journal article·2015-02

Passive/active oxidation transition for CMC structural materials designed for the IXV vehicle re-entry phase

M. Balat-Pichelin, L. Charpentier, F. Panerai, O. Chazot, B. Helber, K. Nickel

Publisher page

Abstract

Abstract This paper reports the experimental results of oxidation studies for the determination of the transition between passive and active oxidation of two silicon carbide-based materials produced by Herakles-Safran (France) and MT Aerospace (Germany) with also the study of the oxidation kinetics in the active zone for the highest heating conditions of the Intermediate eXperimental Vehicle (IXV) re-entry trajectory. The transition between active and passive oxidation is determined for both materials using two different plasma facilities – a low enthalpy one using the MESOX at PROMES-CNRS (Font-Romeu Odeillo, France) and a high enthalpy one using the Plasmatron at VKI (Rhode St Genese, Belgium) – and the experimental results lead to the same transition law. Characterization by SEM of the oxidized samples (surface and cross-section) is shown. Mass loss rates in active oxidation conditions are reported for both Herakles and MTA materials.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Active to passive transition in the oxidation of silicon carbide at high temperature and low pressure in molecular and atomic oxygen10.1007/BF02403882 ↗
2. Determination of the active-to-passive transition in the oxidation of silicon carbide in standard and microwave-excited air10.1016/0955-2219(95)00104-2 ↗
3. The role of condensed silicon monoxide in the active-to-passive oxidation transition of silicon carbide10.1016/0955-2219(92)90070-T ↗
4. High temperature kinetics of the oxidation and nitridation of pyrolytic silicon carbide in dissociated gases10.1021/j100704a002 ↗
5. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
6. Active-to-passive transition in the oxidation of silicon carbide and silicon nitride in air10.1111/j.1151-2916.1990.tb09793.x ↗
7. Theoretical investigation for the active-to-passive transition in the oxidation of silicon carbide10.1111/j.1551-2916.2008.02353.x ↗
8. High-temperature oxidation behavior of SiC-coated carbon fiber-reinforced carbon matrix composites10.1016/S1359-835X(98)00143-2 ↗
9. Endurance test of oxidation-resistant CVD-SiC coating on C/C composites for space vehicle10.2320/matertrans.42.825 ↗
10. Thermal response and oxidation of Tyranno-fiber-reinforced Si–Ti–C–O matrix composites for a thermal protection system in high-enthalpy dissociated air10.1111/j.1151-2916.2003.tb03383.x ↗
11. High temperature oxidation of sintered silicon carbide under pure CO2 at low pressure: active–passive transition10.1016/S0169-4332(98)00193-7 ↗
12. Oxidation of sintered silicon carbide under microwave-induced CO2 plasma at high temperature: active–passive transition10.1016/S0169-4332(00)00314-7 ↗
13. Investigation of C/SiC breaking point under arc-jet environment at NASA-JSC
14. Oxidation transitions for SiC. Part 1: Active-to-passive transition10.1111/jace.12108 ↗
15. Oxidation transitions for SiC. Part 2: Passive-to-active transition10.1111/jace.12104 ↗
16. Use of volume element methods to understand experimental differences in active/passive transitions and active oxidation rates for SiC10.1111/jace.12141 ↗
17. Neutral oxygen atom density in the MESOX air plasma solar furnace facility10.1016/j.chemphys.2006.03.034 ↗
18. Investigations of passive to active oxidation on C/SiC hot structures
19. Simulation methodology in plasmatron facility and hypersonic wind tunnels
20. TPS ground testing in plasma wind tunnel for catalytic properties determination
21. Condition of simulation of stagnation point heat transfer from high enthalpy flow10.1007/BF01055676 ↗
22. Flight extrapolation of plasma wind tunnel of stagnation region flowfield10.2514/1.17185 ↗
23. The shock tube: a facility for investigations in fluid dynamics10.1063/1.1741395 ↗
24. Stagnation-point heat transfer measurements in dissociated air
25. Characterization of gas/surface interactions for ceramic matrix composites in high enthalpy, low pressure air flow10.1016/j.matchemphys.2012.03.036 ↗
26. Temperature jump phenomenon during plasmatron testing of ZrB2–SiC ultra high-temperature ceramics10.2514/1.T3798 ↗
27. High-temperature passive oxidation of chemically vapor deposited silicon carbide10.1111/j.1151-2916.1989.tb07658.x ↗
28. High-temperature active oxidation of chemically vapor-deposited silicon carbide in an Ar–O2 atmosphere10.1111/j.1151-2916.1991.tb06803.x ↗
29. Thermodynamic analysis of the high-temperature stability of silicon nitride and silicon carbide10.1016/0390-5519(76)90022-3 ↗
30. Thermodata, 38400 Saint Martin d’Hères, France.
31. Feigl · 2005