journal article·2019-08Open access

Ti3SiC2-Cf composites by spark plasma sintering: Processing, microstructure and thermo-mechanical properties

M.A. Lagos, C. Pellegrini, I. Agote, N. Azurmendi, J. Barcena, M. Parco, L. Silvestroni, L. Zoli, D. Sciti

Abstract

MAX phases, and particularly Ti 3 SiC 2 , are interesting for high temperature applications. The addition of carbon fibers can be used to reduce the density and to modify the properties of the matrix. This work presents the densification and characterization of Ti 3 SiC 2 based composites with short carbon fibers using a fast and simple fabrication approach: dry mixing and densification by Spark Plasma Sintering. Good densification level was obtained below 1400 °C even with a high amount of fibers. The reaction of the fibers with the matrix is limited thanks to the fast processing time and depends on the amount of fibers in the composite. Bending strength at room temperature, between 437 and 120 MPa, is in the range of conventional CMCs with short fibers and according to the resistance of the matrix and the presence of residual porosity. Thermo-mechanical properties of the composites up to 1500 °C are also presented.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Tensile properties of Ti3SiC2 in the 25-1300C temperature range10.1016/S1359-6454(99)00351-1 ↗
2. Mechanical properties of Ti3SiC2 at high temperature
3. Effect of temperature, strain rate and grain size on the compressive properties of Ti3SiC210.1016/j.actamat.2005.05.020 ↗
4. Compressive creep of fine and coarse-grained Ti3SiC2 in air in the 1100–1300 °C temperature range10.1016/j.actamat.2005.05.037 ↗
5. Current status in layered ternary carbide Ti3SiC2, a review10.1016/j.jmst.2018.09.005 ↗
6. Preparation of SiC reinforced Ti3SiC2-base composite and its biocompatibility evaluation10.1016/j.ceramint.2013.10.113 ↗
7. Ti3SiC2 as a bonding phase in diamond composites10.1023/A:1012535100330 ↗
8. Max phase carbides and nitrides, properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
9. Synthesis and characterization of 0.3%fTiC–Ti3SiC2 and 0.3 vol% SiC–Ti3SiC2 composite10.1016/S0925-8388(02)00985-4 ↗
10. Rapid fabrication of Ti3SiC2 nanocomposite using the spark plasma sintering-reactive (SPS-RS) method10.1016/j.scriptamat.2006.09.029 ↗
11. Microstructure and properties of Ti3SiC2/SiC nanocomposites fabricated by spark plasma sintering10.1016/j.compscitech.2007.06.006 ↗
12. Relationships between Carbon fiber type and interfacial domain in ZrB2-based ceramics10.1016/j.jeurceramsoc.2015.09.026 ↗
13. Novel Cr2AlC MAX-phase/SiC fiber composites: synthesis, processing and tribological response10.1016/j.jeurceramsoc.2016.09.029 ↗
14. On the thermal shock resistance and mechanical properties of novel unidirectional UHTCMCs for extreme environments10.1038/s41598-018-27328-x ↗
15. Understanding the mechanical properties of novel UHTCMCs through random forest and regression tree analysis10.1016/j.matdes.2018.02.061 ↗
16. Tough salami-inspired Cf/ZrB2 UHTCMCs produced by electrophoretic deposition10.1016/j.jeurceramsoc.2017.09.047 ↗
17. Fabrication of fiber composites with a MAX phase matrix by reactive melt infiltration10.1088/1757-899X/18/20/202030 ↗
18. Influence of pyrocarbon amount in C/C preform on the microstructure and properties of C/ZrC composites prepared via reactive melt infiltration10.1016/j.matdes.2013.12.071 ↗
19. Processing, microstructure and ablation behaviour of C/SiC–Ti3SiC2 composites fabricated by liquid silicon infiltration10.1016/j.corsci.2013.04.029 ↗
20. Fabrication and properties of 3-D Cf/ZrB2-ZrC-SiC composites via polymer infiltration and pyrolysis10.1016/j.ceramint.2012.11.074 ↗
21. UHTC–carbon fibre composites: preparation, oxyacetylene torch testing and characterization10.1016/j.jeurceramsoc.2012.08.018 ↗
22. Phase evolution of Ti3SiC2 annealing in vacuum at elevated temperatures10.1111/j.1744-7402.2012.02760.x ↗
23. Rapid Spark Plasma Sintering to produce dense UHTCs reinforced with undamaged carbon fibres10.1016/j.matdes.2017.05.029 ↗
24. Influence of SPS parameters on the density and mechanical properties of sintered Ti3SiC2 powders10.1016/j.ijrmhm.2013.01.016 ↗
25. Low-temperature fabrication of high purity Ti3SiC210.1016/j.jallcom.2007.05.074 ↗
26. Synthesis of the MAX phases by pulse discharge sintering10.1111/j.1744-7402.2010.02555.x ↗
27. Effect of milling on the mechanical properties of chopped SiC fiber-reinforced ZrB210.3390/ma6051980 ↗
28. Relationships between Carbon fiber type and interfacial domain in ZrB2-based ceramics10.1016/j.jeurceramsoc.2015.09.026 ↗
29. Heidenreich · 2008 · 113
30. Thermal properties of Ti3SiC210.1016/S0022-3697(98)00313-8 ↗
31. Synthesis and some properties of Ti3SiC2 by hot pressing of Ti, Si and C powders part 2 – mechanical and other properties of Ti3SiC210.1179/174328405X58841 ↗