journal article·2011-07

Non-uniform ageing behavior of individual grain boundaries in ZnO varistor ceramics

Jinliang He, Jun Liu, Jun Hu, Rong Zeng, Wangcheng Long

Publisher page

Abstract

Abstract In this paper, the ageing characteristics of individual grain boundaries in ZnO varistor ceramics were directly measured for the first time, which were carried out based on the microcontact technique in combination with accelerated AC voltage ageing tests. The current–voltage ( I – V ) characteristics of individual grain boundaries were measured on a microprobe station after the sample was degraded under different ageing time. The results indicated that the I – V characteristics of individual grain boundaries varied non-uniformly during ageing process, which could be roughly classified into two categories as monotonic and non-monotonic. It is revealed that degradation and recovery of electrical properties coexisted in the ageing process, which could be explained with ion migration and oxygen desorption mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Dielectric properties of ceramics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Zinc oxide varistors10.1109/57.44606 ↗
2. Application of zinc oxide varistors10.1111/j.1151-2916.1990.tb05232.x ↗
4. Random quasi-phase-matching in bulk polycrystalline isotropic nonlinear materials10.1038/nature03027 ↗
5. Barrier voltage deformation of ZnO varistors by current pulse10.1063/1.352175 ↗
6. Role of oxygen at the grain boundary of metal oxide varistors: a potential barrier formation mechanism10.1063/1.1378051 ↗
7. Diffusion of zinc vacancies and interstitials in zinc oxide10.1063/1.2206559 ↗
8. Electron-trapping polycrystalline materials with negative electron affinity10.1038/nmat2289 ↗
9. Optical and electrical resistivity studies of isovalent and aliovalent 3d transition metal ion doped ZnO10.1103/PhysRevB.80.045210 ↗
10. Defects and degradation in ZnO varistor10.1063/1.117775 ↗
11. Effect of long-term electrical degradation on the distribution of donor impurities in ZnO varistor ceramics10.1007/BF02758435 ↗
12. Thermal degradation of electrical properties and morphology of bulk single-crystal ZnO surfaces10.1063/1.1801674 ↗
13. Comparison of non-ohmic accelerated ageing of the ZnO- and SnO2-based voltage dependent resistors10.1088/0022-3727/42/1/015503 ↗
14. Incorporation of monovalent ions in ZnO and their influence on varistor degradation10.1111/j.1151-2916.1993.tb07779.x ↗
15. Degradation mechanism of ZnO ceramic varistors studied by electrochemical hydrogen charging10.1143/JJAP.42.L48 ↗
16. Thermal conductivity features of ZnO-based varistors using the laser-pulse method10.1016/j.msea.2003.09.069 ↗
17. Electroplating-induced degradation in ZnO ceramic varistors10.1007/s10853-005-2149-7 ↗
18. Degradation phenomena due to humidity in low voltage ZnO varistors10.1016/j.ceramint.2005.08.009 ↗
19. Degradation characteristics of low-voltage ZnO varistor manufactured by chemical coprecipitation processing10.1016/j.jmatprotec.2007.09.033 ↗
20. Direct determination of barrier voltage in ZnO varistors10.1063/1.326015 ↗
21. Different “single grain junctions” within a ZnO varistor10.1063/1.338091 ↗
22. Characterization of individual interfacial barriers in a ZnO varistor material10.1063/1.344453 ↗
23. Electrical nonuniformity of grain boundaries with in ZnO varistors10.1111/j.1151-2916.1993.tb03733.x ↗
24. Single junctions in ZnO varistors studied by current–voltage characteristics and deep level transient spectroscopy10.1143/JJAP.34.1765 ↗
25. ICTS measurements of single grain boundaries in ZnO:rare-earth varistor10.1023/A:1009973704222 ↗
26. Characterization of ZnO-degraded varistors used in high-tension devices10.1016/j.materresbull.2006.09.001 ↗
27. Comparative electrical behavior at low and high current of SnO2 and ZnO-based varistors10.1111/j.1551-2916.2008.02436.x ↗
28. A grain-boundary defect model for instability/stability of a ZnO varistor10.1007/BF01113755 ↗
29. A new interpretation for the degradation phenomenon of ZnO varistors10.1007/BF02403838 ↗
30. Importance of oxygen atmosphere to recover the ZnO-based varistors properties10.1007/s10853-006-0589-3 ↗
31. Evolution of CaCu3Ti4O12 varistor properties during heat treatment in vacuum10.1016/j.ceramint.2006.04.003 ↗