Abstract A dense silicon carbide (SiC) ceramic with a very high flexural strength at 2000 °C (981 ± 128 MPa) was obtained by conventional hot-pressing with extremely low additive content (2000 ppm Y2O3). Observations using high-resolution transmission electron microscopy (HRTEM) showed that (1) homophase (SiC/SiC) boundaries were clean without an intergranular glassy phase and (2) junction pockets consisted of nanocrystalline Y-containing phase embedded in an amorphous Y-Si-O-C-N phase. The excellent strength at 2000 °C was attributed to the clean SiC/SiC boundary and the strengthening effect of plastic deformation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Role of the grain-boundary phase on the elevated-temperature strength toughness, fatigue and creep resistance of silicon carbide sintered with Al, B and C10.1016/S1359-6454(00)00246-9 ↗
2. Improved high temperature properties of SiC-ceramics sintered with Lu2O3-containing additives10.1016/S0955-2219(02)00282-0 ↗
3. Effect of Y2O3-Al2O3 ratio on inter-granular phases and films in tape-casting α-SiC with high toughness10.1016/j.actamat.2004.10.055 ↗
4. Nano- versus macro-hardness of liquid phase sintered SiC10.1016/j.jeurceramsoc.2004.01.026 ↗
5. Sliding-wear-resistant liquid-phase-sintered SiC processed using α-SiC starting powders10.1111/j.1551-2916.2006.01421.x ↗
6. Electrochemical corrosion of silicon carbide ceramics in H2SO410.1016/j.jeurceramsoc.2013.08.024 ↗
7. Electrochemical corrosion of silicon carbide ceramics in sodium hydroxide10.1016/j.jeurceramsoc.2013.12.043 ↗
8. Microstructure and thermal conductivity of silicon carbide with yttria and scandia10.1111/jace.12737 ↗
9. Exceptional micromachining performance of silicon carbide ceramics by adding graphene nanoplatelets10.1016/j.jeurceramsoc.2017.03.072 ↗
10. SiC and Si3N4 materials with improved fracture resistance10.1016/0955-2219(92)90028-C ↗
11. Heat-resistant silicon carbide with aluminum nitride and erbium oxide10.1111/j.1151-2916.2001.tb00958.x ↗
12. Microstructural analysis of liquid-phase-sintered β-silicon carbide10.1111/j.1151-2916.2002.tb00107.x ↗
13. Intergranular film thickness of self-reinforced silicon carbide ceramics10.1016/j.jeurceramsoc.2003.12.029 ↗
14. Electrical resistivity of α-SiC ceramics sintered with Al2O3 or AlN additives10.1016/j.jeurceramsoc.2014.01.004 ↗
15. Intergranular glassy phase free SiC ceramics retains strength at 1500°C10.1016/j.scriptamat.2004.02.008 ↗
16. High-temperature strength of silicon carbide ceramics sintered with rare-earth oxide and aluminum nitride10.1016/j.actamat.2006.08.059 ↗
17. High-temperature effects in the fracture mechanical behavior of silicon carbide liquid-phase sintered with AlN-Y2O3 additives10.1016/S0955-2219(00)00317-4 ↗
18. High-temperature strength of liquid-phase-sintered SiC with AlN and Re2O3 (RE=Y, Yb)10.1111/j.1151-2916.2002.tb00211.x ↗
19. Effect of liquid phase sintering on microstructure and mechanical properties of Yb2O3-AlN containing SiC-based ceramics10.1111/j.1551-2916.2005.00212.x ↗
20. Heat-resistant silicon carbide with aluminum nitride and scandium oxide10.1016/j.actamat.2005.07.002 ↗
21. High-temperature mechanical property improvements of SiC ceramics by NITE process10.2320/matertrans.47.1204 ↗
22. High-temperature strength of silicon carbide sintered with 1wt% aluminum nitride and lutetium oxide10.1016/j.jeurceramsoc.2012.09.005 ↗
23. High-temperature strength of a thermally conductive silicon carbide ceramic sintered with yttria and scandia10.1016/j.jeurceramsoc.2016.02.028 ↗
24. Gas pressure sintering of SiC sintered with rare-earth-(III)-oxides and their mechanical properties10.1016/j.ceramint.2004.06.027 ↗
25. Electrodischarge-machinable silicon carbide ceramics sintered with yttrium nitrate10.1111/j.1551-2916.2011.04419.x ↗
26. Rare-earth nitrate additives for the sintering of silicon carbide10.1016/j.jeurceramsoc.2013.05.017 ↗
27. Influence of Y2O3 addition on electrical properties of β-SiC ceramics sintered in nitrogen atmosphere10.1016/j.jeurceramsoc.2012.07.001 ↗
28. Mechanical properties of electrically conductive silicon carbide ceramics10.1016/j.ceramint.2014.03.036 ↗
29. Conductive SiC ceramics fabricated by spark plasma sintering10.1016/j.ceramint.2016.07.126 ↗
30. Tribological characteristics of SiC ceramics sintered with a small amount of yttria10.1016/j.ceramint.2015.07.210 ↗
31. Standard test method for flexural strength of advanced ceramics at ambient temperature
32. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
33. Interface characteristics affecting electrical properties of Y-doped SiC10.1557/JMR.2003.0365 ↗
34. Mechanical properties of hot-forged silicon carbide ceramics10.1016/j.scriptamat.2004.09.012 ↗
35. Deformation of UO2 at high temperatures10.1111/j.1151-2916.1971.tb12230.x ↗
36. Brittle-ductile transition in polycrystalline aluminum oxide10.1080/14786436608213531 ↗
37. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
38. Sintering and mechanical properties of ZrB2-TaSi2 and HfB2-TaSi2 ceramic composites10.1111/j.1551-2916.2008.02593.x ↗
39. Microstructure and high-temperature strength of textured and non-textured ZrB2 ceramics10.1088/1468-6996/15/1/014202 ↗