Oxidation/corrosion of BN-based coatings as prospective interphases for SiC/SiC composites
Source abstract
Abstract
Abstract The ceramic matrix composites envisaged as structural parts in the hot section of aircraft engines consist of SiC-based fibres and matrices with a BN interphase coating between them. To control their service life, the oxidation/corrosion behaviour of these materials must be determined. For this purpose, samples of different geometries were prepared by chemical vapour deposition and thermally subjected to wet air. The behaviour of BN alone depends on its crystallization degree, structural homogeneity and the considered direction in the coating. In the case of a thin layer of pure BN of interphase type, recession is significantly reduced at 800 °C by the formation of a sealing borosilicate phase in the confined space surrounded by SiC. At 1000 °C, the protection is no longer sufficient and a steady recession remains. The presence of aluminium added to BN improves protection at 1000 °C due to the formation of alumina combined with borosilicate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Ceramic matrix composites taking flight at GE Aviation
2. Design, preparation and properties of nonoxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. 5.3 Advanced SiC/SiC Composite Systems
4. Oxidation resistance of SiC/SiC micro and minicomposites with a highly crystallised BN interphase10.1016/S0955-2219(98)00120-4 ↗
5. Investigation of the BN films prepared by low pressure chemical vapor deposition10.1016/S0257-8972(99)00306-0 ↗
6. SiC/SiC minicomposites with structure-graded BN interphases10.1016/S0955-2219(00)00064-9 ↗
7. Low pressure chemical vapour deposition of BN: Relationship between gas phase chemistry and coating microstructure10.1016/j.tsf.2018.08.020 ↗
8. Effect of temperature on the growth of boron nitride interfacial coatings on SiC fibers by chemical vapor infiltration10.1016/j.ceramint.2019.06.077 ↗
9. High temperature mechanical behaviour of ceramic composites
10. Single and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview10.1111/j.1744-7402.2009.02424.x ↗
11. Oxidation of boron nitride under nonisothermal conditions, Powder Metall
12. Paralinear oxidation of CVD SiC in water vapor; J. Am10.1111/j.1151-2916.1997.tb02810.x ↗
13. High-temperature oxidation of boron nitride: I, monolithic boron nitride
14. A pervasive mode of oxidative degradation in a SiC–SiC composite10.1111/j.1151-2916.1998.tb02696.x ↗
15. High temperature crack sealant based on SiO2-B2O3 for SiC coating on carbon-carbon composites10.1163/156855103772658498 ↗
16. Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments
17. Quantification of higher SiC fiber oxidation rates in presence of B2O3 under air
18. Silicon carbide fiber oxidation behavior in the presence of boron nitride10.1111/jace.15807 ↗
19. Tensile stress rupture of SiCf/SiCm minicomposites with carbon and boron nitride interphases at elevated temperatures in air10.1111/j.1151-2916.1997.tb03087.x ↗
20. Environmental durability of BN‐based interphases (for SiCf/SiCm composites) in H2O containing atmospheres at intermediate temperatures10.1002/9780470294437.ch58 ↗
21. Microstructure and damage evolution of SiCf/PyC/SiC and SiCf/BN/SiC mini-composites: A synchrotron X-ray computed microtomography study10.1016/j.ceramint.2019.03.004 ↗
22. Degradation mechanisms of SiC/BN/SiC after low temperature humidity exposure10.1016/j.jeurceramsoc.2020.05.007 ↗
23. Degradation of a SiC‐SiC composite in water vapor environments10.1111/jace.16838 ↗
24. High temperature Si‐doped BN interphases for woven SiC/SiC composites10.1002/9780470294741.ch34 ↗
25. K. Grente, S. Bertrand, F. Rebillat, F. Langlais, F. Lamouroux, Réalisation de matériaux composites à matrice céramique ayant une tenue améliorée à haute température sous atmosphère corrosive, Patent, France n° 04 11262, 22/10/2004, FR2877016 (A1); FR2877016 (B1), internationale classification C23C16/06, C04B35/01, C23C16/22.
26. Influence of alumina reaction tube impurities on the oxidation of Chemically-VaporDeposited silicon carbide10.1111/j.1151-2916.1995.tb08449.x ↗
27. Identification of complex oxidation/corrosion behaviours of boron nitride under high temperature10.1007/s11085-017-9739-z ↗
28. An X-ray study of boron nitride10.1107/S0365110X52001064 ↗
29. High temperature oxidation of ceramic matrix composites10.1351/pac199870020493 ↗
30. Oxidative and hydrolytic stability of boron nitride – A new approach to improving the oxidation resistance of carbonaceous structures10.1016/0008-6223(94)00163-T ↗
31. Stability to moisture for chemically vapour-deposited boron nitride10.1007/BF01174496 ↗
32. Stability of BN coatings processed from BCl3-NH3-H3 gas mixture
33. Phase relations in the system boron oxide-silica, J. Am10.1111/j.1151-2916.1965.tb11803.x ↗
34. Herbreteau · 2016
35. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys10.1149/1.2424115 ↗
36. McKee · 2000 · 12
37. Oxygen transport through silica surface layers on silicon-containing ceramic materials
38. Oxygen transport through glass layers formed by a gel process10.1016/0022-3093(84)90396-X ↗