Particle size effect of starting SiC on processing, microstructures and mechanical properties of liquid phase-sintered SiC

Yoshihiro Hirata, Naoto Suzue, Naoki Matsunaga, Soichiro Sameshima

Publisher page

Abstract

Abstract Dense SiC (97.3–99.2% relative density) of 1.1–3.5 μm average grain size was prepared by the combination of colloidal processing of bimodal SiC particles with sintering additives (Al 2 O 3 plus Y 2 O 3 , 2–4 vol%) and subsequent hot-pressing at 1900–1950 °C. The fracture toughness of SiC was sensitive to the grain boundary thickness which was controlled by grain size and amount of oxide additives. A maximum fracture toughness (6.2 MPa m 1/2 ) was measured at 20 nm of grain boundary thickness. The mixing of 30 nm SiC (25 vol%) with 800 nm SiC (75 vol%) was effective to reduce the flaw size of fracture origin, in addition to a high fracture toughness, leading to the increase of flexural strength. However, the processing of a mixture of 30 nm SiC (25 vol%)–330 nm SiC (75 vol%) provided too small grains (1.1 μm average grain size), resultant thin grain boundaries (12 nm), decreased fracture toughness, and relatively large defect of fracture origin, resulting in the decreased strength.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Pressureless sintering of SiC10.1111/j.1151-2916.1982.tb10460.x ↗
2. Hot-pressing behavior of silicon carbide powders with additions of aluminium oxide10.1007/BF00540356 ↗
3. Low-temperature pressureless sintering of β-silicon carbide with aluminium oxide and yttrium oxide additions
4. Colloidal processing and mechanical properties of SiC with Al2O3 and Y2O310.2109/jcersj.112.22 ↗
5. Colloidal processing and liquid phase sintering of SiC–Al2O3–Y3+ ions system10.1002/9781118406861.ch11 ↗
6. Colloidal processing of SiC with 700MPa of flexural strength10.1002/9781118406861.ch12 ↗
7. Colloidal processing of the SiC–Al2O3–Y3+ ions system and sintering behavior of the consolidated powder compacts
8. Interactions in the silicon carbide–polyacrylic acid–yttrium ion system10.1111/j.1151-2916.2003.tb03269.x ↗
9. Mixing effect of nanometer-sized SiC powder on processing and mechanical properties of SiC using submicrometer-sized powder
10. Hot-pressing and mechanical properties of SiC ceramics with polytitanocarbosilane
11. Processing of high performance silicon carbide10.2109/jcersj2.116.665 ↗
12. Improvement of strength, Weibull modulus and damage tolerance of SiC10.4028/www.scientific.net/MSF.561-565.489 ↗
13. Sintering and mechanical properties of SiC using nanometer-size powder
14. Enhancement of strength of SiC by heat-treatment in air
15. Interaction between alpha-alumina surface and polyacrylic-acid10.2109/jcersj.100.7 ↗
16. Aqueous processing, hot-pressing and mechanical properties of silicon carbide with Al2O3 with Y2O310.2109/jcersj.113.143 ↗
17. Colloidal processing and mechanical properties of silicon carbide with alumina10.1557/JMR.1997.0411 ↗
18. Hirata · Adv Sci Technol · 1999 · 14 · 637
19. Levin · 1969 · 165
20. Liquid phase sintering and mechanical properties of SiC with rare-earth oxide10.2109/jcersj.114.247 ↗
21. Swalin · 1972
22. Doremus · 1985
23. Sinterability of SiC powder coated uniformly with Al ions10.1557/JMR.1998.0104 ↗
24. Mechanical properties of SiC processed with nanometer-sized powder and polytitanocarbosilane10.4028/www.scientific.net/KEM.352.73 ↗