journal article·2016-01

Crack healing induced electrical and mechanical properties recovery in a Ti 2 SnC ceramic

Shibo Li, Guoping Bei, Xiaodong Chen, Linquan Zhang, Yang Zhou, Mirza Mačković, Erdmann Spiecker, Peter Greil

Publisher page

Abstract

Abstract Ceramics are able to heal cracks and flaws by triggering local sintering (internal cracks) or oxidation reaction (surface cracks) which may induce the recovery of mechanical strength. Crack healing in ceramics, however, is limited to micro-sized cracks and requires elevated temperatures (above 1000 °C) and long time periods even up to 100 h. In this work we report on accelerated crack healing of a Ti 2 SnC ceramic which is capable to repair thermal shock induced cracks at a relatively low temperature of 800 °C within only 1 h. After healing treatment both the low flexural strength and electrical conductivity measured on the damaged material after quenching were almost fully recovered. Furthermore, Ti 2 SnC exhibits repeatable healing capability which offers a high potential for developing durable ceramics with prolonged lifetime under harsh thermal conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · 2D Materials and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Self-healing behaviour in man-made engineering materials: bioinspired but taking into account their intrinsic character10.1098/rsta.2009.0020 ↗
2. van der Zwaag · 2007
3. Ghosh · 2009
4. Self-healing polymers and composites10.1146/annurev-matsci-070909-104532 ↗
5. Generic principles of crack-healing ceramics10.1007/s40145-012-0020-2 ↗
6. The influence of annealing on the strength of corundum crystals
7. Spheroidization of tubular voids in Al2O3 crystals at high temperatures10.1111/j.1151-2916.1972.tb13417.x ↗
8. High-temperature healing of lithographically introduced cracks in sapphire10.1111/j.1151-2916.1990.tb06558.x ↗
10. Healing of lithographically introduced cracks in glass and glass-containing ceramics10.1111/j.1151-2916.1998.tb02743.x ↗
12. Crack healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗
13. Healing of surface cracks in SiC by oxidation10.1111/j.1151-2916.1970.tb12104.x ↗
14. Effects of oxidation under load on strength distribution of Si3N410.1111/j.1151-2916.1982.tb10451.x ↗
15. Crack-healing behavior and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900, 1000°C)10.1016/S0955-2219(02)00428-4 ↗
16. Crack-healing behavior of Al2O3 toughened by SiC whiskers10.1111/j.1151-2916.2003.tb03622.x ↗
17. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
18. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
19. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
20. Self-healing performance of Ti2AlC ceramic10.1039/c2jm16123k ↗
21. Oxidation and self-healing behavior of a fine-grained Cr2AlC ceramic10.1111/jace.12170 ↗
22. Theoretical investigation of A-element atom diffusion in Ti2AC (A=Sn, Ga, Cd, In, and Pb)10.1063/1.3130093 ↗
23. The Mn+1AXn phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
24. Fabrication and characterization of M2SnC (M=Ti, Zr, Hf and Nb)10.1016/S1359-6462(97)00288-1 ↗
25. Preparation of Ti2SnC by solid–liquid reaction synthesis and simultaneous densification method10.1007/s10019-002-0200-8 ↗
26. Solid–liquid reaction synthesis and thermal stability of Ti2SnC10.1039/b008973g ↗
27. Oxidation behavior of MAX phase Ti2Al(1−x)SnxC solid solution10.1111/jace.12358 ↗
28. Bimodal microstructure and reaction mechanism of Ti2SnC synthesized by high temperature reaction using Ti/Sn/C and Ti/Sn/TiC powder compacts10.1111/j.1551-2916.2006.01275.x ↗
29. Synthesis of Ti2SnC at low-temperature using mechanically activated sintering process10.1016/j.msea.2007.01.095 ↗
30. Low-temperature instability of Ti2SnC: a combined transmission electron microscopy, differential scanning calorimetry, and X-ray diffraction investigations10.1557/JMR.2009.0012 ↗
31. Crack healing in Ti2Al0.5Sn0.5C–Al2O3 composites10.1111/jace.13496 ↗
32. High-temperature oxidation behavior of a polycrystalline Ti2SnC ceramic10.1023/B:OXID.0000032329.73914.55 ↗
33. Dean · 1992
34. Carney · 2006
35. Synthesis and characterization of Hf2PbC, Zr2PbC and M2SnC (M=Ti, Hf, Nb or Zr)10.1016/S0955-2219(00)00127-8 ↗
36. Thermal expansion of anatase and rutile between 300 and 575K using synchrotron powder X-ray diffraction10.1154/1.2790965 ↗
37. The surface and materials science of tin oxide10.1016/j.progsurf.2005.09.002 ↗
38. Ho · 1998
39. Electrical conductivity, seebeck coefficient and optical properties of SnO2 film deposited on ITO by dip coating10.1016/j.jallcom.2008.03.013 ↗
40. High strength, electrically conductive pore-free TiO2 ceramics made by hot isostatic pressing10.1557/JMR.1997.0147 ↗