journal article·2012-09Open access

Microstructure of friction surface developed on carbon fibre reinforced carbon–silicon carbide (Cf/C–SiC)

Yuan Wang, Houzheng Wu

Abstract

We have used TEM to study the microstructure of friction surface of carbon fibre/carbon–silicon carbide composites brake discs after multi braking stop by using organic pads. A friction surface layer was developed consistently on the top of Si regions of the composites, but inconsistently on that of SiC and C. Inside the layer, amorphous silicon/silicon oxides appeared extensively with various non-metallic and metallic crystallites dispersed inside with sizes ranging from a few nanometers to several microns. A coherent interface between the friction layer and the composite surface was established under the braking conditions, whilst its sustainability varied notably in SiC and C regions. Microcracking near the friction surface appeared in SiC and Cf/C regions largely due to the extensive ductile deformation of SiC and weak interfaces between C and Cf. Material joining mechanisms were discussed to enlighten the friction transfer layer development on the surface of the composite discs.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Brake Systems and Friction Analysis · Tribology and Wear Analysis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. C/C–SiC composites for advanced friction systems10.1002/1527-2648(20020717)4:7<427::AID-ADEM427>3.0.CO;2-C ↗
2. High-speed tribological behavior of a carbon/silicon carbide composite10.1016/S0266-3538(00)00124-X ↗
3. Tribological properties of C/C–SiC composites for brake discs10.1007/s12540-010-0061-4 ↗
4. Friction surface evolution of carbon fibre reinforced carbon/silicon carbide (Cf/C–SiC) composites10.1016/j.jeurceramsoc.2010.07.019 ↗
5. Microstructure and tribological properties of 3D needle-punched C/C–SiC brake composites10.1016/j.solidstatesciences.2010.01.014 ↗
6. Preparation and friction behavior of carbon fiber reinforced silicon carbide matrix composites10.1016/j.ceramint.2005.10.008 ↗
7. The role of friction film in friction, wear and noise of automotive brakes10.1016/0043-1648(91)90226-K ↗
8. Wear debris compaction and firction film formation of polymer composites10.1016/0043-1648(89)90110-5 ↗
9. Tribological surfaces on organic brake pads10.1016/S0301-679X(00)00127-4 ↗
10. Third body formation on brake pads and rotors10.1016/j.triboint.2005.04.021 ↗
11. Comprehensive microscopic study of third body formation at the interface between a brake pad and brake disc during the final stage of a pin-on-disc test10.1016/j.wear.2008.11.023 ↗
12. A TEM snapshot of magnetite formation in brakes: the role of the disc's cast iron graphite lamellae in third body formation10.1016/j.wear.2010.11.008 ↗
13. Friction layers and friction films on PMC brakes pads10.1016/j.wear.2003.12.017 ↗
14. Towards a better understanding of bake friction materials10.1016/j.wear.2006.12.020 ↗
15. Understanding the development of the microstructure inside Cf/C–SiC composites manufactured by liquid silicon infiltration
16. C/C–SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
17. An investigation of heterogeneity of the degree of graphitization in carbon–carbon composites10.1016/S0254-0584(03)00332-8 ↗
18. Microstructure of worn pitch/resin/CVI C–C composites10.1016/0008-6223(91)90202-T ↗
19. Effect of sliding speed on the tribological behavior of a PAN–pitch carbon–carbon composite10.1016/0254-0584(94)01427-I ↗
20. The dependence of grain size on stress during dynamic recrystallisation10.1016/0956-7151(91)90295-C ↗
21. Steady-state creep of single-phase crystalline matter at high temperature10.1007/BF00540888 ↗
22. Liquidus and solidus boundaries in the vicinity of order–disorder transitions in the Fe–Si system10.1016/j.scriptamat.2004.09.026 ↗
23. Amorphization and conductivity of silicon and germanium by indentation10.1103/PhysRevLett.60.2156 ↗
24. Survey on wetting of SiC of molten metals10.1016/j.ceramint.2010.01.001 ↗
25. An electron microscopy study of worn ceramic surfaces10.1016/0301-679X(93)90075-C ↗
26. A thermodynamic assessment of the Cu–O–CaO–SiO2
27. Massalski · 1990
28. Contact reaction of SiC with fused Cu
29. Review advances in brazing of ceramics10.1007/BF01117909 ↗
30. Dissolution wetting of Si by molten Cu10.1007/s10853-008-2814-8 ↗
31. Fracture toughness of 2-D carbon fibre reinforced carbon composites10.1007/BF00552386 ↗