Abstract Despite of good oxidation resistance and ablation resistance, challenge to densify and tendency to loss high temperature (H.T.) strength have limited its potential applications in aerospace for HfB2–SiC ceramic. In this work, dense HfB2–SiC ceramic with improved H.T. flexural strength was prepared using WC as sintering aid. Pure HfB2–SiC ceramic exhibited creep deformation at 1600 °C with measured strength value of 389 ± 82 MPa, whereas WC doped sample showed much higher flexural strength of 658 ± 69 MPa with linear elastic behavior prior to fracture. In addition to clean grain boundary, the addition of 5 vol.%WC into HfB2–SiC ceramic promoted the formation of fine (Hf,W)B2, (Hf,W)C and WB precipitates. This combinative effect is responsible for its excellent H.T. mechanical property of WC doped HfB2–SiC ceramic.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Fahrenholtz · 2014
2. UHTCs: ultra-high temperature ceramic materials for extreme environment applications
3. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
4. Designing for ultrahigh-temperature applications: the mechanical and thermal properties of HfB2, HfCx, HfNx and αHf(N)10.1023/B:JMSC.0000041690.06117.34 ↗
5. Microstructure and properties of an HfB2–SiC composite for ultra high temperature applications10.1002/adem.200400016 ↗
6. Densification behavior and microstructure evolution of hot-pressed HfB210.1111/j.1551-2916.2010.04063.x ↗
7. Hot pressed HfB2 and HfB2–20vol.%SiC ceramics based on HfB2 powder synthesized by borothermal reduction of HfO210.1111/j.1744-7402.2009.02404.x ↗
8. Hot pressing of hafnium diboride aided by different sinter additives10.1007/s10853-007-2247-9 ↗
9. Fabrication and properties of HfB2–MoSi2 composites produced by hot pressing and spark plasma sintering10.1557/jmr.2006.0180 ↗
10. Microstructure and properties of ZrB2–SiC and HfB2–SiC composites fabricated by spark plasma sintering (SPS) using TaSi2 as sintering aid10.2109/jcersj2.118.997 ↗
11. The effect of B4C on the microstructure and thermo-mechanical properties of HfB2-based ceramics10.1016/j.jallcom.2008.05.093 ↗
12. Pressureless sintering of HfB2–SiC ceramics doped with WC10.1016/j.jeurceramsoc.2012.05.001 ↗
13. Oxidation resistance of hafnium diboride ceramics with additions of silicon carbide and tungsten boride or tungsten carbide10.1111/j.1551-2916.2011.04462.x ↗
14. Improved oxidation resistance of zirconium diboride by tungsten carbide additives10.1111/j.1551-2916.2008.02713.x ↗
15. High strength zirconium diboride-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
16. Microstructure and high-temperature strength of textured and non-textured ZrB2 ceramics10.1088/1468-6996/15/1/014202 ↗
17. Loehman · 2006
18. High-temperature bending strength, internal friction and stiffness of ZrB2–20vol.%SiC ceramics10.1016/j.jeurceramsoc.2012.01.035 ↗
19. Strong ZrB2–SiC–WC ceramics at 1600°C10.1111/j.1551-2916.2011.05062.x ↗
20. Synthesis of monodispersed fine hafnium diboride powders using carbo/borothermal reduction of hafnium dioxide10.1111/j.1551-2916.2008.02466.x ↗
21. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
22. Reaction thermodynamics in the SiO2–SiC system10.1007/BF01295401 ↗
23. Mechanical behavior of zirconium diboride–silicon carbide–boron carbide ceramics up to 2200°C10.1016/j.jeurceramsoc.2014.09.021 ↗
24. Measurement of thermal residual stresses in ZrB2–SiC composites10.1016/j.jeurceramsoc.2011.03.024 ↗
25. The phenomenon of rupture and flow in solids10.1098/rsta.1921.0006 ↗
26. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
27. Refractory diborides as engineering materials
28. Strength of zirconium diboride to 2300°C10.1111/jace.12114 ↗
29. 2013
30. TEM investigation of hot pressed 10vol.%SiC–ZrB2 composite10.1179/174367510X12722693956310 ↗