Qualitative analysis of hafnium diboride based ultra high temperature ceramics under oxyacetylene torch testing at temperatures above 2100°C
Source abstract
Abstract
Abstract Oxidation tests were carried out on HfB2–SiC, HfB2–HfC, HfB2–WC–SiC, and HfB2–WSi2 ceramics using an oxyacetylene torch. The samples were oxidized between 2100 and 2300 °C. From cross-sectional images, scale non-adherence was noted as a limiting factor in oxidation resistance. The sample with the best scale adherence was HfB2–WSi2. Factors involving scale non-adherence such as vapor pressure, coefficient of thermal expansion mismatch and phase transformations were considered. In comparing the scale adherence of the samples it was hypothesized that vapor pressure buildup is the principal contributing factor in the scale adherence differences observed among the tested samples. However, the coefficient of thermal expansion mismatch and HfO2 phase transformation cannot be neglected as contributing factors to scale non-adherence in all samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Designing for ultrahigh-temperature applications:The mechanical and thermal properties of HfB2, HfCx, HfNx and αHf10.1023/B:JMSC.0000041690.06117.34 ↗
2. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
3. Rapid oxidation characterization of ultra-high temperature ceramics10.1111/j.1551-2916.2007.01861.x ↗
4. Convection patterns in liquid oxide films on ZrB2–SiC composites oxidized at a high temperature10.1111/j.1551-2916.2007.01784.x ↗
5. The repeated thermal shock behaviors of a ZrB2–SiC composite heated by electrical resistance method10.1016/j.ijrmhm.2010.06.012 ↗
6. Non-contact mechanical property measurements at ultrahigh temperatures10.1016/j.jeurceramsoc.2010.01.006 ↗
7. Ultra high temeprature ceramics: densification, properties and thermal stability
8. Laser modified microstructures in ZrB2, ZrB2/SiC and ZrC10.1016/j.jeurceramsoc.2010.03.001 ↗
9. The addition of lanthanum hexaboride to zirconium diboride for improved oxidation resistance10.1016/j.scriptamat.2007.07.036 ↗
10. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
11. Ablation behavior and mechanism of 3D C/ZrC composite in oxyacetylene torch environment10.1016/j.compscitech.2011.05.005 ↗
12. ZrB2–SiC composite parts in oxyacetylenic torch tests: experimental and computational assessment of chemical, thermal and mechanical behavior10.1016/j.msea.2011.06.008 ↗
13. UHTC composites for hypersonic applications
14. Ablation behavior of ZrB2–SiC ultra high temperature ceramics under simulated atmospheric re-entry condition10.1016/j.compscitech.2008.02.009 ↗
15. Plasma torch test of an ultra-high temeprature ceramics nose cone demonstrator10.2514/1.42834 ↗
16. A model for the oxidation of ZrB2, HfB2, and TiB210.1016/j.actamat.2007.07.027 ↗
17. Modeling surface oxidation intransient aerothermal heating environments
18. Oxidation resistance of hafnium diboride—silicon carbide from 1400 to 2000°C10.1007/s10853-009-3799-7 ↗
19. Effect of various additives on the oxidation behavior of ZrB2-based ultra-high temperature ceramics10.1111/j.1551-2916.2009.03420.x ↗
20. Separating test artifacts from material behavior in the oxidation studies of HfB2–SiC at 2000°C and above10.1111/j.1744-7402.2011.02730.x ↗
21. ZrB2–SiC sharp leading edges in high enthalpy supersonic flows10.1111/j.1551-2916.2012.05226.x ↗
22. Oxidation of zirconium diboride with tungsten carbide additions10.1111/j.1551-2916.2010.04216.x ↗
23. Oxidation resistnace of hafnium diboride ceramic with addtions of silicon carbide and tungsten boride or tungsten carbide10.1111/j.1551-2916.2011.04462.x ↗
24. Two dimensional distributions of C2, CH, and OH in a diamond depositing oxyacetylene flame measured by laser induced fluorescence10.1063/1.360186 ↗
25. Degenerate four-wave mixing spectroscopy and spectral simulation of C2 in an atmospheric pressure oxy-acetylene flame10.1063/1.473563 ↗
26. Experiments on ceramic formation from liquid precursor spray axially injected into an oxy-acetylene flame10.1016/j.actamat.2005.08.001 ↗
27. Cu–W (Copper–Tungsten)
28. Oxidation-based materials selection for 2000°C+ hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
29. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
30. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
31. Bubble formation in oxide scales on SiC10.1111/j.1151-2916.1984.tb19160.x ↗
32. Some new perspectives on oxidation of silicon carbide and silicon nitride10.1111/j.1151-2916.1991.tb04348.x ↗
33. Resistance to thermal shock and to oxidation of metal diborides–SiC ceramics for aerospace application10.1111/j.1551-2916.2007.01589.x ↗
34. Dynamic oxidation of ultra-high temperature ZrB2–SiC under high enthalpy supersonic flows10.1016/j.corsci.2010.11.018 ↗
35. Condensed phase relations in the systems ZrO2–WO2–WO3 and HfO2–WO2–WO310.1111/j.1151-2916.1967.tb15084.x ↗
36. ZrW2O8-contianing composites with near-zero coefficient of thermal expansion fabricated by various methods: comparison and optimization10.1016/j.compscitech.2008.09.032 ↗
37. Negative thermal expansion materials10.1039/a904297k ↗
38. Condensed phase relations in the systems ZrO2–WO2–WO3 and HfO2–WO2–WO310.1111/j.1151-2916.1967.tb15084.x ↗