The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO–SiO2 based slag
Source abstract
Abstract
One of the main factors limiting the lining lifetime in pyrometallurgical smelters is continuous refractory oxides dissolution in the slag bath. The overall wear is accelerated when the slag infiltrates the porous brick and the dissolution thus occurs in a larger part of the lining. This work investigates the possibility of preventing deep infiltration by sealing off the pores with newly formed phases. Static finger tests at constant temperature (1200°C) were performed in contact with a synthetic non-ferrous PbO-SiO-MgO slag, showing the formation of forsterite (MgSiO) throughout the refractory sample by the reaction between SiO (slag) and MgO (refractory). This phase grows with time, eventually sealing off the pores near the interface with the bath. The phase grows too slow to prevent full infiltration of the refractory but creates an equilibrium state in the sealed off part of the sample, ceasing the chemical corrosion in that part of the sample.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · Materials Engineering and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Refractories for the copper and lead industry
2. Chemical corrosion mechanisms of magnesia–chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
3. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
4. Penetration and corrosion of magnesia grain by silicate slags10.1179/096797800681036 ↗
5. Comparison of ferrous calcium silicate slag and calcium ferrite slag interactions with magnesia–chrome refractories10.1007/s11663-011-9499-0 ↗
6. Analysis and interpretation of refractory microstructures in studies of corrosion mechanisms by liquid oxides10.1016/j.jeurceramsoc.2007.10.012 ↗
7. In situ observation of the direct and indirect dissolution of MgO particles in CaO–Al2O3–SiO2-based slags10.1016/j.jeurceramsoc.2006.05.107 ↗
8. Forsterite bursting in mangesia chromite bricks – two case studies from lead and copper smelting furnaces
9. Reactions of dense MgO with calcium ferrite-based slags at 1573K10.1007/s11663-005-0055-7 ↗
10. In-situ observation of slag penetration into MgO refractory10.1034/j.1600-0692.2002.310109.x ↗
11. A consideration on corrosion of magnesia refractory brick by silicate slag
12. Effect of spinel content on slag attack resistance of high alumina refractory castables10.1016/j.jeurceramsoc.2007.04.007 ↗
13. The corrosion and microstructure relationship for cement-bonded spinel refractory castables10.1016/j.ceramint.2011.10.061 ↗
14. Factors affecting the corrosion by fayalite slags and the thermal shock performance of magnesia–chrome bricks
15. Flame-assisted laser surface treatment of refractory materials for crack-free densification10.1016/S0921-5093(99)00592-4 ↗
16. Surface modification of alumina-based refractories using a xenon arc lamp10.1016/S0169-4332(99)00421-3 ↗
17. Influence of chrome-bearing sols vacuum impregnation on the properties of magnesia–chrome refractory10.1016/j.ceramint.2006.12.002 ↗
18. Effect of temperature gradient on industrial gasifier coal slag infiltration into alumina refractory10.1111/j.1551-2916.2011.04782.x ↗
19. Influence of oxygen partial pressure on synthetic coal slag infiltration into porous Al2O3 refractory10.1111/j.1551-2916.2012.05175.x ↗
20. Changes in microstructure of a high chromia refractory due to interaction with infiltrating coal slag in a slagging gasifier environment10.1016/j.ceramint.2007.08.010 ↗
21. Dissolution of refractories for gasification process of petroleum coke for the steel industry10.1016/j.fuel.2011.08.039 ↗
22. Experimental study of phase equilibria in the PbO–MgO–SiO2 system10.1007/s11663-001-0002-1 ↗
23. A study of slag-infiltrated magnesia–chromite refractories using hybrid microwave heating10.1016/S0955-2219(00)00343-5 ↗
24. Using confocal scanning laser microscopy for the in situ study of high-temperature behaviour of complex ceramic materials10.1016/j.jeurceramsoc.2007.01.022 ↗
25. The direct bond in magnesia chromite and magnesia spinel refractories10.1111/j.1151-2916.1995.tb08885.x ↗
26. Degradation mechanisms of magnesia–chromite refractories in vacuum-oxygen decarburisation ladles during production of stainless steel10.1179/030192300677525 ↗
27. Kowalski · 1995
28. Growth of multilayered polycrystalline reaction rims in the MgO–SiO2 system, Part I: Experiments10.1007/s00410-010-0517-z ↗
29. Degradation mechanisms and use of refractory linings in copper production processes: A critical review10.1016/j.jeurceramsoc.2013.10.005 ↗