journal article·2010-10

Powder-binder separation in injection moulded green parts

Anne Mannschatz, Sören Höhn, Tassilo Moritz

Publisher page

Abstract

Abstract For powder injection moulding (PIM) the ceramic powder is mixed with a thermoplastic binder system to achieve an injectable feedstock. In contrast to injection moulding of polymeric components, the binder must be removed after the shaping step before sintering the ceramic part to full density. During the mould filling process shear forces act on the blend that might cause separations of powder particles and binder. In this case polymer films form at the mould surface and at internal interfaces which induce microstructural defects in the debinded part. In particular for multi-component parts this effect is critical since binder films in the joining zone weaken the bonding strength between the two components that might even lead to delamination. For detecting binder separations within the injection moulded bulk material and at joining zones of two-component parts the microstructure of green samples has been studied. Since conventional machining techniques like grinding and polishing modify the original structure, e.g. when particles are pulled out of the matrix and binder smears onto the surface, a special ceramographic method for the preparation of cross-sections was applied. This approach bases on broad ion beam techniques and enables the simultaneous polishing of hard ceramic particles and soft polymer molecules without destroying the structure or producing a relief at the surface. In the analysed samples binder accumulations were found along flow lines, at weld lines, at boundaries of so-called dead water regions and at the interface of two-component parts.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Injection Molding Process and Properties · Additive Manufacturing and 3D Printing Technologies · Polymer Foaming and Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Homogeneity effects on feedstock viscosity in powder injection molding10.1111/j.1151-2916.1994.tb06992.x ↗
2. German · 1997
3. Binder evolution from powder compacts: thermal profile for injection-molded articles10.1111/j.1151-2916.1989.tb05981.x ↗
4. Debinding and sintering defects from particle orientation in ceramic injection moulding10.1007/BF01152138 ↗
5. The orientation of binders and particles during ceramic injection moulding10.1016/S0955-2219(96)00070-2 ↗
6. Characterization of particle packing in an injected molded green body10.1111/j.1151-2916.1995.tb09090.x ↗
7. Characterization of micro- and macrostructure of injection-molded green body by liquid immersion method10.1016/S0955-2219(96)00128-8 ↗
8. Engineering of high performance injection moulded ceramic components by polarised light optical texture analysis (PLOTA)10.1504/IJMPT.2009.025684 ↗
9. Quantitative study of powder binder separation of feedstocks
10. Mannschatz · 2008
11. Particle contact before firing10.1016/S0955-2219(96)00126-4 ↗
12. Flow and void formation in powder injection moulding feedstocks made with PEG/PMMA binders part 2–slip band model10.1179/174329008X271628 ↗
13. Flow instabilities in capillary flow of concentrated suspensions10.1007/BF00453463 ↗
14. A review of the slip (wall depletion) of polymer solutions, emulsions and particle suspensions in viscometers: its cause, character, and cure10.1016/0377-0257(94)01282-M ↗
15. Modell zur Beschreibung des Fließens wandgleitender Substanzen durch Düsen10.1007/BF01538515 ↗