Abstract
A tungsten carbide ceramic containing 5 vol% silicon carbide was hot pressed to full density at 1820 °C. A small amount of transient liquid phase based on W-C-Si-O facilitated oxide removal in the reducing environment and favoured the development of a bimodal microstructure containing sub-micrometric grains with square or rod-like morphologies. These microstructural features led to outstanding mechanical properties from room to elevated temperatures. For the first time, WC-materials were characterized up to 1500 °C exhibiting flexural strength over 1 GPa in the whole temperature range and fracture toughness from 7 to 15 MPa??m.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Cermets and hardmetals
2. Tarragó · 2016
3. The high-temperature properties of ceramics and cermets10.1179/pom.1958.1.1-2.020 ↗
4. Buss · 2004
5. High temperature mechanical properties of WC–Co hard metals10.1016/j.ijrmhm.2016.01.002 ↗
6. Microstructural study of hot-deformed cemented carbides10.1080/01418618008241826 ↗
7. Comportement mecanique entre 800°C et 2200°C de l’hemicarbure de tungsten10.1016/0036-9748(80)90135-0 ↗
8. Toth · 1971
9. Bulk ultrafine binderless WC prepared by spark plasma sintering10.1016/j.scriptamat.2005.10.014 ↗
10. Binderless WC and WC–VC materials obtained by pulsed electric current sintering10.1016/j.ijrmhm.2007.01.002 ↗
11. Spark plasma sintering of diamond binderless WC composites10.1111/j.1551-2916.2011.05009.x ↗
12. Plasma sintering behavior of binderless WC powders
13. Sparking plasma sintering of nanometric tungsten carbide10.1016/j.ijrmhm.2008.06.004 ↗
14. Influence and effectivity of VC and Cr3C2 grain growth inhibitors on sintering of binderless tungsten carbide10.1016/j.ijrmhm.2011.11.006 ↗
15. Effects of carbide grain growth inhibitors on the microstructures and mechanical properties of WC–SiC–Mo2C hard ceramics10.1016/j.ijrmhm.2013.11.016 ↗
16. Properties of ultra-fine binderless cemented carbide RCCFN10.1016/0263-4368(95)92676-B ↗
17. Microstructure and mechanical properties of WC-SiC composites10.2320/matertrans.M2011045 ↗
18. Case study: building an ultrahigh-temperature mechanical testing system
19. Fracture toughness calculations from maximum load in four point bend tests of chevron notch specimens10.1007/BF00013393 ↗
20. Indentation fracture of WC–Co cermets10.1007/BF00555296 ↗
21. An analysis of grain boundaries and grain growth in cemented tungsten carbide using orientation imaging microscopy10.1007/s11661-006-0032-z ↗
22. Hardness anisotropy and slip in WC crystals
23. German · 1996
24. Grain growth inhibition of hardmetals during initial heat-up10.1016/j.ijrmhm.2017.12.016 ↗
25. Combined effects of WC and SiC on densification and thermo-mechanical stability of ZrB2 ceramics10.1016/j.matdes.2016.06.114 ↗
26. Tungsten carbides and W-C phase diagram10.1134/S0020168506020051 ↗
27. Low‐temperature spark plasma sintering of pure nano WC powder10.1111/jace.12365 ↗
28. Field assisted sintering technique compaction of ultrafine-grained binderless WC hard metals10.12693/APhysPolA.122.639 ↗
29. Properties of nanostructured tungsten carbide and their rapid consolidation by pulsed current activated sintering10.1088/0031-8949/2010/T139/014043 ↗
30. Thermodynamic assessment of the Si-Ta and Si-W systems10.1007/s11669-009-9579-x ↗
31. The bend deformation of WC–Co cemented carbides at temperatures up to 1273 K10.2320/matertrans1960.23.77 ↗
32. The mechanical behaviour of cemented carbides at high temperatures10.1016/0025-5416(88)90716-1 ↗
33. Plastic flow in WC–13 wt% Co at high temperatures10.1016/0921-5093(92)90144-P ↗
34. Elevated temperature properties of WC–Co cemented carbides10.1016/0025-5416(88)90718-5 ↗
35. mechanical properties in bending tests and mechanical behavior of submicron and micron WC–Co grades at elevated temperatures
36. High temperature fatigue of cemented carbides under cyclic loads10.1016/S0263-4368(99)00014-1 ↗
37. Swab · 2005