizing SiC and producing a porous partially oxidized layer between the outer protective layer and the underlying unoxidized material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Evaluation of ultra high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
2. Development and characterization of metal–diboride-based composites toughened with ultra-fine SiC particulates10.1016/j.solidstatesciences.2005.02.007 ↗
3. The resistance to oxidation of an HfB2–SiC composite10.1016/j.jeurceramsoc.2004.05.009 ↗
4. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
5. The hypersonic environment: required operating conditions and design challenges10.1023/B:JMSC.0000041688.68135.8b ↗
6. Oxidation of ZrB2–SiC ceramics under atmospheric and reentry conditions
7. Oxidation behavior of a pressureless sintered ZrB2–MoSi2 ceramic composite10.1557/JMR.2005.0111 ↗
8. Oxidation of ZrB2-based ceramics in dry air10.1149/1.1618226 ↗
9. Oxidation of ultra high temperature ceramics in water vapor10.1149/1.1786929 ↗
10. High temperature behavior of plasma sprayed ZrB2–SiC composite coatings
11. Mechanical properties of ceramic matrix composite for high temperature applications obtained by plasma spraying
12. Processing and properties of zirconium diboride-based composites10.1016/S0955-2219(01)00284-9 ↗
13. Engineering properties of borides
14. High-temperature oxidation: III. Zirconium and hafnium diborides10.1149/1.2424154 ↗
15. The Oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures10.1149/1.2426263 ↗
16. Thermogravimetric study of the oxidation of ZrB2 in the temperature range of 800–1500°C10.1149/1.2408279 ↗
17. Oxidation of titanium diboride and zirconium diboride at high temperatures10.1016/0022-5088(68)90067-2 ↗
18. Oxidation behavior of zirconium diboride
19. Short-term oxidation of a ternary composite in the system AlN–SiC–ZrB210.1016/j.jeurceramsoc.2004.12.007 ↗
20. Oxidation of zirconium diboride–silicon carbide at 1500°C in a low partial pressure of oxygen10.1111/j.1551-2916.2006.01229.x ↗
21. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
22. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
23. Selection of materials for use at temperatures above 1500°C in oxidizing atmospheres10.1016/S0955-2219(98)00247-7 ↗
24. Strength and scaling resistance of a composite based on zirconium diboride10.1007/BF02227282 ↗
25. Oxidation behavior of graphite–B4C/SiC/ZrB2 composite in dry and moist atmosphere10.2109/jcersj.100.398 ↗
26. High temperature properties of refractory composites
27. Effect of an SiC addition on the oxidation of ZrB2
28. Oxidation of ZrB2- and HfB2-based ultra-high temperature ceramics: effect of Ta additions10.1023/B:JMSC.0000041693.32531.d1 ↗
29. Processing, properties, and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics10.1023/B:JMSC.0000041689.90456.af ↗
30. Oxidation of ZrB2–SiC10.1002/9780470294680.ch27 ↗
31. Synthesis of oxidation resistance metal diboride composites
32. Some new perspective on oxidation of silicon carbide and silicon nitride10.1111/j.1151-2916.1991.tb04348.x ↗
33. Reactions of silicon carbide and silicon (IV) oxide at elevated temperatures10.1111/j.1151-2916.1992.tb04232.x ↗
34. High strength ZrB2-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
35. Effect of hot pressing time and temperature on the microstructure and mechanical properties of ZrB2–SiC10.1007/s10853-006-1274-2 ↗
36. Beneficial effects of ultra-fine α-SiC incorporated on the sinterability and mechanical properties of ZrB210.1007/s00339-005-3327-9 ↗
37. Evolution of Structure During the Oxidation of Zirconium Diboride-Silicon Carbide in Air up to 1500(C10.1016/j.jeurceramsoc.2006.10.012 ↗
38. Review – graphical displays of the thermodynamics of high temperature gas–solid reactions and their application to oxidation of metals and evaporation of oxides10.1111/j.1151-2916.1985.tb15264.x ↗
39. Volatility diagrams for silica, silicon nitride, and silicon carbide and their application to high temperature decomposition and oxidation10.1111/j.1151-2916.1990.tb06677.x ↗
40. Theoretical and experimental approach to the active-to-passive transition in the oxidation of silicon carbide experiments at high temperatures and low total pressures10.1023/A:1004313022769 ↗
41. Corrosion of silicon–based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗