Abstract A new design of seamless joining was proposed to join SiC using electric field-assisted sintering technology. A 500 nm Y coating on SiC was used as the initial joining filler to obtain a desired transition phase of Y3Si2C2 layer via the appropriate interface reactions with the SiC matrix. The phase transformation and decomposition of the transition phase of Y3Si2C2 was designed to achieve almost seamless joining of SiC. The decomposition of the joining layer to SiC, followed up by the inter-diffusion and complete densification with the initial SiC matrix, resulted in the formation of an almost seamless joint at the temperature of 1900 °C. The bending strength of the seamless joint was 134.8 ± 2.1 MPa, which was comparable to the strength of the SiC matrix. The proposed design of seamless joining could potentially be applied for joining of SiC-based ceramic matrix composites with RE3Si2C2 as the joining layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
2. Silicon carbide composites as fusion power reactor structural materials10.1016/j.jnucmat.2011.03.005 ↗
3. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
4. Recent progress in the development of SiC composites for nuclear fusion applications10.1016/j.jnucmat.2018.06.017 ↗
5. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
6. Radiation-tolerant joining technologies for silicon carbide ceramics10.1016/j.jnucmat.2013.10.002 ↗
7. Microstructure evolution of SiC/SiC joints during ultrasonic-assisted air bonding using a Sn-Zn-Al alloy10.1016/j.ceramint.2017.07.169 ↗
8. Wetting of SiC by Al-Ti alloys and joining by in-situ formation of interfacial Ti3Si(Al)C210.1016/j.jeurceramsoc.2018.04.025 ↗
9. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
10. R&D of joining technology for SiC components with channel10.1016/j.jnucmat.2008.12.263 ↗
11. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass10.1016/j.ceramint.2018.02.092 ↗
12. CaO-Al2O3 glass-ceramic as a joining material for SiC based components: a microstructural study of the effect of Si-ion irradiation10.1016/j.jnucmat.2018.01.033 ↗
13. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
14. High temperature properties of the monolithic CVD β-SiC materials joined with a pre-sintered MAX phase Ti3SiC2 interlayer via solid-state diffusion bonding10.1016/j.jeurceramsoc.2016.11.006 ↗
15. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using spark plasma sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
16. Flashing joining of CVD-SiC coated Cf/SiC composites with a Ti interlayer10.1016/j.jeurceramsoc.2016.11.006 ↗
17. Joining of SiC monoliths using a thin MAX phase tape and the elimination of joining layer by solid-state diffusion10.1016/j.jeurceramsoc.2018.04.006 ↗
18. Joining of SiCf/SiC using a Ti3AlC2 filler and subsequent elimination of the joining layer10.1016/j.ceramint.2018.09.090 ↗
19. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
20. Joining of carbon fiber reinforced carbon composites with Ti3SiC2 tape film by Electric Field Assisted Sintering Technique10.1016/j.carbon.2016.02.036 ↗
21. Residual thermal stress of SiC/Ti3SiC2/SiC joints calculation and relaxed by post-annealing10.1111/ijac.12900 ↗
22. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
23. Barsoum · 2013
24. MAX phase carbides and nitrides: properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
25. Thermal properties of Ti3SiC210.1016/S0022-3697(98)00313-8 ↗
26. Reaction synthesis of TiB2-TiC composites with enhanced toughness10.1016/S1359-6454(01)00034-9 ↗
27. SiC ceramics joined with an in-situ reaction gradient layer of TiC/Ti3SiC2 and interface stress distribution simulations10.1016/j.ceramint.2018.05.255 ↗
28. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
29. Modeling thermal and irradiation-induced swelling effects on the integrity of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.09.011 ↗
30. A dual-phase microstructural approach to damage and fracture of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.11.054 ↗
31. Fabrication and characterization of SPS sintered SiC-based ceramic from Y3Si2C2-coated SiC powders10.1016/j.jeurceramsoc.2018.07.054 ↗
32. Y5Si3C and Y3Si2C2: theoretically predicted MAX phase like damage tolerant ceramics and promising interphase materials for SiCf/SiC composites10.1016/j.jmst.2018.09.041 ↗
33. Thermodynamic description of the sintering aid system in silicon carbide ceramics with the addition of yttrium10.1016/j.jeurceramsoc.2019.07.012 ↗
34. Superhard V-Si-N coatings (&50GPa) with the cell-like nanostructure prepared by magnetron sputtering10.1016/j.surfcoat.2013.06.035 ↗
35. Dislocations, kink bands, and room-temperature plasticity of Ti3SiC210.1007/s11661-999-0172-z ↗
36. MAX phases: bridging the gap between metals and ceramics
37. Z-Contrast tomography: a technique in three-dimensional nanostructural analysis based on Rutherford scattering10.1039/b101819c ↗
38. Magnetic and electrical properties of a new series of rare earth silicide carbides with the composition of R3Si2C2 (R=Y, La-Nd, Sm, Gd-Tm)10.1006/jssc.1998.7772 ↗