Microstructure evolution and mechanical properties of porous Si3N4 and dense Si3N4 joints bonded using CaO–Li2O-Al2O3–SiO2 glass-ceramic
Source abstract
Abstract
Abstract A novel CaO-Li2O-Al2O3-SiO2 (CLAS) glass was developed for the joining of porous Si3N4 and dense Si3N4. A multiphase interlayer consisting of CaAl2Si2O8, LiAlSi2O6 and CaSiO3 phases was formed in joint, which possessed matched CTE with the Si3N4 substrates. In addition, the infiltrated layer with bilayer structure in the porous Si3N4 substrate was observed. The effects of joining temperature and cooling rate on microstructure, phase evolution and shear strength of joints were studied carefully. The results showed that the kinds of precipitated phases remained invariable with the joining temperature increased, but the crystallinity in the interlayer was improved remarkably as the cooling rate reduced. The maximum shear strength of 45 MPa was obtained when the joining temperature and cooling rate were 1100 °C and 5 °C/min, respectively. Moreover, fracture during the shear test occurred mainly within porous Si3N4 side, indicating superior joining of dense Si3N4/glass-ceramic/porous Si3N4.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Dielectric and mechanical properties of porous Si3N4 ceramics prepared via low temperature sintering10.1016/j.ceramint.2008.09.010 ↗
2. Oxidation bonding of porous silicon nitride ceramics with high strength and low dielectric constant10.1016/j.matlet.2006.08.067 ↗
3. Effect of TiO2 addition on the microstructures, mechanical and dielectric properties of porous Si3N4-based ceramics10.1080/17436753.2017.1320063 ↗
4. Joining of engineering ceramics10.1179/174328009X461078 ↗
5. Silicon nitride and related materials10.1111/j.1151-2916.2000.tb01182.x ↗
6. Mechanical properties of silicon nitride-based ceramics and its use in structural applications at high temperatures10.1016/j.msea.2009.09.064 ↗
7. Chemical behavior in diffusion bonding of Si3N4-Ni and Si3N4-superalloy IN-73810.1016/1359-6462(96)00161-3 ↗
8. Microstructure and mechanical properties of partial transient liquid phase bonded Si3N4–DZ483 superalloy joints10.1016/j.matlet.2014.01.072 ↗
9. Microstructure and strengthening mechanism of Si3N4/Invar joint brazed with TiNp-doped filler10.1016/j.msea.2015.10.038 ↗
10. Microstructure and brazing mechanism of porous Si3N4/Invar joint brazed with Ag-Cu-Ti/Cu/Ag-Cu multi-layered filler10.1016/j.jmst.2017.07.001 ↗
11. Interfacial microstructure and mechanical properties of porous-Si3N4 ceramic and TiAl alloy joints vacuum brazed with AgCu filler10.1016/j.ceramint.2017.04.149 ↗
12. Design and properties of glass-ceramics10.1146/annurev.ms.22.080192.000515 ↗
13. Y2O3–Al2O3–SiO2-based glass-ceramic fillers for the laser-supported joining of SiC10.1016/j.jeurceramsoc.2014.01.019 ↗
14. CaO-Al2O3 glass-ceramic as a joining material for SiC based components: a microstructural study of the effect of Si-ion irradiation10.1016/j.jnucmat.2018.01.033 ↗
15. Application of Nd2O3–Al2O3–SiO2 glass solder for joining of silicon carbide components10.1016/j.jeurceramsoc.2016.01.020 ↗
16. Silicon nitride joining10.1111/j.1151-2916.1985.tb15811.x ↗
17. Bonding of silicon nitride ceramic composites with Y2O3-La2O3-Al2O3-SiO2 mixtures10.1557/JMR.2002.0291 ↗
18. Silicon nitride joining using silica and yttria ceramic interlayers10.1111/j.1151-2916.2002.tb00196.x ↗
19. Microstructure and properties of porous Si3N4/Dense Si3N4 joints bonded using RE–Si–Al–O–N (RE = Y or Yb) glasses10.3390/met7110500 ↗
20. Joining of dense Si3N4 ceramics with tape cast Lu-Al-Si-ON interlayer10.1016/j.ceramint.2017.12.070 ↗
21. Joining of Si3N4/Si3N4 with in-situ formed Si-Al-Yb oxynitride glasses interlayer10.1016/j.ceramint.2018.01.217 ↗
22. Preparation and characterization of CaO-Al2O3-SiO2 (CAS) glass-ceramics10.1016/j.jnoncrysol.2016.10.019 ↗
23. Effect of TiO2 content on the crystallization behavior and properties of CaO-Al2O3-SiO2 glass ceramic fillers for high temperature joining application10.1016/j.jallcom.2017.10.166 ↗
24. Silicon nitride: the engineering material of the future10.1007/s10853-011-5942-5 ↗
25. Crystallization behavior and thermal properties of B2O3–containing MgO-Al2O3-SiO2-Li2O glass-ceramic and its wettability on Si3N4 ceramic10.1016/j.jeurceramsoc.2018.12.002 ↗
26. Crystallization, microstructures and properties of low temperature co-fired CaO-Al2O3-SiO2 glass-ceramic10.1007/s10832-016-0048-8 ↗
27. Microstructure-based simulation of thermomechanical behavior of composite materials by object-oriented finite element analysis10.1016/S1044-5803(03)00054-8 ↗
28. Sinterable β-Spodumene glass-ceramics10.1111/j.1151-2916.1989.tb05994.x ↗
29. The influence of different CaO source in the production of anorthite ceramics10.1016/j.ceramint.2008.02.024 ↗
30. Glass-based seals for solid oxide fuel and electrolyzer cells–a review10.1016/j.mser.2009.12.002 ↗
31. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
32. Pre-infiltration and brazing behaviors of Cf/C composites with high temperature Ti-Si eutectic alloy10.1016/j.carbon.2018.08.021 ↗
33. Ablation resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3,000 °C10.1038/ncomms15836 ↗
34. Toughening of CaO–Al2O3–SiO2 glass by dmisteinbergite precipitation10.1016/j.matlet.2016.05.123 ↗
35. Joining of porous alumina with a CaO-Al2O3-SiO2 glass-ceramic10.1111/jace.12310 ↗