journal article·2012-02

Effect of intergranular phase chemistry on the sliding-wear resistance of pressureless liquid-phase-sintered α-SiC

E. Ciudad, O. Borrero-López, F. Rodríguez-Rojas, A.L. Ortiz, F. Guiberteau

Publisher page

Abstract

Abstract The effect was investigated of the intergranular phase chemistry on the sliding-wear resistance of pressureless liquid-phase-sintered (PLPS) α-SiC densified with 10 vol.% 5Al 2 O 3 + 3RE 2 O 3 (RE = La, Nd, or Yb) additives. It was found that the sliding-wear behaviour of these ceramics is similar to what is observed in other polycrystalline ceramics: initial mild, plasticity-controlled wear followed by severe, fracture-controlled wear, with a well-defined wear transition. Most importantly, the sliding-wear resistance of PLPS SiC is found to increase with decreasing size of the RE 3+ cation in the rare-earth oxide additive, with a lower susceptibility to mild and severe wear and a delayed transition to severe wear. Underlying this effect is likely the hardening of the intergranular phase resulting from the increase in the field strength of the RE 3+ –O 2− bonds as the size of the RE 3+ cation decreases. Tailoring the intergranular phase chemistry via the selection of RE 2 O 3 sintering additives with cations as small as possible thus emerges as a potentially interesting approach to improving the sliding-wear resistance of PLPS SiC ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Meetham · 2000
2. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
3. Micro- and macro-tribological properties of SiC ceramics in sliding contact10.1016/S0043-1648(01)00595-6 ↗
4. Thermal conductivity of liquid phase sintered silicon carbide10.1016/S0955-2219(02)00271-6 ↗
5. Melting points, crystallographic transformation and thermodynamic values
6. Effect of boron and carbon on sintering of SiC10.1111/j.1151-2916.1975.tb18990.x ↗
7. Sintering of silicon carbide with rare-earth oxide additives
8. Densification of liquid-phase-sintered silicon carbide10.1023/A:1006753213286 ↗
9. Core/rim structure of liquid-phase-sintered silicon carbide10.1111/j.1151-2916.1993.tb03677.x ↗
10. Effect of intergranular phase chemistry on the microstructure and mechanical properties of silicon carbide ceramics densified with rare-earth oxide and alumina additives10.1111/j.1151-2916.2001.tb00891.x ↗
11. Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
12. Grain-size and R-curve effects in the abrasive wear of alumina10.1111/j.1151-2916.1989.tb09718.x ↗
13. The transition from mild to severe wear in alumina during sliding10.1016/0956-7151(92)90212-W ↗
14. Wear and wear transition mechanisms of ceramics10.1016/0043-1648(95)06800-7 ↗
15. Wear-resistant ultra-fine-grained ceramics10.1016/j.actamat.2004.09.020 ↗
16. Stepwise-graded Si3N4–SiC ceramics with improved wear properties10.1111/j.1151-2916.2002.tb00404.x ↗
17. Effect of microstructure on sliding-wear properties of liquid-phase-sintered α-SiC10.1111/j.1551-2916.2005.00394.x ↗
18. Improved sliding-wear resistance in in-situ toughened silicon carbide10.1111/j.1551-2916.2005.00628.x ↗
19. Sliding-wear-resistant liquid-phase sintered SiC processed using α-SiC starting powders10.1111/j.1551-2916.2006.01421.x ↗
20. Effect of the nature of the intergranular phase on sliding-wear resistance of liquid-phase-sintered α-SiC10.1016/j.scriptamat.2007.05.021 ↗
21. Microstructural evolution in liquid-phase-sintered SiC. Part I. Effect of starting powder10.1111/j.1151-2916.2001.tb00880.x ↗
22. Green · 1998
23. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
24. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
25. Hertzian Contacts
26. Oxidation behaviour of pressureless liquid-phase-sintered α-SiC with additions of 5Al2O3+3RE2O3 (RE=La, Nd, Y, Er, Tm, or Yb)10.1016/j.jeurceramsoc.2010.07.013 ↗
27. Hardness degradation in liquid-phase-sintered SiC with prolonged sintering10.1016/j.jeurceramsoc.2007.02.189 ↗
28. The cation field strengths and their relation to devitrifying process to compound formation and to the melting points of silicates
29. Making ceramics “ductile”10.1126/science.263.5150.1114 ↗
30. Model for toughness curves in two-phase ceramics. I. Basic fracture mechanics10.1111/j.1151-2916.1993.tb07759.x ↗
31. Model for toughness curves in two-phase ceramics. II. Microstructural variables10.1111/j.1151-2916.1993.tb07760.x ↗
32. Thermal expansion of rare-earth aluminum garnets