Tuning the interfacial reaction between CaO–SrO–Al2O3–B2O3–SiO2 sealing glass–ceramics and Cr-containing interconnect: Crystalline structure vs. glass structure
Source abstract
Abstract
Abstract In this paper, Al 2 O 3 was added to CaO–SrO–B 2 O 3 –SiO 2 sealing system to tailor the structure of sealing glass–ceramics and glass–ceramics/metal interfacial reaction. The addition of alumina in glasses contributes to increasing fraction of bridging oxygen in silica tetrahedral as well as the change in boron environment from three-fold to four-fold (BO 4 → BO 3 ). The devitrification tendency of glasses also decreases with increasing Al 2 O 3 content. The condensed glass structure and increasing residual glass content play opposite roles on the interfacial reaction, consequently resulting in a maximum fraction of Cr 6+ in reaction couples between Cr 2 O 3 and glass containing 6 mole% Al 2 O 3 at 700 °C. In addition, the good bonding can be observed at the interface between Cr-containing interconnect (Crofer 22APU) and glass containing 4 mole% Al 2 O 3 , held at 700 °C for 100 h. The reported results support the suitability of the prepared glass–ceramics as sealing materials for SOFC applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Microwave Dielectric Ceramics Synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. A chemically stable electrolyte with a novel sandwiched structure for proton-conducting solid oxide fuel cells (SOFCs)10.1016/j.elecom.2013.09.011 ↗
2. Performance of a novel type of electrolyte-supported solid oxide fuel cell with honeycomb structure10.1016/j.jpowsour.2009.08.017 ↗
3. Performance and testing of joined Crofer22APU-glass–ceramic sealant-anode supported cell in SOFC relevant conditions10.1016/j.matlet.2010.12.050 ↗
4. Anode-supported planar SOFC with high performance and redox stability10.1016/j.elecom.2010.07.011 ↗
5. Cathode materials for solid oxide fuel cells: a review10.1007/s10008-009-0932-0 ↗
6. Cathode–anode side interaction in SOFC hybrid systems10.1016/j.apenergy.2013.01.029 ↗
7. Stability of the cathode for solid oxide fuel cells10.1149/1.3397854 ↗
8. Effect of volatile boron species on the electrocatalytic activity of cathodes of solid oxide fuel cells10.1149/2.007303jes ↗
9. Impact of volatile boron species on the microstructure and performance of nano-structured (Gd,Ce)O2 infiltrated (La,Sr)MnO3 cathodes of solid oxide fuel cells10.1016/j.elecom.2012.07.025 ↗
10. Boron poisoning of (La, Sr)(Co, Fe)O3 cathodes of solid oxide fuel cells
11. Recent development of SOFC metallic interconnect10.1016/S1005-0302(10)60049-7 ↗
12. Aluminosilicate-based sealants for SOFCs and other electrochemical applications – a brief review10.1016/j.jpowsour.2013.05.099 ↗
13. Chemical compatibility of barium–calcium–aluminosilicate-based sealing glasses with the ferritic stainless steel interconnect in SOFCs10.1149/1.1590325 ↗
14. Compliant alkali silicate sealing glass for solid oxide fuel cell applications: combined stability in isothermal ageing and thermal cycling with YSZ coated ferritic stainless steels10.1016/j.jpowsour.2011.09.027 ↗
15. Sealants for solid oxide fuel cells10.1016/j.jpowsour.2005.05.002 ↗
16. Glass-based seals for solid oxide fuel and electrolyzer cells – a review10.1016/j.mser.2009.12.002 ↗
17. Glass–ceramic seal to join Crofer 22 APU alloy to YSZ ceramic in planar SOFCs10.1016/j.jeurceramsoc.2007.05.006 ↗
18. Thermal cycling of Crofer22APU-sealant-anode supported electrolyte joined structures for planar SOFCs up to 3000h10.1016/j.matlet.2013.08.025 ↗
19. Performance of a glass–ceramic sealant in a SOFC short stack10.1016/j.ijhydene.2012.07.025 ↗
20. Optimization of La2O3-containing diopside based glass–ceramic sealants for fuel cell applications10.1016/j.jpowsour.2009.01.013 ↗
21. Optimization of glass–ceramic sealant compositions in the system MgO–BaO–SiO2 for solid oxide fuel cells (SOFC)10.1016/j.jpowsour.2007.01.040 ↗
22. Effect of pre-oxidation and environmental aging on the seal strength of a novel high-temperature solid oxide fuel cell (SOFC) sealing glass with metallic interconnect10.1016/j.jpowsour.2008.06.020 ↗
23. Chromate formation at the interface between a solid oxide fuel cell sealing glass and interconnect alloy10.1016/j.jpowsour.2012.01.043 ↗
24. Reduction of chromate formation at the interface of solid oxide fuel cells by different additives10.1016/j.jpowsour.2010.04.060 ↗
25. Tailoring the sealing properties of TiO2–CaO–SrO–B2O3–SiO2 glass–ceramic seals: thermal properties, chemical compatibility and electrical property10.1016/j.jpowsour.2013.04.134 ↗
26. Improving the chemical compatibility of sealing glass for solid oxide fuel cells: blocking the reactive species by controlled crystallization
27. Evaluation of chemical durability, thermal properties and structure characteristics of Nb–Sr–phosphate glasses by Raman and NMR spectroscopy10.1016/j.jnoncrysol.2011.08.006 ↗
28. Properties and structure of binary tin phosphate glasses10.1016/j.jnoncrysol.2010.12.061 ↗
29. Network structure and thermal stability study of high temperature seal glass10.1063/1.2979323 ↗
30. Effects of nickel on network structure and thermal properties of a new solid oxide cell seal glass10.1016/j.jpowsour.2008.09.006 ↗
31. 11B NMR studies and structural modeling of Na2O–B2O3–SiO2 glasses of high soda content10.1016/0022-3093(83)90097-2 ↗
32. Development and performance of diopside based glass–ceramic sealants for solid oxide fuel cells10.1016/j.jnoncrysol.2010.01.012 ↗
33. Diopside–Ba disilicate glass–ceramic sealants for SOFCs: enhanced adhesion and thermal stability by Sr for Ca substitution10.1016/j.ijhydene.2012.12.074 ↗
34. Effect of alumina on the structure and properties of Li2O–B2O3–P2O5 glasses10.1016/j.jnoncrysol.2011.04.022 ↗
35. Effect of Al2O3 content on BaO–Al2O3–B2O3–SiO2 glass sealant for solid oxide fuel cell10.1016/j.ceramint.2009.09.045 ↗
36. Stepwise dealumination of zeolite beta at specific T-sites observed with 27Al MAS and 27Al MQ MAS NMR10.1021/ja002689d ↗
37. Study of melilite based glasses and glass–ceramics nucleated by Bi2O3 for functional applications10.1039/c2ra22001f ↗
38. Preparation and characterisation of high refractive index PbO–TiO2–TeO2 glass systems10.1039/JM9960601811 ↗
39. Bonding strength of glass–ceramic trabecular-like coatings to ceramic substrates for prosthetic applications10.1016/j.msec.2012.12.058 ↗
40. Al-MCM-41 inside a glass–ceramic scaffold: a meso–macroporous system for acid catalysis10.1016/j.jeurceramsoc.2013.01.004 ↗
41. Bioactive glass–derived trabecular coating: a smart solution for enhancing osteointegration of prosthetic elements
42. Seal glass compatibility with bare and (Mn,Co)3O4 coated Crofer 22 APU alloy in different atmospheres10.1016/j.jpowsour.2010.07.084 ↗