Mullite-bonded SiC-whisker-reinforced SiC matrix composites: Preparation, characterization, and toughening mechanisms
Source abstract
Abstract
Abstract A novel mullite-bonded SiC-whisker-reinforced SiC matrix composite (SiCw/SiC, SiC whisker-to-SiC powder mass ratio of 1:9) was designed and successfully prepared. Before preparing the composite, the inexpensive lab-made SiCw was first modified by an oxidation/leaching process and then coated with Al2O3. The kinetics results indicate that the oxidation process can be described by improved shrinking-cylinder models. The aspect ratio of SiCw improved after modification. Subsequently, raw materials with a SiC–SiO2–Al2O3 triple-layered structure were obtained after the Al2O3-coating process and used as feedstocks during the subsequent hot-pressing sintering. Finally, the characterization of the composites indicates that the mullite-bonded sample performs better (relative density of 93.8 ± 1.4%, flexural strength of 533.3 ± 18.2 MPa, fracture toughness of 13.6 ± 2.1 MPa m1/2, and Vickers hardness of 20.6 ± 2.5 GPa) than the reference sample without the mullite interface. The improved toughness could essentially be attributed to the moderately strong interface bonding and effective load transfer effects of the mullite interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Formation of carbon-rich layer on the surface of SiC fiber by sintering under vacuum for superior mechanical and thermal properties10.1016/j.jeurceramsoc.2016.10.013 ↗
2. Scalable fabrication of novel SiC nanowire nonwoven fabric10.1007/s10853-017-1815-x ↗
3. Oxidation resistance of SiC/SiC composites containing SiBC matrix fabricated by liquid silicon infiltration10.1016/j.jeurceramsoc.2017.09.004 ↗
4. Tension-tension fatigue behavior of a PIP SiC/SiC composite at elevated temperature in air10.1016/j.ceramint.2015.10.116 ↗
5. Microstructure evolution and high-temperature mechanical properties of SiCf/SiC composites in liquid fluoride salt environment10.1016/j.corsci.2017.05.016 ↗
6. Microhardness and microstructure correlations in SiC/SiC composites10.1016/j.matlet.2017.11.093 ↗
7. Effects of the single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process10.1016/j.ceramint.2010.05.014 ↗
8. RVE model with porosity for 2D woven CVI SiCf/SiC composites10.1007/s11665-016-2393-9 ↗
9. Microstructure characteristic and its influence on the strength of SiC ceramic joints diffusion bonded by spark plasma sintering10.1016/j.ceramint.2017.11.185 ↗
10. Modeling of stress concentration in ceramic matrix composites10.1016/j.compositesb.2012.07.034 ↗
11. SiC/SiC composites through transient eutectic-phase route for fusion applications10.1016/j.jnucmat.2004.04.157 ↗
12. Efforts on large scale production of NITE-SiC/SiC composites10.1016/j.jnucmat.2007.03.053 ↗
13. High thermal conductivity SiC/SiC composites for fusion applications10.1016/S0022-3115(00)00213-0 ↗
14. Very high pressure hot pressing of silicon carbide
15. Sintering of silicon carbide
16. Haris · 1995
17. Sintering additives for SiC based on the reactivity: a review10.1016/j.ceramint.2016.09.022 ↗
18. Aqueous colloidal processing of SiC with Y3Al5O12 liquid-phase sintering additives10.1016/j.jeurceramsoc.2013.01.030 ↗
19. Incorporating Zr to achieve self-protecting and enhancement of silica sol bonded SiC castables at active oxidation condition10.1016/j.ceramint.2017.12.240 ↗
20. Mechanical properties of SiC/SiC composites by PIP process with a new precursor at elevated temperature10.1016/j.msea.2014.03.011 ↗
21. Glass coating for SiCf/SiC composites for high-temperature application10.1016/S1359-6454(00)00263-9 ↗
22. The effect on the tensile properties of PIP-processed SiC/SiC composite of a chemical vapor-infiltrated SiC layer overlaid on the pyrocarbon interface layer10.1016/j.compositesa.2016.04.021 ↗
23. Mechanical and electromagnetic shielding properties of SiCf/SiC composites fabricated by combined CVI and PIP process10.1016/j.ceramint.2014.02.103 ↗
24. Comparison of cyclic fatigue behavior between C/SiC and SiC/SiC ceramic-matrix composites at elevated temperatures using hysteresis dissipated energy10.1016/j.compstruct.2016.05.006 ↗
25. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre-matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
26. Mechanical properties and in situ crack growth observation of SiC/SiC composites10.1016/j.ceramint.2013.12.098 ↗
27. Novel two-step process for synthesising β-SiC whiskers from coal fly ash and water glass10.1016/j.ceramint.2018.03.082 ↗
28. Microwave digestion and alkali fusion procedures for the determination of the platinum-group elements and gold in geological materials by ICP-MS10.1016/0009-2541(95)00021-D ↗
29. Effect of oxidation treatment on KD-II SiC fiber-reinforced SiC composites10.1016/j.ceramint.2017.05.001 ↗
30. Influence of the α/β-SiC phase transformation on microstructural development and mechanical properties of liquid phase sintered silicon carbide10.1023/A:1004552704872 ↗
31. Sintering behaviour of silicon carbide matrix composites reinforced with multilayer grapheme10.1016/j.ceramint.2017.01.010 ↗
32. Zhu · 2006
33. Levenspiel · 1998
34. A cleaner vanadium extraction method featuring non-salt roasting and ammonium bicarbonate leaching10.1016/j.jclepro.2017.02.093 ↗
35. Controllable synthesis and characterization of alumina/MWNT nanocomposites10.1002/pssb.201100095 ↗
36. Aluminium tri-iso-propoxide: shelf life, transport properties, and decomposition kinetics for the low temperature processing of aluminium oxide-based coatings10.1016/j.surfcoat.2007.04.063 ↗
37. Comparative study of Al2O3-coated LiCoO2 electrode derived from different Al precursors: uniformity, microstructure and electrochemical properties10.1016/j.electacta.2015.08.039 ↗
38. Improved mechanical properties of Al2O3-25 vol% SiCw composites prepared by oscillatory pressure sintering10.1016/j.ceramint.2017.08.087 ↗