Influence of fibre content on the strength of carbon fibre reinforced HfC/SiC composites up to 2100 °C
Source abstract
Abstract
The influence of carbon fibre content on the mechanical behaviour of HfC/SiC composites was investigated up to 2100 degrees C for specimens containing 40 or 55 vol% fibres. Silicon carbide was added as a sintering aid during hot pressing. Increasing the fibre content made infiltration more difficult, which resulted in higher porosity in the specimen with 55 vol% fibres. The room temperature flexural strength ranged from 340 to 380 MPa, and it increased to more than 400 MPa at 1800 degrees C due to stress relaxation. Increasing temperature was accompanied by a decrease in the slope of the load-displacement curve, indicating a decrease in elastic modulus, but plastic deformation was not observed below 2100 degrees C. At 2100 degrees C, the specimen containing a higher fibre content underwent significant deformation due to low interfacial strength between the fibre plies, retaining a strength at the proportional limit of 290 MPa and an ultimate strength of 520 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. New generation of solid propellants for space launchers10.1016/S0094-5765(00)00049-7 ↗
2. Davidenko · 2016 · 1
3. CMC thermal protection system for future reusable launch vehicles: generic shingle technological maturation and tests10.1016/j.actaastro.2009.01.035 ↗
4. Ablation behavior and mechanism analysis of C/SiC composites10.1016/j.jmrt.2015.10.004 ↗
5. Operational limits for reusable space transportation systems due to physical boundaries of C/SiC materials10.1016/S1270-9638(03)00054-3 ↗
6. Hybrid carbon-carbon ablative composites for thermal protection in aerospace10.1155/2014/825607 ↗
7. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds10.1016/S0955-2219(99)00129-6 ↗
8. Improved microstructure and fracture properties of short carbon fiber-toughened ZrB2-based UHTC composites via colloidal process10.1016/j.ijrmhm.2016.07.010 ↗
9. On the thermal shock resistance and mechanical properties of novel unidirectional UHTCMCs for extreme environments10.1038/s41598-018-27328-x ↗
10. Mechanical behaviour of carbon fibre reinforced TaC/SiC and ZrC/SiC composites up to 2100 °C10.1016/j.jeurceramsoc.2018.11.017 ↗
11. Understanding the mechanical properties of novel UHTCMCs through random forest and regression tree analysis10.1016/j.matdes.2018.02.061 ↗
12. Arc-jet testing on HfB2 and HfC-based ultra-high temperature ceramic materials10.1016/j.jeurceramsoc.2007.11.021 ↗
13. Densification and mechanical behavior of HfC and HfB2 fabricated by spark plasma sintering10.1111/j.1551-2916.2007.02248.x ↗
14. Ablation tests on HfC- and TaC-based ceramics for aeropropulsive applications10.1016/j.jeurceramsoc.2014.11.018 ↗
15. Microstructure, mechanical properties and oxidation behavior of TaC- and HfC-based materials containing short SiC fiber10.1016/j.ceramint.2014.09.070 ↗
16. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
17. Effects of high-energy ball milling and reactive spark plasma sintering on the densification of HfC-SiC composites10.1016/j.jeurceramsoc.2016.12.036 ↗
18. Low temperature sintering of HfC/SiC nanocomposites using HfSi2 -C additives10.1111/jace.14301 ↗
19. Sanders · 1969
20. Carbon fiber reinforced hafnium carbide composite10.1023/B:JMSC.0000041696.64055.8c ↗
21. Hafnium and silicon carbide multilayer coatings for the protection of carbon composites10.1016/j.surfcoat.2013.06.022 ↗
22. Preparation and characterization of ultra high-temperature ternary ceramics Ta4HfC510.1111/jace.14436 ↗
23. UHTC – carbon fiber composites: preparation, oxyacetylene torch testing and characterization10.1016/j.jeurceramsoc.2012.08.018 ↗
24. UHTC, UHTC-composites for hypersonic applications
25. Thermal properties of Cf/HfC and Cf/HfC-SiC composites prepared by precursor in filtration and pyrolysis10.1016/j.jeurceramsoc.2017.12.051 ↗
26. Phase Equilibria Diagrams Online Database (NIST Standard Reference Database 31), The American Ceramic Society and the National Institute of Standards and Technology, 2019. Figure Number 4443; www.nist.gov/srd/nist31.cfm, (n.d.).
27. Ceramic matrix composites: matrices and processing
28. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
29. UHTC-carbon fibre composites: preparation, oxyacetylene torch testing and characterisation10.1016/j.jeurceramsoc.2012.08.018 ↗
30. Evaluation of oxidation behaviors of HfC-SiC ultra-high temperature ceramics at above 2500 °C via oxyacetylene torch10.1016/j.ceramint.2018.02.049 ↗
31. Efficacy of a ZrB2–SiC matrix in protecting C fibres from oxidation in novel UHTCMC materials10.1016/j.matdes.2016.09.104 ↗
32. Continuous C fibre composites with a porous ZrB2 matrix10.1016/j.matdes.2015.06.136 ↗
33. Formation of silicon carbide on carbon fibers by carbothermal reduction of silica10.1016/j.diamond.2003.11.062 ↗
34. Thermal expansion of some transition metal carbides10.1021/j150563a030 ↗
35. Oxidation of hafnium carbide in the temperature range 1400° to 2060 °C10.1111/j.1151-2916.1993.tb05332.x ↗
36. Oxidation behaviour of a continuous carbon fibre reinforced ZrB2–SiC composite10.1016/j.corsci.2017.04.012 ↗
37. Nanostructured HfC – SiC composites prepared by high-energy ball-milling and reactive spark plasma sintering10.1016/j.jeurceramsoc.2015.09.024 ↗
38. The tensile behavior of carbon fibers at high temperatures up to 2400 °C10.1016/j.carbon.2003.11.020 ↗
39. Theories of creep in ceramics10.1080/10408439608241255 ↗
40. Mechanical properties and grain orientation evolution of zirconium diboride-zirconium carbide ceramics10.1016/j.jeurceramsoc.2017.09.013 ↗