Abstract
Abstract An in-situ SiC-HfB2-Si ternary coating was deposited on C/C composites (C/Cs) via slurry panting plus gaseous Si infiltration composite method, to improve the oxidation and ablation resistance of C/Cs above 1773 K. The coating formation mechanism was investigated by microstructural analyses and thermo-dynamic calculations. The oxidation behavior of the coated specimens subjected either to high-temperature testing at 1773 K and 1973 K in static air furnace or to ablation testing with oxyacetylene torch upon ultra-high temperature service were studied, base on thermo-dynamic computations, numerical simulations and microstructure evolution. The SiC-HfB2-Si coating protected C/Cs against oxidation at 1773 K for more than 1507 h which is longer than that of the reported SiC-HfB2-based coatings, due to the as-prepared compact mosaic coating filled with HfB2-rich Si-based multiphase and the consequently formed dense Hf-Si-O oxide layer. Moreover, a good ablation resistance with relatively low linear and mass ablation rates of −0.72 μm/s and 0.07 mg/s, respectively, was achieved due to the stable oxide scale with high viscosity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites10.1016/j.jeurceramsoc.2017.08.013 ↗
2. Gel reactive melt infiltration: a new method for large-sized complex-shaped C/C components ceramic modification10.1016/j.ceramint.2019.04.115 ↗
3. High temperature coatings for oxidation and ablation protection of Heat-Resistant carbonaceous materials in High-Speed flows10.4028/www.scientific.net/KEM.771.103 ↗
4. A WSi2-HfB2-SiC coating for ultralong-time anti-oxidation at 1973 K10.1016/j.corsci.2019.108119 ↗
5. Fabrication and characteristics of a HfC/TiC multilayer coating by a vacuum plasma spray process to protect C/C composites against oxidation10.1016/j.corsci.2020.109068 ↗
6. In-situ formation of SiC, ZrB2-SiC and ZrB2-SiC-B4C-YAG coatings for high temperature oxidation protection of C/C composites10.1016/j.corsci.2018.07.002 ↗
7. SiC/Si–ZrSi2–ZrB2-HfB2/SiC coating for oxidation protection of C/C composites prepared by three-step method10.1016/j.jallcom.2020.155532 ↗
8. Microstructure and resistance to thermal shock of SiC coatings that are prepared on C/C-composite pyrocarbon matrices of various textures
9. Comparing oxidation behaviors at 1773 K and 1973 K of HfB2-MoSi2/SiC-Si coating prepared by a combination method of pack cementation, slurry painting and in-situ synthesis10.1016/j.surfcoat.2020.126418 ↗
10. The oxidation resistance of two-temperature synthetic HfB2-SiC coating for the SiC coated C/C composites10.1016/j.jallcom.2018.03.043 ↗
11. Microstructure and ablative properties of Si-SiC coating prepared by spark plasma sintering10.1016/j.ceramint.2018.02.033 ↗
12. SiC-Si coating with micro-pores to protect carbon_carbon composites against oxidation10.1016/j.jeurceramsoc.2020.08.045 ↗
13. Multiphase composite Hf0.8Ti0·2B2–SiC–Si coating providing oxidation and ablation protection for graphite under different high temperature oxygen-containing environments10.1016/j.ceramint.2020.09.019 ↗
14. Difference evaluation on ablation behaviors of ZrC-based and ZrB2-based UHTCs coatings
15. Molten salt synthesis, formation mechanism, and oxidation behavior of nanocrystalline HfB2 powders10.1007/s40145-019-0345-1 ↗
16. Synthesis and flash sintering of (Hf1-xZrx)B2 solid solution powders10.1016/j.jeurceramsoc.2020.12.015 ↗
17. An oxidation and ablation protective WSi2-HfB2-SiC coating for SiC coated C/C composites at 1973 K and above10.1016/j.corsci.2020.108964 ↗
18. Dynamic oxidation protective behaviors and mechanisms of HfB2-20wt%SiC composite coating for carbon materials10.1016/j.jeurceramsoc.2019.01.033 ↗
19. Oxidation and ablation protection of double layer HfB2-SiC-Si/SiC-Si coating for graphite materials10.1016/j.jallcom.2018.12.256 ↗
20. Ultrahigh temperature ceramic HfB2-SiC coating by liquid phase sintering method to protect carbon materials from oxidation10.1016/j.matchemphys.2018.07.018 ↗
21. Ablation properties of HfB2 coatings prepared by supersonic atmospheric plasma spraying for SiC-coated carbon/carbon composites10.1016/j.surfcoat.2018.09.060 ↗
22. Oxidation inhibition behaviors of the HfB2-SiC-TaSi2 coating for carbon structural materials at 1700 °C10.1016/j.corsci.2020.108982 ↗
23. A CrSi2-HfB2-SiC coating providing oxidation and ablation protection over 1973 K
24. TaxHf1−xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
25. HfB2-SiC-MoSi2 oxidation resistance coating fabricated through in-situ synthesis for SiC coated C/C composites10.1016/j.jallcom.2017.06.008 ↗
26. Ultra-high-temperature ceramic HfB2-SiC coating for oxidation protection of SiC-coated carbon/carbon composites10.1111/ijac.12241 ↗
27. Gradient HfB2-SiC multilayer oxidation resistant coating for C/C composites10.1016/j.ceramint.2018.08.104 ↗
28. Bamboo like SiC nanowires grown in a Dual-Temperature zone reaction system enhance the oxidation and thermal shock resistance of SiC coatings
29. Design and fabrication of HfC, SiC/HfC and HfC-SiC/HfC interlayers for improving the adhesion between diamond coatings and cemented carbides10.1016/j.jallcom.2019.152405 ↗
30. Oxidation behavior of SiC-HfB2-Si coating on C/C composites prepared by slurry dipping combined with gaseous Si infiltration10.1016/j.surfcoat.2020.125335 ↗
31. Structural design and ablation performance of ZrB2/MoSi2 laminated coating for SiC coated carbon/carbon composites10.1016/j.jeurceramsoc.2019.09.046 ↗
32. Data collection of properties of hard Materials
33. Constructing self-healing ZrSi2-MoSi2 coating for C/C composites with enhanced oxidation protective ability10.1016/j.surfcoat.2018.05.002 ↗
34. Review on ultra-high temperature boride ceramics10.1016/j.pmatsci.2020.100651 ↗
35. 2019
36. Riedel · 2000 · 202
37. Mechanical properties of ZrB2- and HfB2-based ultra-high temperature ceramics fabricated by spark plasma sintering10.1016/j.jeurceramsoc.2012.12.009 ↗
38. Properties and uses of diborides
39. Pierre Villars (Chief Editor), PAULING FILE in: Inorganic Solid Phases, SpringerMaterials (online database), Springer, Heidelberg (ed.) SpringerMaterials.
40. Murr · 2021 · 1
41. Scale characterisation of an oxidised (Hf,Ti)C-SiC ultra-high temperature ceramic matrix composite10.1016/j.jeurceramsoc.2020.08.048 ↗
42. Ablation behavior of HfC coating with different thickness for carbon/carbon composites at ultra-high temperature
43. Formation mechanism and supersonic flame ablation behavior of SiC and SiC-SiCnano single-layer oxidation protective coatings for carbon materials by reactive melt infiltration (RMI) method10.1016/j.corsci.2019.108136 ↗
44. Microstructure and ablation behaviour of a strong, dense, and thick interfacial ZrxHf1-xC/SiC multiphase bilayer coating prepared by a new simple one-step method10.1016/j.ceramint.2020.01.244 ↗
45. National Standard Committee of China · 1996
46. A novel Hf-Si-O wire drawing phenomenon after ablation of SiCnws/HfC SiC coating on C/C composites
47. Ablation resistance of HfC(Si, O)-HfB2(Si, O) composites fabricated by one-step reactive spark plasma sintering10.1016/j.jeurceramsoc.2020.11.054 ↗
48. Densification behavior and ablation property of C/C-ZrC composites prepared by chemical liquid vapor deposition process at temperatures from 800 to 1100 °C10.1016/j.ceramint.2018.01.239 ↗
49. Thermodynamic assessment of the group IV, V and VI oxides for the design of oxidation resistant multi-principal component materials10.1016/j.jeurceramsoc.2018.11.004 ↗
50. Corrosion behavior of a Mo(Si, Al)2 composite at 1700°C in 95% N2 + 5% H210.1016/j.jeurceramsoc.2019.08.017 ↗
51. Arc-jet wind tunnel characterization of ultra-high-temperature ceramic matrix composites10.1016/j.corsci.2018.12.039 ↗
52. Investigation on the ablation performance and mechanism of HfC coating modified with TaC10.1016/j.corsci.2020.108649 ↗
53. Crack development behavior in thermally sprayed anti-oxidation coating under repeated thermal-oxygen coupling environment
54. Multi-layered structural designs of MoSi2/mullite anti-oxidation coating for SiC-coated C/C composites10.1016/j.surfcoat.2021.126901 ↗
55. Zirconium carbide skeleton reinforced pyrocarbon composites with tunable mechanical strength, thermophysical properties and ablation resistance10.1016/j.corsci.2021.109274 ↗
56. ZrB2 particles reinforced glass coating for oxidation protection of carbon/carbon composites10.1007/s40145-018-0298-9 ↗
57. Fabrication and microstructure of ZrB2–ZrC–SiC coatings on C/C composites by reactive melt infiltration using ZrSi2 alloy10.1007/s40145-017-0257-x ↗
58. Effect of Si addition on hot-pressed ZrB2–SiC composite with polycarbosilane as a precursor10.1016/j.matlet.2008.04.034 ↗
59. Oxidation protection and mechanism of the HfB2-SiC-Si/SiC coatings modified by in-situ strengthening of SiC whiskers for C/C composites10.1016/j.ceramint.2018.04.025 ↗
60. The effect of HfB2 content on the oxidation and thermal shock resistance of SiC coating10.1016/j.surfcoat.2018.02.029 ↗
61. The resistance to oxidation of an HfB2–SiC composite10.1016/j.jeurceramsoc.2004.05.009 ↗
62. High-temperature oxidation at 1500℃ and 1600℃ of SiC/graphite coated with sol-gel-derived HfO210.1111/j.1551-2916.2005.00202.x ↗
63. Thermodynamic modeling of the Hf–Si–O system10.1016/j.calphad.2006.08.006 ↗
64. Theoretical and experimental investigation of thermal stability of HfO2/Si and HfO2/SiO2 interfaces
65. Siliconization elimination for SiC coated C/C composites by a pyrolytic carbon coating and the consequent improvement of the mechanical property and oxidation resistances10.1016/j.jeurceramsoc.2021.04.008 ↗
66. Ablation properties of HfB2 coatings prepared by supersonic atmospheric plasma spraying for SiC-coated carbon/carbon composites10.1016/j.surfcoat.2018.09.060 ↗
67. Ablation resistance of HfB2-SiC coating prepared by in-situ reaction method for SiC coated C/C composites10.1016/j.ceramint.2017.06.052 ↗
68. Fabrication and optimization of 3D-Cf/HfC-SiC-based composites via sol-gel processing and reactive melt infiltration10.1016/j.jeurceramsoc.2020.10.053 ↗
69. Improved aero-thermal resistance capabilities of ZrB2-based ceramics in hypersonic environment for increasing SiC content10.1016/j.corsci.2020.109067 ↗
70. New insight into the ablation behavior of C/C-ZrC composites in a nitrogen plasma torch with a high heat flux of ∼25 MW/m210.1016/j.corsci.2021.109409 ↗
71. Ablation behavior of nose-shaped HfB2-SiC modified carbon/carbon composites exposed to oxyacetylene torch10.1016/j.corsci.2019.02.015 ↗
72. Nanotube/nanowire-toughened carbon/carbon composites and their coatings
73. Improvement of ablation resistance of CVD-HfC/SiC coating on hemisphere shaped C/C composites by introducing diffusion interface10.1016/j.jeurceramsoc.2021.02.004 ↗
74. Oxidation and ablation behaviour of multiphase ultra-high-temperature ceramic Ta0·5Zr0·5B2–Si–SiC protective coating for graphite10.1016/j.ceramint.2020.12.262 ↗
75. Laser ablation behavior of SiHfC-based ceramics prepared from a single-source precursor: effects of Hf-incorporation into SiC10.1016/j.jeurceramsoc.2019.01.040 ↗